Stainless Steel Glass Spigot Castings

Custom Stainless Steel Glass Spigot Castings

1. Introduction

Glass spigots are compact, visible hardware that play an outsized role in the safety, appearance and long-term performance of glass balustrades and pool fences.

When produced as precision castings in stainless steel, spigots combine integrated geometry, tight tolerances and attractive finishes that simplify installation and reduce visible joins.

2. What a Glass Spigot Is — and Why Castings Are Used

A glass spigot is a compact, usually stainless-steel fitting that anchors and clamps a single glass panel to a floor, deck, coping or substrate.

It is a common component in frameless balustrades, pool fences, stair guards and glazed barriers where a minimalist, frameless aesthetic is required while meeting safety and load requirements.

Stainless Steel Spigot Castings
Stainless Steel Spigot Castings

Why Casting Is the Preferred Manufacturing Method

Casting is the dominant process for producing glass spigots due to its unique advantages over alternative methods (stamping, machining, forging):

  • Complex Geometry Capability: Casting can integrate intricate features—such as internal threads, load-distributing ribs, and glass-seating grooves—in a single piece.
    This eliminates the need for assembly, reducing part count by 30–50% compared to machined spigots.
  • Dimensional Precision: Investment casting (the most common method for spigots) achieves tolerances of ±0.1–0.3 mm, critical for ensuring uniform glass alignment and load distribution.
  • Material Efficiency: Near-net-shape casting reduces material waste to 10–15% (vs. 20–30% for machining), lowering raw material costs.
  • Cost-Effectiveness for Customization: Casting enables low-to-medium volume production of custom spigot designs (e.g., branded or architect-specific profiles) without expensive tooling rework.
  • Structural Integrity: Castings have homogeneous grain structures, providing consistent tensile strength (≥500 MPa for 316L) across the component—critical for safety-critical applications.

3. Materials: Stainless Options and Their Trade-Offs

The choice of stainless steel grade is fundamental to the performance, durability, and appearance of a glass spigot casting.

Because these fittings are frequently exposed to chlorinated water, marine air, and outdoor weather, the selected alloy must balance corrosion resistance, mechanical strength, castability, and cost.

Common Stainless Steel Grades for Glass Spigot Castings

Alloy Grade Type / Microstructure Typical Composition (wt%) Corrosion Resistance Mechanical Strength Relative Cost Typical Applications
304 (CF8) Austenitic Cr 18–20, Ni 8–10.5 Good for indoor, mild outdoor 515 MPa (UTS) ★★☆☆☆ Interior railings, commercial interiors
316 / 316L (CF8M) Austenitic (Mo-bearing) Cr 16–18, Ni 10–14, Mo 2–3 Excellent in chloride & pool environments 520–620 MPa ★★★☆☆ Pool fences, outdoor façades, coastal projects
2205 Duplex
Duplex (austenite + ferrite) Cr 22, Ni 5–6, Mo 3, N 0.15 Superior resistance to pitting, stress corrosion, and fatigue 750–850 MPa ★★★★☆ Marine-grade spigots, coastal resorts, heavy-duty installations
2507 Super Duplex Duplex (super alloy) Cr 25, Ni 7, Mo 4, N 0.3 Outstanding resistance to seawater corrosion 800–900 MPa ★★★★★ Offshore, oceanfront, or chemical environments
17-4PH (AISI 630) Precipitation-hardening Cr 15–17, Ni 3–5, Cu 3–5 Moderate corrosion resistance, very high strength 1000–1200 MPa ★★★★☆ Heavy-duty structural clamps, high-load mounts

4. Manufacturing Routes: Investment Casting and Alternatives

The production of stainless steel glass spigots demands precision, strength, and a high-grade finish suitable for visible architectural hardware.

Among all manufacturing routes, investment casting (lost wax casting) is the dominant process because it uniquely delivers tight tolerances, complex geometries, and smooth surfaces straight from the mold.

However, alternative methods—such as machining, forging, or sand casting—are sometimes used for specific performance or cost reasons.

316 Stainless Steel Glass Spigot Castings
316 Stainless Steel Glass Spigot Castings

Investment Casting (Lost Wax Process)

Investment casting is the preferred and most advanced method for manufacturing stainless steel glass spigot bodies. It allows the production of near-net-shape components with minimal post-machining.

Process Overview

  1. Wax Pattern Creation – Wax replicas of the spigot are made using precision injection molds.
  2. Assembly and Shell Building – The wax pattern is assembled onto a tree and repeatedly dipped into ceramic slurry and fine sand to build a hard shell.
  3. Dewaxing – The wax is melted out, leaving a precise negative cavity inside the ceramic mold.
  4. Metal Pouring – Molten stainless steel (e.g., 316L or 2205) is poured into the shell under controlled temperature conditions.
  5. Shell Removal – After solidification, the ceramic shell is broken off mechanically or chemically.
  6. Cutting and Finishing – Individual castings are cut from the sprue, cleaned, shot-blasted, and polished.

