1. Introduction
Sand serves as the backbone of sand casting, forming the mold cavity that directly shapes every casting.
By packing sand around a pattern, foundries create the negative impression into which molten metal flows, solidifies, and takes on its final geometry.
Sand selection plays a pivotal role: it influences surface finish, gas permeability, dimensional accuracy, and ultimately, cost.
In the following sections, we examine the principal sand systems—green, chemically bonded, sodium silicate, resin‑coated, and specialty sands—highlighting their compositions, properties, and ideal applications.
2. Green Sand
Green sand serves as the workhorse mold medium in over 70% of global sand‑casting operations.
Foundries favor it for its low cost, ease of reuse, and adaptability to a broad range of part sizes and geometries.

Composition
A typical green‑sand mixture contains:
| Component | Typical Proportion | Function |
| Silica sand | 85–90 wt % | Provides refractory skeleton and definition |
| Bentonite clay | 5–10 wt % | Imparts plasticity, “green strength,” and collapsibility |
| Water | 2–4 wt % | Activates clay binder; controls mold plasticity |
| Additives (sea‑coal, 1–3 wt %) | 1–3 wt % | Enhances surface finish and promotes lustrous carbon |
Key Properties
- Moisture Content (2–4 %)
Ensures good sand plasticity for pattern imprinting. Too little moisture causes crumbling; too much yields poor permeability and gas defects. - Green Strength (30–50 psi)
Measures the unbaked mold’s ability to support molten metal without collapse. - Permeability (200–400 PN)
Indicates how readily gases escape mold cavities—critical to avoid porosity. - Collapsibility (0.5–1.5 mm)
Describes mold’s controlled deformation on solidification, reducing hot‑tear defects.
Advantages and Applications
Green sand’s low tooling cost ($50–$200 per mold) and reusability over 5–20 cycles make it ideal for large,
heavy castings such as engine blocks, pump housings, and agricultural machinery components.
Foundries also utilize green sand for prototype parts, where rapid turnover and minimal upfront investment matter.
Limitations & Mitigations
- Dimensional Tolerance (± 0.5–1.5 %)
Green‑sand molds exhibit looser tolerances than resin‑bonded processes. Engineers tighten tolerances by precisely controlling clay and moisture levels. - Washout in Thin Sections
Extended contact with molten metal can erode fine details. Increasing clay content or applying refractory coatings to mold walls mitigates washout.
3. Chemically Bonded Sand
Chemically bonded sand systems transform simple silica grains into high‑performance molds and cores by using synthetic resins as binders.
Foundries select from three leading resin chemistries—phenolic, furan, and epoxy—each tailored to specific strength, cure, and gas‑generation profiles.
Resin Types and Properties
- Phenolic Resins: Offer excellent thermal stability (up to 300 °C) and low gas evolution (≤ 0.2 L/kg sand).
They achieve bench strengths of 200–300 psi (1.4–2.1 MPa) within 5–10 minutes. - Furan Resins: Cure rapidly (1–3 minutes) with moderate gas evolution (0.3–0.5 L/kg).
Their bench strengths reach 250–350 psi (1.7–2.4 MPa), making them ideal for medium‑run steel castings. - Epoxy Binders: Deliver the highest strengths (300–400 psi / 2.1–2.8 MPa) and minimal gas output (< 0.1 L/kg).
Although cure times extend to 15–30 minutes, epoxy sands produce exceptionally clean surfaces for thin‑walled aluminum parts.
Transitioning from resin chemistry to process selection, foundries choose between No‑Bake and Cold‑Box methods:
No‑Bake Process
- Mechanism: Mix sand with liquid resin and catalyst; allow the mold to cure at ambient temperature.
- Advantages: Simple setup, energy‑efficient (no external heating), accommodates large molds (> 2 m in length).
- Typical Metrics: Compressive strengths > 10 MPa within 2–5 minutes; bench life of 10–15 minutes for mold assembly.
Cold‑Box Process
- Mechanism: Pack sand–resin mix in a flask, then pass a gaseous amine catalyst through the sand to trigger instant cure.
