AISI 316 vs. EN 1.4581 Stainless Steel

AISI 316 vs. EN 1.4581 Stainless Steel

1. Introduction

Stainless steel is a vital material in many industries due to its remarkable corrosion resistance, strength, and versatility.

Among the numerous grades available, AISI 316 and EN 1.4581 are two widely used stainless steels, known for their ability to perform in harsh environments.

Choosing the right grade is critical to ensuring optimal performance, longevity, and cost-effectiveness in various applications.

This blog will provide a comprehensive comparison of AISI 316 and EN 1.4581 stainless steel, examining their chemical composition, properties, and applications to help readers make an informed decision.

2. What is AISI 316 Stainless Steel?

AISI 316, often referred to as marine-grade stainless steel, is renowned for its excellent corrosion resistance, particularly in environments rich in chlorides, such as marine and coastal applications.

This stainless steel contains 16-18% chromium, 10-14% nickel, and 2-3% molybdenum, which enhances its ability to resist pitting and crevice corrosion.

It was first developed to address the shortcomings of other stainless steels in demanding conditions, making it a material of choice in industries like chemical processing, pharmaceuticals, and food production.

AISI 316 stainless steel plate
AISI 316 stainless steel plate

AISI 316 is regulated by standards such as ASTM A240 and ISO 9444, ensuring consistency in quality and performance across various applications.

Its low-carbon variant, 316L, offers additional resistance to sensitization, particularly in welded structures, making it a popular option for applications requiring extensive welding.

3. What is EN 1.4581 Stainless Steel?

EN 1.4581 stainless steel is a cast version of stainless steel similar to AISI 316 but specifically designed for applications requiring casting.

It shares a similar chemical makeup—chromium, nickel, and molybdenum—but is produced in cast form, making it ideal for complex, intricate shapes that cannot be easily produced using wrought stainless steel.

EN 1.4581 is commonly referred to under casting standards such as ASTM CF8M and EN 10213,

making it suitable for industrial components like pumps, valves, and fittings that need to withstand high-stress and corrosive environments.

EN 1.4581 Stainless Steel
EN 1.4581 Stainless Steel

Due to its casting nature, EN 1.4581 is slightly less ductile compared to its wrought counterpart,

but it offers enhanced corrosion resistance and strength, especially in high-temperature environments or aggressive industrial settings.

4. Chemical Composition Comparison

The chemical composition of AISI 316 and EN 1.4581 is very similar, with both grades containing significant amounts of chromium, nickel, and molybdenum.

However, there are subtle differences that can influence their performance in specific applications.

For instance, EN 1.4581 typically has a slightly higher carbon content compared to AISI 316L (low-carbon version), which may affect its corrosion resistance in welded components.

Element AISI 316 (Wrought) EN 1.4581 (Cast)
Carbon 0.08% max 0.08% max
Chromium 16-18% 16-18%
Nickel 10-14% 10-14%
Molybdenum 2-3% 2-3%

The addition of molybdenum in both alloys significantly improves resistance to chloride-induced corrosion.

This composition makes both materials well-suited for environments where exposure to saltwater or corrosive chemicals is a concern.

5. Mechanical and Physical Properties

When comparing the mechanical properties of AISI 316 and EN 1.4581, it is important to consider their form—wrought versus cast.

Generally, AISI 316 has better elongation and ductility, which makes it easier to form and work within applications requiring bending or shaping.

EN 1.4581, being a cast material typically exhibits higher strength but lower ductility, which is expected in cast components.

Tensile and Yield Strength

  • AISI 316: Tensile strength of approximately 515 MPa, yield strength of 205 MPa.
  • EN 1.4581: Tensile strength can vary from 485 MPa to 620 MPa, with yield strength typically around 240 MPa, depending on the casting process and heat treatment.

Hardness

  • Both grades have comparable hardness values, with EN 1.4581 being slightly harder due to its cast structure, making it more resistant to wear in heavy-duty applications.

Physical Properties

  • Density: Both grades have a similar density of around 8 g/cm³.
  • Thermal Expansion: Slightly higher in EN 1.4581 due to the casting process, affecting its performance in high-temperature environments.

6. Corrosion Resistance

One of the most significant advantages of AISI 316 vs. EN 1.4581 stainless steel is its corrosion resistance.

