1. Introduction
In engineering environments where sub-zero performance is critical, material reliability cannot be compromised.
ASTM A352 is a widely recognized specification developed by ASTM International that addresses this very concern—covering cast carbon and low-alloy steels intended for pressure-containing parts that operate in low-temperature service conditions.
These steels are essential in industries such as LNG, cryogenics, oil and gas, and power generation, where mechanical integrity under cold stress is non-negotiable.
This article provides a comprehensive analysis of ASTM A352, exploring its metallurgical principles, mechanical requirements, applications, and manufacturing implications
to support engineers, specifiers, and procurement professionals in making informed material choices.
2. Scope and Purpose of ASTM A352
ASTM A352 covers castings for pressure-retaining parts designed to operate at low temperatures down to -50°F (-46°C) or even lower, depending on the grade.

It ensures that the cast steel maintains ductility, toughness, and resistance to brittle fracture when exposed to these demanding environments.
Unlike ASTM A216 (for general-purpose cast carbon steels) or A351 (for corrosion-resistant austenitic stainless castings), A352 is tailored to low-temperature applications.
It is frequently dual certified with ASME SA352, making it suitable for pressure vessel and piping code compliance.
3. Classification of ASTM A352 Grades
ASTM A352 includes a range of cast carbon and low-alloy steel grades specifically engineered for low-temperature service in pressure-containing components.
The classification is based on chemical composition, mechanical performance, and service conditions.

These grades are broadly grouped into carbon steels, low-alloy steels, and martensitic stainless steels, each tailored to meet specific operational demands.
Below is a detailed classification of the most common ASTM A352 grades:
| Grade | Type | Primary Alloying Elements | Typical Service Temperature (°C) | Common Applications |
|---|---|---|---|---|
| LCA | Carbon Steel | Mn, C | Down to -46°C | Low-temp pipe fittings, flanges |
| LCB | Carbon Steel (Enhanced) | Ni (~0.5%), Mn, C | Down to -46°C | Valve bodies, actuator housings |
| LCC | Carbon Steel (High Impact) | Ni (~1.0%), Mn, C | Down to -46°C | Pressure-retaining parts, cryogenic valves |
| LC1–LC9 | Low-Alloy Steels | Varies: Ni, Cr, Mo, Cu | -46°C to -100°C+ (depending on alloy) | Specialty pressure equipment in harsh environments |
| CA6NM | Martensitic Stainless Steel | 13Cr, 4Ni | Down to -60°C | Steam turbine parts, seawater valves |
UNS Number Mapping
Each ASTM A352 grade also has a corresponding Unified Numbering System (UNS) designation to support traceability and alloy standardization:
- LCA – UNS J03000
- LCB – UNS J03001
- LCC – UNS J03002
- CA6NM – UNS J91540
Comparison to Wrought Equivalents
While ASTM A352 governs cast products, many of its grades can be loosely compared to wrought steel specifications used in similar applications. For example:
- A352 LCC roughly parallels ASTM A350 LF2 (forged carbon steel)
- CA6NM is metallurgically similar to wrought 13-4 stainless steel (AISI 410 with Ni)
4. Chemical Requirements
The table summarizes typical maximum and minimum composition ranges:
| Element | LCB (%) | LCC (%) | LC1/LC2 (%) | LCB-CR (%) | Function |
|---|---|---|---|---|---|
| Carbon (C) | 0.24 – 0.32 | 0.24 – 0.32 | 0.24 – 0.32 | 0.24 – 0.32 | Base strength and hardness |
| Manganese (Mn) | 0.60 – 1.10 | 0.60 – 1.10 | 0.60 – 1.10 | 0.60 – 1.10 | Deoxidation, grain refinement |
| Silicon (Si) | 0.40 – 0.60 | 0.40 – 0.60 | 0.40 – 0.60 | 0.40 – 0.60 | Fluidity, deoxidation |
| Phosphorus (P) | ≤ 0.025 | ≤ 0.025 | ≤ 0.025 | ≤ 0.025 | Control brittle segregation |
| Sulfur (S) | ≤ 0.015 | ≤ 0.015 | ≤ 0.015 | ≤ 0.015 | Control sulfide inclusions |
| Nickel (Ni) | – | – | – | 1.00 – 2.00 | Enhances low-temperature toughness (CR variant) |
| Chromium (Cr) | – | – | – | 0.25 – 0.50 | Corrosion/pitting resistance (CR variant) |
| Molybdenum (Mo) | – | – | – | 0.25 – 0.50 | Strength at elevated/low temperatures |
| Vanadium (V) | 0.05 – 0.15 | 0.05 – 0.15 | 0.05 – 0.15 | 0.05 – 0.15 | Grain refinement, tensile strength |
| Copper (Cu) | – | ≤ 0.40 | – | – | Improves as-cast machinability |
| Nitrogen (N) | ≤ 0.012 | ≤ 0.012 | ≤ 0.012 | ≤ 0.012 | Controlled to prevent blowholes |
| Aluminum (Al) | 0.02 – 0.05 (max) | 0.02 – 0.05 | 0.02 – 0.05 | 0.02 – 0.05 | Inclusion modification (deoxidizer) |
Influence of Alloying Elements on Low-Temperature Toughness
- Carbon (0.24–0.32%): A balance between strength and toughness; excessive carbon (> 0.32%) can increase hardness and reduce Charpy energy at −50 °F and below.