- Advantages: Cycle times as low as 30 seconds, ideal for high‑volume production and intricate cores.
- Typical Metrics: Compressive strengths of 10–15 MPa in under 1 minute; low residual catalyst minimizes defects.
While chemically bonded sands deliver bench strength up to 15 MPa and collapsibility adequate for complex geometries, they demand rigorous gas‑management.
Excessive gas evolution can cause pinholes and blow‑holes; thus, foundries regulate resin dosage,
optimize core-box venting, and employ vacuum or low‑pressure pours to mitigate defects.
Applications range from large marine engine blocks—where dimensional tolerances tighten to ± 0.2 mm—to aerospace turbine housings requiring Ra ≤ 2 µm finishes.
In these scenarios, chemically bonded sands meet both the dimensional precision and surface‑quality standards that green sand cannot achieve.
4. Sodium Silicate (Water Glass) Sand
Building on chemically bonded systems, sodium silicate sand—often called water glass sand—offers a distinctive CO₂‑curing mechanism that balances speed, strength, and surface quality.
Foundries employ it primarily for core making and medium‑volume castings where rapid turnaround and good finishes matter.

Binding Mechanism and CO₂ Hardening
- Mixing: Operators blend silica sand with a liquid sodium silicate solution (8–12 wt %).
- Mold Assembly: Technicians pack or shoot the wet sand around the pattern or core box.
- CO₂ Curing: A stream of 100% CO₂ (flow rate 4–8 m³/h) passes through the mold.
- Set Time: The silicate gel forms in 10–30 seconds, yielding a rigid mold ready for immediate assembly.
Thanks to this rapid hardening, sodium silicate cores can enter the flask and be poured within 1–2 minutes of CO₂ exposure, dramatically shortening cycle times compared to resin systems.
Advantages
- Fast Cure: Complete gelation in under 30 seconds eliminates lengthy bench times, boosting throughput.
- Good Surface Finish: Cured cores exhibit surface roughness around Ra 3–5 µm, finer than green sand by 30–50%.
- Low Smoke and Odor: CO₂ curing generates negligible volatile byproducts, improving foundry working conditions.
- Reusability: When properly reclaimed, sodium silicate sand can cycle through 8–12 uses before significant strength loss.
Drawbacks
- Reclamation Challenges: High sodium carbonate content necessitates wet or thermal reclamation at 600–800 °C to strip binders—raising energy costs.
- Reduced Sand Life: Recycled sand eventually accumulates carbonate and fines, degrading strength by up to 15% after 10 cycles.
- Moisture Sensitivity: Ambient humidity above 70% can pre-harden mixtures or slow CO₂ penetration, requiring climate control.
Applications
Foundries leverage sodium silicate sand when they need a balance of speed and accuracy:
- Core Making: Gas‑hardened cores for pump impellers, valve bodies, and heat‑exchange passages.
- Medium‑Size Steel Castings: Manifolds and gearbox housings (10–200 kg range) that require moderate dimensional tolerances (± 0.3 mm).
5. Resin‑Coated Sands
Resin‑coated sands—commonly used in shell molding—combine the precision of chemically bonded systems with the speed of high‑volume production.
By applying a thin, pre‑catalyzed resin layer to each sand grain, foundries create robust “shells” that capture fine detail and maintain exceptional dimensional accuracy.

Shell Molding Process
- Resin Coating: Manufacturers uniformly coat high‑purity silica sand (AFS 50–70) with 1–2 wt % thermosetting resin (phenolic or epoxy).
- Shell Formation: They tumble the coated sand around a pre‑heated pattern (175–200 °C); heat cures the resin, forming a rigid shell approximately 2–5 mm thick.
- Core Assembly: Technicians remove unbonded sand, assemble shell halves into a flask, and backfill with uncoated sand for support.
- Casting: Rapid shell production yields molds ready for pouring—often within 5 minutes of pattern removal.
Key Advantages
- Exceptional Surface Finish: Shell‑molded castings achieve Ra ≤ 2 µm—up to 80% smoother than green‑sand counterparts.
