1. Hōʻikeʻike
Nalowale-wax casting (Kāhaka kūʻai kūʻai) He ala pololei ia e hana ana i ka upena kokoke, nā mea keleawe kikoʻī kiʻekiʻe me ka hoʻopau ʻana i ka ʻili maikaʻi a me ka mana dimensional.
Ke hoʻohui pū ʻia me ke keleawe keleawe kūpono a me nā mana kaʻina hana paʻa, ʻO ka hoʻolei kālā e hāʻawi i nā ʻāpana i hoʻohana ʻia i nā kiwi, hana hanohano, nā mea kani, nā mea hoʻopili a me nā ʻāpana mechanical precision.
Loaʻa ka holomua ma ka hoʻohālikelike ʻana i nā kemika alloy a me nā ʻāpana kaʻina hana, hoʻolālā no ka castability, ka hoʻomalu ʻana i ka pūpū seramika a heheʻe, a me ka hoʻokō ʻana i ka hōʻoia ʻana i ka maikaʻi.
2. He aha ka Brass Investment Casting?
Nalowale-wax casting (Kāhaka kūʻai kūʻai) hoʻololi i ke ʻano wax mōhai i loko o ka poʻi seramika a laila i ʻāpana metala.
Hana ʻia ke ʻano wax e ka hoʻoheheʻe ʻana (no nā ʻano hana hou) a i ʻole mea hana lima (No nā prototypes).
Hoʻohui ʻia nā hiʻohiʻona ma kahi ʻōnaehana puka, uhi ʻia me ka slurry refractory a me ka stucco, dewaxed, a ua puhi ʻia ka pūpū seramika a hoʻopiha ʻia me ka metala hoʻoheheʻe ʻia.
Ma hope o ka paʻa ʻana a me ka hoʻoluʻu ʻana, wehe ʻia ka keramika a hoʻopau ʻia nā hoʻoheheʻe ʻana.
Koho ʻia ka hoʻolei kālā no ke keleawe i ka wā geometry (nā pāʻili, nā lua kūloko, Nā kiko'ī maikaʻi), ʻoi aku ka nui o ka hoʻopau ʻana o ka ʻili a i ʻole ka dimensional repeatability ma mua o ke kumukūʻai haʻahaʻa haʻahaʻa o ka hoʻolei ʻana i ke one.

Nā hiʻohiʻona o ke keleawe nalowale-wax hoʻolei ʻana
- Kiʻekiʻe geometric pololei a me ka repeatability. ʻO nā hoʻomanawanui maʻamau i hiki ke loaʻa ma ka laulā o ± 0.1-0.5 mm no nā hiʻohiʻona liʻiliʻi., ʻokoʻa me ka nui a me ka hana hana ʻana.
- Hoʻopau maikaʻi loa. Hoʻopau maʻamau ka hoʻopau ʻana i ka Ra 0.8–3.2 μm ma muli o ke ʻano o ka pūpū a me ke ʻano; Pono ka mīkini liʻiliʻi no nā noi he nui.
- Hiki ke hoʻolei i nā paia lahilahi a me nā kiko'ī o loko. ʻO ka hoʻolei kālā me ka hilinaʻi e hana i nā ʻāpana lahilahi (liʻiliʻi loa ~1.0–1.5 mm no nā hiʻohiʻona liʻiliʻi loa, maʻamau ≥1.5–3.0 mm no nā ʻāpana haʻahaʻa).
- Loaʻa ka waiwai. E ʻae ana ka hoʻolele kālā i nā ʻano keleawe he nui me nā ʻano like ʻole kepau, hiki ke hoʻokō i ka wai inu a me nā koi hoʻoponopono.
- E hoʻohaʻahaʻa i ka leo machining downstream. ʻO nā ʻano ʻupena kokoke e hōʻemi i ka ʻōpala a me ka manawa mīkini i hoʻohālikelike ʻia me ka forgings a i ʻole ka mīkini billet.