- Manganese (0.60–1.10%): Promotes deoxidation during melting and contributes to solid-solution strengthening.
Mn also helps refine pearlite/pearlitic-ferrite mixtures during heat treatment, improving toughness. - Nickel (1.00–2.00%) (LCB-CR only): Nickel significantly enhances curve shift (NDT shift) in the Charpy transition region, allowing steels to maintain ductile behavior at lower temperatures.
- Chromium (0.25–0.50%) and Molybdenum (0.25–0.50%): These elements combine to form carbides (Cr₇C₃, Mo₂C) that retard grain growth during heat treatment and improve hardenability,
thereby improving both tensile strength and low-temperature toughness. - Vanadium (0.05–0.15%): Acts as a potent grain refiner by forming fine VC precipitates, which pin austenite grain boundaries during casting and heat treatment.
A finer grain size (ASTM 6–8) directly correlates with higher Charpy V-notch energy at cryogenic temperatures.
5. Physical Properties
Density and Thermal Conductivity
- Density: Approximately 7.80 g/cm³ (0.283 lb/in³) for all A352 grades, since the alloying additions (Mo, Ni, Cr, V) are relatively minor (≤ 3% total).
- Thermal Conductivity:
-
- As-Cast: ~ 30 W/m·K at 20 °C.
- Normalized/Tempered: Slightly reduced (~ 28 W/m·K) due to finer grain structure and tempered carbides.
- Cryogenic Effect: At −100 °C, conductivity rises modestly (to ~ 35 W/m·K) because phonon scattering decreases,
which can be beneficial for applications requiring rapid heat transfer (e.g., cryogenic valves).
Coefficient of Thermal Expansion (CTE) at Cryogenic Temperatures
- CTE (20 °C to −100 °C): ~ 12 × 10⁻⁶ /°C
- CTE (−100 °C to −196 °C): ~ 11 × 10⁻⁶ /°C
Compared to austenitic stainless steels (≈ 16 × 10⁻⁶ /°C), A352 cast steel exhibits lower thermal expansion, which is advantageous when bolting or sealing with materials having similar CTEs (e.g., carbon steels).
Designers must still account for differential expansion when mating with aluminum or copper alloys, especially in cryogenic applications.
6. Mechanical Properties of ASTM A352 Cast Steels
ASTM A352 cast steels are specifically engineered for applications requiring high strength and excellent toughness at low or cryogenic temperatures. The mechanical properties vary slightly among the grades based on chemical composition and heat treatment processes. Below is a comparison of several commonly used A352 grades.

Typical Mechanical Properties by Grade
| Grade | Type | Tensile Strength (MPa / ksi) | Yield Strength (MPa / ksi) | Elongation (%) | Impact Energy at −46°C (J / ft-lb) | Hardness (HB) |
|---|---|---|---|---|---|---|
| LCA | Carbon Steel | 415 min (60 ksi) | 240 min (35 ksi) | 22 min | 27 J (20 ft-lb) | 170–207 |
| LCB | Carbon Steel | 485–655 (70–95 ksi) | 250 min (36 ksi) | 22 min | 27 J (20 ft-lb) | 170–229 |
| LCC | Carbon Steel | 485–655 (70–95 ksi) | 250 min (36 ksi) | 22 min | 27 J (20 ft-lb) | 170–229 |
| LC2 | Low Alloy Steel | 485–655 (70–95 ksi) | 275 min (40 ksi) | 20 min | 27 J (20 ft-lb) | 179–229 |
| LC2-1 | Low Alloy Steel | 550–690 (80–100 ksi) | 310 min (45 ksi) | 20 min | 27 J (20 ft-lb) | 197–235 |
| LC3 | Low Alloy Steel | 585–760 (85–110 ksi) | 310 min (45 ksi) | 20 min | 27 J (20 ft-lb) | 197–241 |
CA6NM |
13% Cr, 4% Ni Martensitic SS | 655–795 (95–115 ksi) | 450–550 (65–80 ksi) | 15–20 | 40–120 J (30–90 ft-lb) depending on heat treatment | 200–240 |
| CA15 | 13% Cr Martensitic SS | 620–760 (90–110 ksi) | 450 min (65 ksi) | 15–20 | 20–40 J (15–30 ft-lb) | 200–240 |
| CF8M | Austenitic Stainless (316 type) | 485 min (70 ksi) | 205 min (30 ksi) | 30 min | Not typically used for impact service | 150–180 |
| CD4MCuN | Duplex Stainless Steel | 655–795 (95–115 ksi) | 450 min (65 ksi) | 20–25 | 70–100 J (50–75 ft-lb) | 200–250 |
Notes on Special Grades
- CA6NM: Widely used in hydroelectric turbines, valve bodies, and pump casings for its excellent cavitation resistance, weldability, and impact toughness at subzero temperatures.