- Tight Tolerances: Dimensional accuracy reaches ± 0.1 mm, reducing post‑machining by 30–40%.
- Thin‑Wall Capability: Walls as thin as 1 mm with minimal hot tears or washout.
- Automation‑Friendly: Continuous shell lines produce 100–200 shells per hour, supporting high throughput.
Cost and Cycle‑Time Considerations
| Metric | Shell Molding | Green Sand | Die Casting |
| Mold Cost | $500–$2,000/shell | $50–$200/mold | $10,000–$100,000/die |
| Cycle Time | 5–10 min/shell | 20–60 min | Seconds per shot |
| Part Volume | 1,000–50,000/year | 100–10,000/year | 10,000–1,000,000/year |
| Machining Reduction | 30–40 % | 0–10 % | 40–60 % |
While shell molding requires higher upfront costs, its rapid cycles and reduced finishing make it economically compelling for medium production runs (1,000–50,000 units).
Target Industries and Applications
- Automotive Turbocharger Housings: Thin‑wall, high‑thermal components benefit from shell molding’s precision.
- Aerospace Gearbox Casings: Tight tolerances (± 0.1 mm) and fine finishes meet stringent certification standards.
- Precision Medical Devices: Complex geometries with Ra < 2 µm surfaces require almost no secondary operations.
- Electronics Enclosures: Small, intricate die‑cast alternatives use shell molds to avoid porosity and improve EMI performance.
6. Specialty Sands and Additives
Beyond standard silica mixes, foundries deploy specialty sands and additives to tackle high‑temperature service, improve surface quality, and fine‑tune mold behavior.
By tailoring sand chemistry and grain characteristics, engineers optimize castings for demanding applications.

High‑Temperature Sands
When molten metal temperatures exceed 1,300 °C—or when thermal shock resistance matters—foundries substitute or blend in refractory sands:
| Sand Type | Composition | Melting Point | Benefits | Typical Use Cases |
| Zircon Sand | ZrSiO₄ | > 2,200 °C | Exceptional refractoriness; very low thermal expansion (4.5 × 10⁻⁶/K); minimal metal penetration | Superalloy turbine blades; steel ingot molds |
| Olivine Sand | (Mg,Fe)₂SiO₄ | ~ 1,900 °C | Good thermal stability; low friability; moderate cost (10–20% above silica) | Heavy‑section steel and iron castings |
| Chromite Sand | FeCr₂O₄ | > 1,700 °C | High thermal conductivity (≈ 7 W/m·K); reduced sand‑metal chemical reaction | High‑temperature alloy investment casting; glass molds |
Surface‑Quality Additives
To achieve smoother cast surfaces and minimize washout, foundries introduce fine organic or carbonaceous additives:
- Coal Dust (Sea‑Coal)
-
- Dosage: 1–3 wt % of sand mix
- Function: At casting temperature, coal volatiles deposit a thin carbon layer that improves metal flow and reduces sand fusion, yielding surface finishes 20–30% better than untreated sand.
- Lustrous Carbon Additives
-
- Chemistry: Blend of coal tar pitch and graphite microspheres
- Benefit: Produces a shiny carbon film in the mold cavity, further enhancing detail and preventing metal penetration into sand pores—critical for high‑precision aluminum and brass castings.
Grain Size and Fineness
The American Foundry Society (AFS) Grain Fineness Number guides sand selection:
| AFS Number | Average Grain Diameter | Effect on Mold Behavior |
| 30–40 | 0.6–0.8 mm | High permeability, coarse finish |
| 50–70 | 0.3–0.6 mm | Balance of permeability and detail |
| 80–100 | 0.2–0.3 mm | Fine detail (Ra ≤ 3 µm), lower permeability |
- Coarser Sands (AFS 30–40): Ideal for heavy sections where gas escape outweighs surface requirements.
- Medium Sands (AFS 50–70): The workhorse for general engineering castings, offering a compromise between fillability and detail.
- Fine Sands (AFS 80–100): Required for thin walls, sharp edges, and small features, but often blended with coarser grains to maintain gas flow.