3. Nā māka keleawe maʻamau i hoʻohana ʻia i ka hoʻolei ʻana i ka nalo
I ka hoakaka ana Keihei no ka hoopukapuka (nalowale-wax) kōkua ka hoʻolei ʻana e noʻonoʻo mua ma ohana (alpha, alpha-beta, ʻoki kūʻokoʻa, hoʻemi ʻia ke kēpau/lead-free, a me nā keleawe kūikawā) a laila koho i kahi papa kiko'ī e lawelawe mau ai ka hale hana.
pahu pahu / haʻahaʻa-zinc (a) keleawe - maikaʻi ductility & Ke kū'ē neiʻo Corrosionion
Laʻana maʻamau:US C26000 (70/30 Keihei, keleawe pahu pahu)
- No ke aha i hoʻohana ʻia ai: Hāʻawi ka microstructure α hoʻokahi-phase i ka ductility maikaʻi loa, maikaʻi corrosion kū'ē a me ka maikai formability; hoʻohana mau ʻia no ka pā lahilahi, ʻāpana hoʻonaninani a huki ʻia paha.
- Nā noi i ka hoʻolei kālā: nā mea hoʻonani, kino kiwi pā lahilahi, hale kūkulu hale kahi mea e pono ai ka formability a me ka corrosion.
Nā keleawe alpha-beta - ikaika kiʻekiʻe / hālulu (maikaʻi no nā mea mechanical)
Laʻana maʻamau:UNS C38500 / C37700 ʻohana (nā keleawe hoʻolei ʻenehana maʻamau)
- No ke aha i hoʻohana ʻia ai: ʻOi aku ka nui o ka zinc ma loko o kahi α + β ʻelua ʻano hana e hoʻonui ai i ka ikaika a me ka paʻakikī me nā keleawe α - pono kahi e pono ai ka hana mechanical.
- Noi: Gear Blanks, Bussings, nā hale halihali a me nā ʻāpana mīkini liʻiliʻi e koi ana i ka ikaika i hoʻomaikaʻi ʻia ʻoiai e mālama ana i ka castability kūpono.
ʻoki manuahi (ke kēpau a me ke kēpau) keleawe - machinability focus
Nā hiʻohiʻona maʻamau:US C36000 (ʻO ke keleawe manuahi manuahi); nā mea ʻē aʻe i hoʻemi ʻia ke kēpau (bismuth a i ʻole nā mea hoʻohui silika) hoʻonui nui ʻia no nā noi i hoʻoponopono ʻia.
- No ke aha i hoʻohana ʻia ai: ʻO ka Mancinability maikaʻi (ʻO ke alakaʻi a i ʻole nā mea hoʻokomo pani e hana ma ke ʻano he mea wāwahi chip a me nā lubricants), hiki i ka liʻiliʻi o ka hoʻopau ʻana i ka manawa hana ma hope o ka hoʻolei ʻana.
- Noi: kino hookui, nā ʻāpana pili a me nā ʻāpana pololei kahi e pono ai ka mīkini post-cast.
ʻO nā keleawe pale dezincification (RDA / haʻahaʻa-dezincification) - no ka wai inu & nā wahi hoʻohālikelike
Nā hiʻohiʻona maʻamau: nā mea hao i kūʻai ʻia e like me RDA a i ʻole nā māka UNS i hana ʻia no ka dezincification haʻahaʻa (ʻO kekahi mau ʻohana papa cast i kuhikuhi ʻia e hālāwai me nā hoʻokolohua kūʻē dezincification).
- No ke aha i hoʻohana ʻia ai: Ma nā noi wai inu a me kekahi mau hōʻike kai, hiki i nā keleawe maʻamau ke loaʻa i ka dezincification (ka hoolele koho ana o Zn).
ʻO nā keleawe ʻano DZR e hōʻemi i kēia pilikia a koi pinepine ʻia e nā kūlana paipu. - Noi: mea pono wai inu, nā kīwī a me nā paipu paipu i hana ʻia e ka hoʻolei kālā kahi e koi ʻia ai ke kūpaʻa dezincification lōʻihi.
ʻO nā keleawe keleawe a me ka nickel - corrosion kūikawā a me ke koena ikaika
Nā hiʻohiʻona maʻamau: ʻO nā keleawe i hoʻololi ʻia ke silika a me nā mea hoʻohui liʻiliʻi-Ni i loaʻa e like me nā māka hoʻolei (e ʻimi i ka foundry no nā koho UNS pololei).