AISI 316 is particularly resistant to chloride-induced corrosion, making it ideal for marine environments, swimming pool equipment, and chemical processing plants.

EN 1.4581 offers similar corrosion resistance, with the added benefit of being used in cast form for complex parts exposed to aggressive environments.

Both grades perform exceptionally well in environments with high acidity or exposure to chlorides.

However, the slightly higher carbon content in EN 1.4581 may reduce its resistance to intergranular corrosion when compared to the low-carbon version of AISI 316, especially in welded components.

7. Weldability and Machinability

Welding AISI 316 is straightforward, particularly when using the low-carbon variant, 316L, which minimizes the risk of sensitization and subsequent intergranular corrosion.

The material’s good formability and ductility also make it easier to work with for various welding techniques such as TIG, MIG, and arc welding.

EN 1.4581, while cast, also offers reasonable weldability but requires more careful control of heat input during welding to prevent cracking in the heat-affected zone (HAZ).

It is slightly more challenging to machine due to its cast structure, which is more brittle than wrought stainless steel, but with proper tooling and cooling, it can be processed effectively.

8. Casting vs. Wrought Form

EN 1.4581: Predominantly Used in the Cast Form

EN 1.4581, often associated with casting applications, leverages the inherent benefits of the casting process to create components with intricate designs and complex geometries.
Here’s why casting is significant for EN 1.4581:

  • Complex Shapes: Casting allows for the production of parts with detailed internal structures and external contours that would be difficult or impossible to achieve through traditional forging or rolling processes.
  • Customization: The casting process enables the creation of custom-designed components tailored to specific requirements,
    making it ideal for industries such as marine engineering and pump manufacturing where bespoke solutions are needed.
  • Consistency: Through controlled casting procedures, it’s possible to maintain consistent quality and properties throughout the component, ensuring reliability in critical applications.
  • Reduced Waste: Casting often results in less material waste compared to cutting and shaping wrought materials, making it a more efficient and potentially cost-effective option.
EN 1.4581 Stainless Steel castings
EN 1.4581 Stainless Steel castings

AISI 316: Typically Found in Wrought Forms

On the other hand, AISI 316 is most commonly utilized in wrought forms such as plates, bars, and sheets. The advantages of using wrought AISI 316 include:

  • Versatility: Wrought forms allow for a wide range of applications, from structural components to decorative elements, making AISI 316 a flexible choice for diverse industries.
  • Strength and Durability: The process of working the material through rolling, drawing, or extrusion enhances the grain structure, resulting in increased strength and durability.
  • Ease of Fabrication: Wrought forms are easier to fabricate into final products via cutting, bending, and welding processes, facilitating streamlined manufacturing workflows.
  • Consistent Properties: Wrought AISI 316 exhibits uniform properties throughout the material, ensuring predictability and reliability in end-use applications.

When to Choose Casting Over Wrought Forms

Casting is particularly advantageous when:

  • The design requires complex geometries that cannot be achieved through conventional shaping methods.
  • Customized parts are needed for specialized applications where standard shapes and sizes are insufficient.
  • There is a need to optimize material usage and minimize waste during the production process.
  • The part must have a specific internal structure or intricate external shape that enhances functionality or performance.

When to Choose Wrought Forms Over Casting

Wrought forms are preferable when:

  • Standard shapes and sizes are sufficient for the application.
  • High strength and uniform properties are critical for the part’s performance.
  • Ease of fabrication and processing is a priority.
  • Cost-effectiveness and streamlined production are important considerations.

9. Applications of AISI 316 vs. EN 1.4581 Stainless Steel

Both AISI 316 and EN 1.4581 are used in a wide range of applications, although their form affects their suitability for specific uses.

AISI 316 Applications:

  • Food and beverage processing equipment: Due to its resistance to food acids and cleaning chemicals.
  • Pharmaceutical and medical devices: For sterile environments where corrosion resistance and hygiene are critical.
  • Chemical processing equipment: High resistance to corrosive chemicals and acids.
1/2 inch AISI 316 Stainless Steel Hex Nipple
1/2 inch AISI 316 Stainless Steel Hex Nipple

EN 1.4581 Applications:

  • Marine hardware: Excellent corrosion resistance in saltwater environments, ideal for shipbuilding and offshore equipment.
  • Industrial pumps and valves: High strength and durability in corrosive environments.
  • Fittings for chemical plants: Complex shapes and high resistance to corrosive materials.