- CA15: Offers good hardness and corrosion resistance but lower impact toughness than CA6NM, making it more suitable for moderate-pressure environments.
- CF8M (316 equivalent): Although not typically part of A352, it is often cast under ASTM A743 and used in corrosive but non-low-temperature conditions.
- CD4MCuN: A duplex stainless grade with a strong balance of corrosion resistance, strength, and impact performance; ideal for aggressive environments like chloride-bearing solutions.
7. Casting and Manufacturing Processes of ASTM A352 Cast Steels
Casting Process Overview
ASTM A352 cast steels are typically produced using sand casting or investment casting, with the choice depending on the complexity, size, and required tolerances of the part.

- Sand Casting: This remains the most common method for producing large valve bodies, pump housings, and flanges specified under ASTM A352.
It offers cost-effective flexibility for intricate shapes and thick sections.
However, it requires meticulous control of mold materials and pouring parameters to minimize defects such as porosity and shrinkage. - Investment Casting: For smaller, more complex components requiring superior surface finish and dimensional precision, investment casting is sometimes employed.
This method yields fewer casting defects and reduces machining allowances, albeit at higher costs.
Heat Treatment
Post-casting, ASTM A352 steels undergo stringent normalizing and tempering to enhance mechanical properties:
- Normalizing: Typically performed at 900–950°C, normalizing refines grain structure, relieves internal stresses, and improves toughness.
- Tempering: Carried out at 600–700°C, tempering balances strength and ductility while reducing brittleness.
- Heat treatment cycles are strictly monitored and documented to ensure compliance with ASTM specifications and to achieve uniform mechanical properties throughout the casting.
Machining and Finishing
Due to complex geometries, cast ASTM A352 components often require machining to achieve final dimensions and tolerances. This includes:
- CNC machining for valve seats, flanges, and critical sealing surfaces.
- Surface treatments such as grinding and polishing to enhance corrosion resistance and sealing performance.
- Machining parameters are optimized based on steel grade and hardness to minimize tool wear and surface defects.
8. Advantages and Limitations of ASTM A352 Cast Steels
ASTM A352 cast steels are widely used in critical applications where strength, toughness, and resistance to low-temperature embrittlement are essential.

Advantages of ASTM A352 Cast Steels
Superior Low-Temperature Toughness
ASTM A352 grades—particularly LCA, LCB, and LCC—are specifically designed for cryogenic and sub-zero service.
With minimum Charpy V-notch impact energy requirements of 27 J at −46°C, these materials ensure structural integrity and reduce the risk of brittle fracture under extreme conditions.
Excellent Pressure Retention
Due to their mechanical strength and ductility, A352 cast steels are ideally suited for pressure-containing parts, such as valves, pumps, and flanges.
Grades like CA6NM also offer enhanced yield strength (>550 MPa), supporting higher-pressure system designs.
Good Castability
The A352 specification covers cast steel components, allowing for complex geometries and near-net-shape manufacturing.
This flexibility reduces the need for extensive machining and enables the production of intricate internal passageways or housings that are otherwise impractical to forge or machine.
Versatility Across Industries
A352 castings are used in diverse sectors—including oil & gas, petrochemical, power generation,
and cryogenics—due to their mechanical reliability, dimensional accuracy, and performance in low-temperature or high-pressure conditions.
Corrosion and Wear Resistance (in Alloyed Grades)
Alloy grades like CA6NM offer a combination of corrosion resistance and moderate hardness (200–260 HBW),
making them suitable for service in wet, acidic, or saline environments, such as subsea equipment or chemical plants.