Advantages of Investment Casting

  • Dimensional accuracy: Typical tolerance range ±0.1–0.3 mm (ISO 8062-3 CT5–CT6).
  • Excellent surface finish: As-cast surface roughness of Ra 3.2–6.3 μm, easily improved to Ra 0.2–0.4 μm after polishing.
  • Design flexibility: Enables intricate internal features, threads, fillets, and decorative geometry.
  • Material efficiency: Minimal waste and reduced machining allowance.
  • Consistency: High repeatability—critical for architectural batches requiring visual uniformity.

Investment casting also supports a wide range of stainless alloys (304, 316L, 2205, 2507), making it adaptable to both standard and high-performance applications.

Machining from Solid Bar or Billet

CNC machining from stainless steel bars or billets is sometimes used for prototype spigots or small production runs.

  • Advantages: No tooling required, immediate design changes possible, exceptional dimensional control.
  • Limitations: High material waste, longer machining cycles, and higher unit cost.
  • Surface Finish: Requires extensive polishing to achieve architectural aesthetics.

Machined spigots are usually chosen for custom designs, rapid prototyping, or when small batch flexibility outweighs tooling costs.

Forging and Machining Hybrid

Forging is occasionally applied for heavy-duty structural spigots needing enhanced mechanical properties. The forged blank is subsequently CNC-machined and polished.

  • Advantages: Superior mechanical strength, fatigue resistance, and grain flow.
  • Limitations: Limited shape complexity; higher forging die cost; additional machining required.
  • Use Case: Public infrastructure or industrial safety barriers requiring high load-bearing capability.

Sand Casting (Gravity or Shell Mold)

Sand casting may be employed for large or simple components, but it is rarely used for architectural spigots due to its rougher surface and lower precision.

  • Typical tolerances: ±0.5–1.0 mm.
  • Surface roughness: Ra 12.5–25 μm.
  • Applications: Low-cost prototypes, non-visible structural fittings, or oversized anchoring bases.

Metal Injection Molding (MIM)

For smaller stainless fittings or brackets integrated with spigot assemblies, MIM technology is occasionally adopted.

  • Advantages: Very fine detail, high repeatability, small component capability (<100 g).
  • Limitations: Limited to smaller parts, high tooling and feedstock costs.

Comparative Summary

Manufacturing Route Dimensional Accuracy Surface Finish (Ra μm) Strength Tooling Cost Typical Use Case
Investment Casting ±0.1–0.3 mm 3.2–6.3 (as-cast), 0.4 (polished) High Medium Standard for stainless glass spigots
CNC Machining (Solid) ±0.05 mm 0.4 (polished) High None Prototypes, small batches
Forging + Machining ±0.1–0.2 mm 0.4 Very High High Heavy-duty, load-bearing fixtures
Sand Casting ±0.5–1.0 mm 12.5–25 Moderate Low Non-visible or large-scale fittings
MIM (Metal Injection Molding) ±0.05 mm 1.6–3.2 Moderate High Miniature components, connectors

5. Typical Stainless Steel Glass Spigot Casting Specifications

Parameter Specification / Data Notes
Product Name Bolt-down Stainless Steel Glass Spigot Precision investment cast body with base plate
Overall Dimensions Ø49 × 151.5 mm (body) Common standard for frameless glass pool fence systems
Base Plate Diameter Ø100 × 8.5 mm Bolt-down base; supports M6–M10 anchors
Cover Plate Ø103 × Ø50 × 15 mm Decorative finish cap concealing bolts
Groove Size 100 × 16 mm Glass seating channel
Glass Thickness Range 8–12 mm EPDM gaskets or rubber spacers used for adjustment
Rubber Spacer (2 pcs) 99 × 44 × 1.0 mm Prevents metal-to-glass contact
Pressure Plate 71 × 28 × 3 mm Stainless clamping plate (mirror polished)
Fasteners M10×12 mm grub screws; M6×60 mm tapping screws AISI 304 or 316L stainless fasteners
Material Options
AISI 316L / Duplex 2205 / AISI 304 Alloy selected by corrosion environment
Surface Finish Options Satin (Ra 0.8–1.2 μm), Mirror Polish (Ra 0.2–0.4 μm) Mirror finish ideal for outdoor and pool installations
Casting Process Silica-sol Investment Casting ISO 8062-3 CT5 dimensional grade
Machining Tolerances ±0.10–0.30 mm (critical faces) After precision CNC finishing
Surface Roughness (as-cast) Ra 3.2–6.3 μm Improved to < Ra 0.4 μm after polishing
Weight N.W. 1.53 kg / G.W. 1.55 kg Typical for 316L cast unit
Load Rating ≥ 1.0 kN (horizontal load test, typical) Complies with pool fence and balustrade standards
Service Life Expectancy > 15 years (316L) / > 25 years (2205 duplex) Under normal pool or coastal conditions