10. Advantages and Disadvantages of AISI 316 vs. EN 1.4581 Stainless Steel

Advantages of AISI 316 Stainless Steel

AISI 316 shines in several areas, making it a versatile choice for a variety of applications:

  • Excellent Corrosion Resistance: AISI 316, with its molybdenum content, offers superior resistance to corrosion, particularly in environments rich in chlorides and acids.
    This makes it ideal for marine applications and chemical processing equipment where exposure to harsh chemicals is common.
  • Good Weldability: Known for its ability to be welded with minimal risk of sensitization, especially when using low-carbon variants like 316L, AISI 316 is favored in applications requiring strong joints and high integrity.
  • Formability: This grade is easily formed into various shapes and sizes, facilitating fabrication processes and allowing for intricate designs.
  • High-Temperature Performance: AISI 316 maintains its strength and resistance to corrosion even at elevated temperatures, making it suitable for use in high-heat environments such as power plants and oil refineries.

Advantages of EN 1.4581 Stainless Steel

EN 1.4581, while sharing many of the same beneficial properties as AISI 316, has certain advantages that make it a preferred choice for specific applications:

  • Castability: With its suitability for casting, EN 1.4581 enables the production of components with complex geometries and intricate designs, such as marine valves and pump parts.
  • Corrosion Resistance: Despite being designed primarily for casting, EN 1.4581 retains excellent corrosion resistance, particularly in environments prone to pitting and crevice corrosion.
  • Good Weldability and Machinability: While its primary use is in casting, EN 1.4581 also demonstrates good weldability and machinability, allowing for flexibility in fabrication methods.
  • Specific Applications: Its ability to be cast into precise shapes makes it ideal for industries requiring custom parts with high corrosion resistance, such as marine engineering and pharmaceutical machinery.

Disadvantages of AISI 316 Stainless Steel

Despite its many benefits, AISI 316 has some drawbacks that users should consider:

  • Cost: Due to its molybdenum content, AISI 316 tends to be more expensive than other stainless steel grades, which can increase the overall cost of projects.
  • Processing Challenges: The high strength and hardness of AISI 316 can pose difficulties during machining and forming processes, requiring specialized equipment and techniques.
  • Limited Applications: Although highly resistant to corrosion, there are environments where even AISI 316 may struggle, particularly in the presence of strong acids or under extremely high temperatures.

Disadvantages of EN 1.4581 Stainless Steel

EN 1.4581 also faces certain limitations that might influence its selection:

  • Cost: Similar to AISI 316, EN 1.4581 can be more costly than standard stainless steel due to its specific alloying elements and manufacturing processes.
  • Specialized Use: While its castability is an advantage, it also means that EN 1.4581 is not as widely applicable as grades like AISI 316, which are used more broadly across industries.
  • Processing Challenges: Although it offers good machinability, the specifics of casting can introduce complexities in terms of material handling and finishing processes.

11. Conclusion

To sum up, recognizing the key differences in the chemical composition, properties, and applications of AISI 316 vs. EN 1.4581 stainless steel is fundamental in selecting the proper stainless steel grade.

Whether you need the broad applicability of AISI 316 or the casting benefits of EN 1.4581, making an informed decision ensures optimal performance tailored to your specific requirements.

12. How to Purchase Stainless Steel Castings from DEZE?

To ensure efficient processing and production, we recommend providing detailed drawings of the required castings.

Our team works primarily with software such as SolidWorks and AutoCAD, and we can accept files in the following formats: IGS, STEP, as well as CAD and PDF drawings for further evaluation.

If you do not have ready-made drawings or designs, simply send us clear pictures with the main dimensions and the unit weight of the product.

Our team will assist you in creating the necessary design files using our software.

Alternatively, you can send us a physical sample of the product. We offer 3D scanning services to generate accurate designs from these samples.

This service is offered free of charge, and we’re happy to support you throughout the process to ensure the best results.

With over 20 years in the foundry industry, DEZE is here to meet your stainless steel casting needs. Contact us today!