| No | China | Japan | America | South Korea | European Union | India | Australia |
|---|---|---|---|---|---|---|---|
| - | GB | JIS | ASTM / UNS | KS | EN | IS | AS |
| 1 | 1Cr17Mn6Ni5N / 12Cr17Mn6Ni5N | SUS201 | 201 / S20100 | STS201 | 1.4372 | 10Cr17Mn6Ni4N20 | 201-2 |
| 2 | 1Cr18Mn8Ni5N / 12Cr18Mn9Ni5N | SUS202 | 202 / S20200 | STS202 | 1.4373 | - | 202 |
| 3 | 1Cr17Ni7 / 12Cr17Ni7 | SUS301 | 301 / S30100 | STS301 | 1.4319 | 10Cr17Ni7 | 301 |
| 4 | 0Cr18Ni9 / 06Cr19Ni10 | SUS304 | 304 / S30400 | STS304 | 1.4301 | 07Cr18Ni9 | 304 |
| 5 | 00Cr19Ni10 / 022Cr19Ni10 | SUS304L | 304L / S30403 | STS304L | 1.4306 | 02Cr18Ni11 | 304L |
| 6 | 0Cr19Ni9N / 06Cr19Ni10N | SUS304N1 | 304N / S30451 | STS304N1 | 1.4315 | - | 304N1 |
| 7 | 0Cr19Ni10NbN / 06Cr19Ni9NbN | SUS304N2 | XM21 / S30452 | STS304N2 | - | - | 304N2 |
| 8 | 00Cr18Ni10N / 022Cr19Ni10N | SUS304LN | 304LN / S30453 | STS304LN | - | - | 304LN |
| 9 | 1Cr18Ni12 / 10Cr18Ni12 | SUS305 | 305 / S30500 | STS305 | 1.4303 | - | 305 |
| 10 | 0Cr23Ni13 / 06Cr23Ni13 | SUS309S | 309S / S30908 | STS309S | 1.4833 | - | 309S |
| 11 | 0Cr25Ni20 / 06Cr25Ni20 | SUS310S | 310S / S31008 | STS310S | 1.4845 | - | 310S |
| 12 | 0Cr17Ni12Mo2 / 06Cr17Ni12Mo2 | SUS316 | 316 / S31600 | STS316 | 1.4401 | 04Cr17Ni12Mo2 | 316 |
| 13 | 0Cr18Ni12Mo3Ti / 06Cr17Ni12Mo2Ti | SUS316Ti | 316Ti / S31635 | - | 1.4571 | 04Cr17Ni12MoTi20 | 316Ti |
| 14 | 00Cr17Ni14Mo2 / 022Cr17Ni12Mo2 | SUS316L | 316L / S31603 | STS316L | 1.4404 | ~02Cr17Ni12Mo2 | 316L |
| 15 | 0Cr17Ni12Mo2N / 06Cr17Ni12Mo2N | SUS316N | 316N / S31651 | STS316N | - | - | 316N |
| 16 | 00Cr17Ni13Mo2N / 022Cr17Ni13Mo2N | SUS316LN | 316LN / S31653 | STS316LN | 1.4429 | - | 316LN |
| 17 | 0Cr18Ni12Mo2Cu2 / 06Cr18Ni12Mo2Cu2 | SUS316J1 | - | STS316J1 | - | - | 316J1 |
| 18 | 00Cr18Ni14Mo2Cu2 / 022Cr18Ni14Mo2Cu2 | SUS316J1L | - | STS316J1L | - | - | - |
| 19 | 0Cr19Ni13Mo3 / 06Cr19Ni13Mo3 | SUS317 | 317 / S31700 | STS317 | - | - | 317 |
| 20 | 00Cr19Ni13Mo3 / 022Cr19Ni13Mo3 | SUS317L | 317L / S31703 | STS317L | 1.4438 | - | 317L |
| 21 | 0Cr18Ni10Ti / 06Cr18Ni11Ti | SUS321 | 321 / S32100 | STS321 | 1.4541 | 04Cr18Ni10Ti20 | 321 |
| 22 | 0Cr18Ni11Nb / 06Cr18Ni11Nb | SUS347 | 347 / S34700 | STS347 | 1.4550 | 04Cr18Ni10Nb40 | 347 |
| No | China | Japan | America | South Korea | European Union | India | Australia |
|---|---|---|---|---|---|---|---|
| - | GB | JIS | ASTM / UNS | KS | EN | IS | AS |
| 23 | 0Cr26Ni5Mo2 | - | SUS329J1 / 329 / S32900 | STS329J1 | 1.4477 | - | 329J1 |
| 24 | 00Cr18Ni5Mo3Si2 / 022Cr19Ni5Mo3Si2N | SUS329J3L | - / S31803 | STS329J3L | 1.4462 | - | 329J3L |
| No | China | China | Japan | America | South Korea | European Union | India | Australia |
|---|---|---|---|---|---|---|---|---|
| - | GB | New national standard (07.10) | JIS | ASTM / UNS | KS | EN | IS | AS |
| 25 | 0Cr13Al | 06Cr13Al | SUS405 | 405 / S40500 | STS405 | 1.4002 | 04Cr13 | 405 |
| 26 | - | 022Cr11Ti | SUH409 | 409 / S40900 | STS409 | 1.4512 | - | 409L |
| 27 | 00Cr12 | 022Cr12 | SUS410L | - | STS410L | - | - | 410L |
| 28 | 1Cr17 | 10Cr17 | SUS430 | 430 / S43000 | STS430 | 1.4016 | 05Cr17 | 430 |
| 29 | 1Cr17Mo | 10Cr17Mo | SUS434 | 434 / S43400 | STS434 | 1.4113 | - | 434 |
| 30 | - | 022Cr18NbTi | - | - | - | S43940 | - | 439 |
| 31 | 00Cr18Mo2 | 019Cr19Mo2NbTi | SUS444 | 444 / S44400 | STS444 | 1.4521 | - | 444 |
| No | China | China | Japan | America | South Korea | European Union | India | Australia |
|---|---|---|---|---|---|---|---|---|
| - | GB | New national standard (07.10) | JIS | ASTM / UNS | KS | EN | IS | AS |
| 32 | 1Cr12 | 12Cr12 | SUS403 | 403 / S40300 | STS403 | - | - | - |
| 33 | 1Cr13 | 12Cr13 | SUS410 | 410 / S41000 | STS410 | 1.4006 | 12Cr13 | 410 |
| 34 | 2Cr13 | 20Cr13 | SUS420J1 | 420 / S42000 | STS420J1 | 1.4021 | 20Cr13 | 420 |
| 35 | 3Cr13 | 30Cr13 | SUS420J2 | - | STS420J2 | 1.4028 | 30Cr13 | 420 |
| 36 | 7Cr17 | 68Cr17 | SUS440A | 440A / S44002 | STS440A | - | - | - |