6. Surface finishes: aesthetics, maintenance, and durability

Stainless Steel Fence Spigot Castings
Stainless Steel Fence Spigot Castings
  • Mirror polish (bright): visually striking, highly reflective, easier to clean — small particles don’t lodge in the surface.
    Typical as-finished Ra ≤ 0.4 µm; achieved by multi-stage mechanical polishing and sometimes electropolishing. Good for high-end façades and where hygiene/cleaning is important.
  • Satin / brushed finish: warm, matte aesthetic; hides minor fingerprints and surface oils; typical Ra 0.5–1.6 µm. Preferred for a restrained look and lower perceived maintenance.
  • Electropolishing (optional): improves corrosion resistance by smoothing micro-peaks and removing embedded contaminants; recommended for marine or pool installations.

7. Corrosion, strength and performance in service

  • Chloride exposure (pools, marine): chloride ions attack passive film on stainless steels, causing pitting.
    Duplex 2205 offers substantially higher resistance than 316/304; electropolishing further increases pitting resistance. Select materials based on exposure class and design life.
  • Galvanic considerations: avoid direct connection of stainless spigot to dissimilar metals without insulation — otherwise risk galvanic corrosion (especially in wet environments).
  • Mechanical load: spigots must be specified and tested against design loads (handrail loads, wind, dynamic impact).
    Structural calculations and field testing are recommended for public access installations.
  • Temperature limits: stainless spigots perform across typical architectural temperature ranges; for elevated-temperature applications consult alloy data.

8. Applications of Stainless Steel Glass Spigot Castings

Stainless Steel Glass Spigot Castings
Stainless Steel Glass Spigot Castings
  • Residential & commercial balustrades (balconies, stairways)
  • Pool fences & glass pool barriers (safety compliance + aesthetics)
  • Public spaces & plazas (frameless glass partitions)
  • Marinas & coastal promenades (when paired with duplex alloys)
  • Retail displays and architectural façades (visible hardware)

9. Why stainless steel casting glass fittings are popular

  • Durability + aesthetics: stainless offers corrosion resistance and high-quality finishes—important in visible architectural hardware.
  • Design freedom: casting produces integrated forms and internal features not practical with fabrication.
  • Cost efficiency at volume: investment casting plus light CNC finishing reduces scrap and machining costs compared with machining from solid.
  • Recyclability: stainless steels are highly recyclable and retain value at end of life—supports sustainability goals.
  • Consistency and QA: modern foundries deliver consistent chemistry, heat treatment and traceability (MTCs, PMI).

10. Why Choose Our Stainless Steel Glass Spigots

  • Experience:  DEZE 10 years specializing in stainless investment cast architectural fittings.
  • Material capability: supply Duplex 2205, 316L, 304 L; MTC and PMI available.
  • Precision: investment casting with CNC finishing yields critical feature tolerances to ±0.05 mm; dimensional control equivalent to CT5 where required.
  • Surface & finishing: mirror, satin, and electropolish finishing in-house; optional assembly, marking and custom packaging.
  • Quality systems: incoming material inspection, CMM inspection, NDT on request, and sample salt spray tests.
  • Service: OEM/ODM, logo engraving, custom drawings accepted, small sample runs to full production.

11. Conclusion

Stainless steel glass spigot castings are a robust, attractive solution for glass fastening in demanding architectural applications.

Success hinges on selecting the correct alloy for the environment (Duplex 2205 for chlorides; 316L for general outdoor use), choosing investment casting plus proper finishing for appearance and tolerance, and specifying installation details (gasketing, anchors, torque) that protect the glass and the fitting.

Clear procurement specs—material certs, finish, tolerances and testing—plus an experienced supplier deliver durable systems that look good and stand up to weather, chlorine and traffic.

 

FAQs

Which stainless grade is best for poolside glass spigots?

Duplex 2205 is preferred for persistent chloride exposure (pools/coastal). 316L is acceptable for less aggressive outdoor conditions.

Can cast spigots be welded on site for modifications?

Welding stainless castings is possible but requires compatible filler, heat control and post-weld cleaning; for duplex grades, welding expertise and proper heat input control are essential.

What finish lasts longest outdoors?

Electropolished or high-quality mirror polished finishes with routine maintenance give the best long-term corrosion resistance in challenging environments.

How do I avoid glass breakage during tightening?

Use the correct EPDM/Neoprene packers sized for glass thickness, follow supplier torque specs, and avoid over-tightening; use calibrated torque wrenches.