Standards-Based Assurance
Being governed by ASTM standards, these castings are subjected to rigorous quality controls—covering heat treatment, chemical composition, and mechanical testing—which ensures global reliability and traceability.
Limitations of ASTM A352 Cast Steels
Casting Defects and Variability
As with any casting process, shrinkage cavities, porosity, or inclusions may occur. These defects, if not identified and corrected, can compromise mechanical performance.
Advanced inspection methods like radiography and ultrasonic testing are often required for critical parts.
Lower Toughness Compared to Forged Materials
Despite good ductility, cast steels generally exhibit lower fracture toughness than wrought or forged equivalents due to grain structure and potential casting flaws.
This may limit their use in ultra-critical fatigue environments.
Heat Treatment Sensitivity
Proper normalizing and tempering are essential to achieve the required mechanical properties.
Inadequate or uneven heat treatment can lead to residual stress, distortion, or even microcracking—particularly in thick or complex castings.
Weldability Concerns
Some grades, particularly alloyed steels (e.g., CA6NM), may require strict welding procedures, including preheating, post-weld heat treatment (PWHT),
and filler metal selection to avoid embrittlement or degradation of corrosion resistance.
Limited Corrosion Resistance in Carbon Grades
Grades such as LCA, LCB, and LCC have limited inherent corrosion resistance.
They often require coatings, lining, or external protection when used in aggressive environments or for long-term service.
Cost Considerations in Alloyed Versions
High-alloy grades like CA6NM or LC3 involve increased costs due to alloying elements (Cr, Ni, Mo) and more demanding casting and heat treatment processes.
9. Applications and Case Studies
Cryogenic Vessels and LNG Storage
- LCB and LCC Valve Bodies:
-
- LNG infrastructure demands valves that remain ductile at −162 °C (−260 °F).
While LCC’s −100 °F CVN rating does not ensure full ductility at −260 °F, it provides a safety margin above the brittle–ductile transition. - Case Study: An LNG terminal in Northern Europe replaced A216 WCB valve bodies (which fractured during cooldown tests) with A352 LCC castings.
Post-installation, no low-temperature fissures were observed after 500 thermal cycles.
- LNG infrastructure demands valves that remain ductile at −162 °C (−260 °F).

Oil & Gas: Valves, Flanges, and Couplings
- Sour Service (H₂S Environment):
-
- LCB-CR castings with 1.5% Ni, 0.35% Cr, and 0.30% Mo exhibit improved resistance to sulfide stress cracking (SSC).
- Case Study: Offshore wellhead assemblies in the North Sea transitioned from 13% Cr stainless steel to LCB-CR for some low-pressure components,
reducing material cost by 20% without sacrificing sour gas compliance (NACE MR0175).
Power Generation: Steam and Boiler Components
- Feedwater Pump Housings:
-
- Operating at −20 °C and low-pressure steam, LCB castings replaced older A216 WCB flanged housings.
Resulted in a 30% weight reduction and improved fatigue life due to finer microstructure. - Case Study: A combined-cycle power plant in Japan reported zero lap joints or core shift defects after implementing meticulous gating and chill practices for A352 LCB turbine bleed valve bodies.
- Operating at −20 °C and low-pressure steam, LCB castings replaced older A216 WCB flanged housings.
Petrochemical Reactors and Pressure Vessels
- Sub-Cooled Liquid Ethylene Pumps:
-
- Ethylene plants store and pump ethylene at −104 °C.
LCC pump casings ensured sufficient margin above the −73 °C certification, maintaining Charpy energy of 20 J at −104 °C during third-party inspection. - Case Study: A U.S. Gulf Coast ethylene complex deployed LCC reactor nozzles.
Over 150,000 hours of service with no brittle fractures, even when unplanned warm-up to −50 °C was required during maintenance.
- Ethylene plants store and pump ethylene at −104 °C.