7. Key Properties of Sand for Sand Casting
| Property | Importance | Typical Range |
| Moisture Content | Plasticity vs. permeability | 2–4% |
| Green Strength | Mold stability before pouring | 30–50 psi (0.2–0.3 MPa) |
| Permeability | Gas escape duringpour | 200–400 (permeability number) |
| Refractoriness | Resistance to molten metal temperature | 1,200–1,400 °C |
| Collapsibility | Ease of sand removal after solidification | 0.5–1.5 mm deformation |
| Grain Fineness | Surface finish vs. permeability | AFS 40–100 |
8. Selection of Sand for Specific Casting Applications
Based on Metal Type
Different metals require different sand characteristics due to their melting points and reactivity:
- Ferrous Alloys (Iron, Steel):
These metals pour at high temperatures, often above 1,400 °C, demanding sands with excellent refractoriness, metal penetration resistance, and thermal stability.
Common choices include:
-
- Chromite sand – superior thermal conductivity and resistance to fusion
- High-purity silica sand – economical and widely available, with moderate refractoriness
- Non-Ferrous Alloys (Aluminum, Copper, Zinc):
These cast at lower temperatures (600–1,100 °C) and are more sensitive to gas defects and surface roughness. Ideal sand systems include:
-
- Zircon sand – low thermal expansion and excellent surface finish
- Fine-grained silica sand – cost-effective and capable of high detail resolution
Based on Casting Complexity
- Simple Shapes: Green sand can be a cost – effective choice due to its ease of molding.
- Complex Shapes: Chemically bonded sands (especially Cold – Box) or resin – coated sands for shell molding are preferred for their precision and detail – holding capabilities.
Based on Production Volume
- Low – Volume Production: Green sand is popular due to its low cost and reusability.
- High – Volume Production: Chemically bonded sands (Cold – Box) or resin – coated sands offer consistent quality and faster cycle times, despite higher initial costs.
9. Sand Reclamation and Recycling in Sand Casting
Importance of Sand Reclamation
- Environmental: Reduces demand for virgin sand, conserving natural resources, and minimizing landfill waste.
- Economic: Cuts down on sand procurement and disposal costs, providing significant savings for foundries.
Reclamation Techniques
- Physical Reclamation: Mechanical processes like screening, attrition, and scrubbing to remove binders and contaminants. Suitable for sands with simple binders (e.g., green sand).
- Thermal Reclamation: Uses heat to burn off binders and organic contaminants. More effective for complex binders but requires more energy and is costlier.
Reclaimed Sand vs. Virgin Sand
Reclaimed sand may have slightly different properties, such as grain size and binder content. However, with proper quality control, it can meet the requirements for many casting applications.
Environmental Impacts and Cost – Benefit Analysis
While reclamation has some environmental impacts (e.g., energy use in thermal reclamation), the overall environmental benefit outweighs the impact of using only virgin sand.
Economically, the savings from reclamation usually exceed the investment in equipment and processes.
10. Future Trends in Sand for Sand Casting
Development of New Sand Materials
- Research efforts to develop new types of sand with enhanced properties, such as improved refractoriness, lower thermal expansion, and better environmental compatibility.
- The exploration of alternative materials to traditional sand types, such as synthetic sands or sands derived from waste materials.
Advancements in Binder Technology
- The development of more environmentally friendly binders with lower emissions and better performance.
- How new binder technologies can improve the strength, permeability, and other properties of sand molds and cores, leading to higher – quality castings.
Automation in Sand Handling and Processing
- The increasing use of automation in sand casting processes, including sand mixing, molding, and reclamation.
- How automation can improve the consistency and efficiency of sand handling, reduce labor costs, and enhance the overall quality of the casting process.
11. Conclusion
Selecting the right sand type forms the foundation of successful sand casting.
From versatile green sand to precision resin‑coated shells, each system delivers unique advantages and trade‑offs.
By understanding sand composition, key properties, and reclamation strategies, foundry engineers ensure high‑quality castings, economical production, and environmental stewardship.
As sand technology advances—embracing eco‑friendly binders, digital process control, and additive manufacturing—sand casting will continue powering innovative applications across diverse industries.