Material Strength Tests

Six Common Material Strength Tests

Material strength plays a pivotal role in determining how a material will behave under different stresses and conditions.

Whether you’re designing a building, a machine part, or an entire structure, knowing how a material will perform under force is crucial.

Different types of material tests are used to measure different kinds of strength, and each test serves a unique purpose.

Below are six common material strength tests, highlighting their methodologies, key measurements, and applications.

1. Tensile Testing

Tensile testing is one of the most widely used methods for assessing the mechanical properties of materials, especially their ability to withstand stretching or pulling forces.

This test involves applying a gradually increasing tensile load to a material sample (usually shaped like a dumbbell) until it breaks.

By recording the applied load, elastic modulus, yield strength, tensile strength, ductility, strain hardening properties, Young’s modulus, and Poisson’s ratio can be calculated.

The test is carried out using a tensile testing machine, also known as a universal testing machine (UTM).

Tensile Testing
Tensile Testing

Key Parameters Measured:

  • Yield Strength: The stress point at which a material begins to deform plastically (permanent deformation). For example, for low-carbon steel, the yield strength is typically around 250 MPa.
  • Ultimate Tensile Strength (UTS): The maximum stress a material can withstand before breaking.
    Steel, for instance, might have a UTS ranging from
    400 MPa to 700 MPa depending on the alloy.
  • Elastic Modulus (Young’s Modulus): The ratio of stress to strain within the elastic region, indicating material stiffness. For steel, Young’s Modulus is typically 200 GPa.
  • Elongation: The percentage of increase in length of the material before it breaks. Materials with high elongation, such as ductile steel, can elongate by more than 10% before failure.

Tensile testing is essential for materials used in structural components, such as metals, plastics, and composite materials.
It provides valuable data on how materials will behave under tension in real-world applications, from cables in bridges to components in airplanes.

2. Compressive Testing

Compressive testing evaluates a material’s ability to withstand compressive forces — forces that push or squeeze the material.
The test is particularly useful for brittle materials, such as concrete, ceramics, and some metals.

In this test, a material sample is placed in a compressive testing machine, where a load is applied until the material deforms or fails.

Compressive Testing
Compressive Testing

Key Parameters Measured:

  • Compressive Strength: The maximum compressive load a material can bear before failure occurs.
    For example, concrete typically has a compressive strength of
    20-40 MPa, while high-strength concrete can exceed 100 MPa.
  • Crushing Strength: The point at which brittle materials fracture under compression.
    This is relevant for materials such as ceramics or castings, which may break at relatively low compressive forces compared to ductile materials.

Compressive testing is especially important in construction and civil engineering, where materials like concrete and steel columns are designed to support significant loads.

This test ensures that materials can bear heavy structural loads without failure.

3. Fatigue Testing

Fatigue testing is critical for materials that are subjected to cyclic or repetitive loads, such as those found in machinery, automotive components, and aircraft.

Materials can often endure high levels of stress but may fail under repeated cycles of loading and unloading.

In a fatigue test, a material is subjected to repeated cycles of stress until it eventually fails.

The test simulates real-world conditions, where parts are subjected to fluctuations in load over time, such as engine parts in a car or turbine blades in an aircraft engine.

Key Parameters Measured:

  • Fatigue Strength: The maximum stress a material can endure for a given number of cycles before failure.
    For example, steel components in automotive parts might have a fatigue strength of around
    250 MPa.
  • S-N Curve (Stress vs. Number of Cycles): This curve plots the relationship between the applied stress and the number of cycles a material can withstand before failure.
    Materials like titanium alloys are known for having high fatigue strength, making them suitable for aerospace applications.

Fatigue testing is vital in industries where components experience cyclical stresses, including automotive, aerospace, and manufacturing, where parts need to endure millions of loading cycles without failure.

4. Torsion Testing

Torsion testing measures a material’s ability to withstand twisting or rotational forces. The material is fixed at one end, and a torque is applied to the other end, causing it to twist.

This test provides insight into the material’s shear strength, plastic deformation characteristics, and response to rotational stresses.

Torsion Testing
Torsion Testing

Key Parameters Measured:

  • Shear Strength: The material’s ability to resist shearing forces. For instance, steel typically has a shear strength of around 300 MPa, while softer materials like aluminum may have lower shear strengths.
  • Torsional Modulus: The material’s resistance to twisting, which helps in determining the overall stiffness of materials used in rotating components like shafts.
  • Plastic Deformation: The degree of permanent twisting or deformation before the material breaks.
    Ductile materials will undergo significant twisting before failure, while brittle materials fail quickly after small amounts of deformation.

Torsion testing is crucial for evaluating materials used in components like shafts, bolts, and pipes that experience rotational forces in machinery, automotive, and aerospace applications.

5. Nick Break Testing

Nick break testing is a specialized impact test primarily used to evaluate the strength of welded joints.

A small notch is created in the welded area, and then the sample is struck with an impact force.

The fracture typically occurs at the welded joint and the way the material fractures can indicate the quality of the weld.

Nick Break Testing
Nick Break Testing

Key Parameters Measured:

  • Weld Strength: This measures the ability of the welded joint to resist fracture under impact. Strong welds will exhibit minimal fracture and maximum energy absorption.
  • Impact Toughness: The ability of the material to absorb energy before failing. Materials with high toughness will resist brittle fracture even in harsh conditions.

This test is essential for industries that rely on welding for structural integrity, such as shipbuilding, construction, and pipeline manufacturing.

6. Creep Testing

Creep testing evaluates how a material deforms under a constant load over an extended period, especially at high temperatures.

For materials exposed to long-term stresses, such as in power plants or aerospace engines, understanding creep behavior is crucial.

During the test, a material is subjected to constant stress at an elevated temperature, and the amount of deformation (creep) is measured over time.

Creep Testing
Creep Testing

Key Parameters Measured:

  • Creep Rate: The rate at which the material deforms under stress over time. Materials like superalloys used in jet engines often have very low creep rates to ensure performance at high temperatures.
  • Creep Strength: The material’s ability to resist deformation under sustained stress at high temperatures.
  • Time-Temperature-Transformation (TTT) Curve: This curve shows how temperature and time affect the material’s creep rate.

Creep testing is particularly important in high-temperature applications such as turbines, engines, and reactors, where materials must withstand prolonged thermal and mechanical stresses without failure.

Conclusion

These six strength tests — tensile, compressive, fatigue, torsion, nick break, and creep — provide crucial insights into how materials will perform under different types of stress.

Each test serves a unique purpose, whether assessing a material’s resistance to tension, compression, cyclic stress, twisting forces, or high-temperature deformation.

By understanding the strengths and weaknesses of materials through these tests, engineers can make more informed decisions when selecting materials for specific applications.

Ensuring safety, durability, and reliability across a range of industries.

 

How to order products from Deze?

To ensure efficient processing and production, we recommend providing detailed drawings of the required products.
Our team works primarily with software such as SolidWorks and AutoCAD, and we can accept files in the following formats: IGS, STEP, as well as CAD and PDF drawings for further evaluation.
If you do not have ready-made drawings or designs, simply send us clear pictures with the main dimensions and the unit weight of the product.
Our team will assist you in creating the necessary design files using our software.

Alternatively, you can send us a physical sample of the product. We offer 3D scanning services to generate accurate designs from these samples.
This service is offered free of charge, and we’re happy to support you throughout the process to ensure the best results.

Whatever your needs, please contact us.