10. Comparison to Other Standards
When selecting materials for critical applications, understanding how ASTM A352 cast steels compare to other relevant standards is essential.
| Standard | Material Type | Temperature Range | Corrosion Resistance | Typical Applications | Key Characteristics |
|---|---|---|---|---|---|
| ASTM A352 | Carbon & Low-Alloy Cast Steels | Cryogenic to ambient (down to −46°C and below) | Moderate (alloy dependent) | Valves, pumps, pressure vessels | Excellent low-temperature toughness; heat treated |
| ASTM A216 | Carbon Steel Castings | Ambient to high temperature | Low | General pressure-containing parts | Cost-effective; not suitable for cryogenic service |
| ASTM A351 | Austenitic Stainless Steel | Ambient to high temperature | High | Corrosive environments | Superior corrosion resistance; less low-temp toughness |
ASTM A217 |
Alloy Steel Castings (Chromium-Molybdenum) | High temperature (up to ~1100°F / 593°C) | Moderate to high | High-temperature valve and pump parts | Designed for elevated temperature service; good strength & creep resistance |
| API 6A | Carbon & Alloy Steel | Oil & gas wellhead service | Variable | Oilfield equipment | Meets stringent oilfield service requirements |
| EN 10213 | Carbon & Low-Alloy Cast Steels | Similar to ASTM A352 | Moderate | Pressure vessels and valves | European standard equivalent |
| JIS G5121 | Carbon & Low-Alloy Cast Steels | Similar to ASTM A352 | Moderate | Pressure components | Japanese standard equivalent |
11. Emerging Trends and Future Developments
Advanced Metallurgy: Cleaner Steelmaking and Grain Refinement
- Microalloying with Niobium (Nb) and Titanium (Ti):
-
- Nb and Ti form (Nb,Ti)C precipitates that pin grain boundaries more effectively than V alone, leading to ASTM 9–10 grain sizes even in large-section castings.
- Improved cryogenic toughness (CVN ≥ 30 J at −100 °F for LCC) demonstrated in prototype trials.
- Vacuum Arc Remelting (VAR):
-
- For critical nuclear or deep-cryogenic castings, VAR eliminates dissolved gases and reduces inclusion content to < 1 ppm—yielding near-impervious components with CVN > 45 J at −150 °F (−100 °C).
Additive Manufacturing (AM) for Low-Temperature Steel Components
- Electron-Beam Melting (EBM) and Selective Laser Melting (SLM) of Nickel–Iron–Chromium powders allow near-net-shape production of small,
intricate components (e.g., cryogenic sensor housings) traditionally made from A352 castings. - Hybrid Casting–AM: Using AM to produce molds with conformal cooling channels accelerates cycle times and improves microstructural homogeneity in castings.
Foundry trials show reduced porosity and improved CVN by 15 %.
Digital Casting: Simulation and Quality Control
- Computational Fluid Dynamics (CFD):
-
- Virtual gating design to optimize metal flow, reducing turbulence-related defects.
- Prediction of solidification shrinkage and porosity using finite-element analysis (FEA).
- Real-Time Monitoring:
-
- Embedding thermocouples and pressure transducers in molds provides instantaneous feedback on pour temperature and pressure, allowing closed-loop control to correct anomalies on the fly.
- Machine Learning (ML) for Defect Prediction:
-
- ML algorithms trained on historic casting data predict defective castings (> 90% accuracy) based on real-time sensor inputs (temperature gradient, gating pressure, furnace emissions).
Novel Coatings and Surface Treatments for Extreme Environments
- Nanocomposite Coatings:
-
- Ti-Al-N and CrN PVD coatings applied to internal passages of A352 castings demonstrate 300 % longer erosion life in cryogenic gas flows containing particulate matter.
- Self-Healing Epoxy Liners:
-
- Incorporation of microencapsulated healing agents that release polymers upon micro-crack formation, sealing pinholes in cryogenic piping without manual maintenance.
- Diamond-Like Carbon (DLC):
-
- DLC coatings on pump impeller surfaces reduce friction and cavitation in LNG pumps, extending MTBF by 40%.
12. Conclusion
ASTM A352 is an essential material specification for engineers designing components exposed to low-temperature and high-pressure service.
Whether it’s in a cryogenic LNG terminal or an Arctic offshore platform, A352 grades like LCC, LCB, and CA6NM provide the strength, toughness, and reliability demanded by modern infrastructure.
By understanding its metallurgical nuances, fabrication requirements, and application relevance, industry professionals can confidently select and specify the right casting grade for safe, long-term performance.
FAQs
What is ASTM A352 used for?
ASTM A352 is primarily used for manufacturing cast steel components such as valves, pumps, and pressure vessels designed for low-temperature or cryogenic service.
Its high toughness and strength make it ideal for demanding industrial environments like chemical processing and power generation.
Can ASTM A352 castings be welded?
Yes, ASTM A352 cast steels can be welded.
Proper preheating, inter-pass temperature control, and post-weld heat treatment are recommended to maintain mechanical properties and avoid cracking.
Are ASTM A352 cast steels corrosion resistant?
ASTM A352 steels offer moderate corrosion resistance, which can be improved through surface treatments or coatings, depending on the service environment.