- No ke aha i hoʻohana ʻia ai: Hoʻomaikaʻi i ka pale ʻana i ka corrosion, ʻoi aku ka maikaʻi o ka castability, a i ʻole ka hoʻomaikaʻi ʻana i ke kūpaʻa wela kiʻekiʻe e pili ana i ka alloy.
Hiki ke hoʻohana ʻia ka silikoni e hoʻonui i ka ikaika a me ka machinability i nā hoʻolālā alakaʻi ʻole. - Noi: nā lako wai kai, nā ʻāpana liʻiliʻi kūʻokoʻa a me nā lako moana kūikawā.
4. ʻO ke kaʻina hana hoʻoheheʻe ʻana i ke keleawe - he haʻihaʻi ʻenehana i kēlā me kēia pae
Hoʻolilo keleawe (nalowale-wax) ʻO ka hoʻolei ʻana he kaʻina o nā hana i hoʻopaʻa ʻia.
Hoʻopili kēlā me kēia pae i ke geometry hope, maikaʻi o ka ʻili a me ka maikaʻi o loko, no laila, pili ka hana o kēia wā i nā ʻāpana kikoʻī, nā puka nānā a me nā hana hoʻoponopono i kēlā me kēia kaʻina.

Hana ʻana i ke ʻano o ka wax
Kumu: e hoʻopuka i kahi ʻano ʻālana kūpono e wehewehe ana i ka geometry as-cast a me ka hoʻopau ʻili.
Nā hana:
- Nā hiʻohiʻona wax i hoʻoheheʻe ʻia (Hoʻohana): wax molten pattern (ʻO ka maʻamau he hui ʻana o nā waxes paraffin/microcrystalline me nā mea plasticizer a me nā mea hana dewax) hoʻokomo ʻia i loko o nā pahu kila paʻakikī.
ʻO nā kaomi maʻamau maʻamau mai 0.7–3.5 MPa (100–500 psi) a ʻo ka maʻamau maʻamau ka wela 60-80 ° C e hōʻoia i ka hoʻopiha a me ka reproducible shrinkage. Hoʻopili ʻia nā manawa kaʻa i ka nui o ka lua (kekona i kekahi mau minuke). - Nā hiʻohiʻona kalai lima a i ʻole CNC wax/resin (Pūnaehana, holo pōkole): e ʻae i nā kiʻi hoʻokahi a paʻakikī ʻaʻole i kūpono i ka mea hana.
Nā mana & QC: ka nānā ʻana o nā mamana (Nā mea kāhea, mea hoʻohālikelike optical a i ʻole 3D scanner); nānā maka no nā humuhumu, nā hakahaka a me ka uila.
Hōʻole a hana hou i nā mamana hemahema. E hoʻopaʻa i ka ʻāpana wax a me ka ʻike mea paahana no ka traceability.
Hui hoohalike (lāʻau) a me ka hoʻolālā puka
Kumu: hoʻohui i nā hiʻohiʻona he nui ma luna o kahi ʻōnaehana sprue e hana i hoʻokahi lāʻau hoʻolei no ka hoʻoheheʻe ʻana a me ka ninini ʻana.
E hoʻomaʻamaʻa: hoʻolālā i nā ʻāpana keʻa / sprue e hāʻawi i ka meaʻai metala kūpono a me ka paʻa kuhikuhi.
E noʻonoʻo i ka hapa nui, ʻokoʻa ka mānoanoa o ka pā a me ka manawa hoʻopiha i ka wā e hoʻonui ai i nā puka; ʻano pālākiō maʻamau me ka leo hapa. E hoʻohana i nā mea ʻai wela a me ke anuanu inā pono no nā ʻāpana nui.
Nā mana & QC: e helu i ka manawa hoʻopiha a me ka hiki ke piʻi; hoʻohālikelike i ka kahe a holo i nā hoʻokolohua kino no nā geometries koʻikoʻi.
E nānā i nā hui no ka hoʻopaʻa paʻa ʻana ma waena o nā mamana a me ka sprue, hoʻonohonoho kūpono a me nā ala hoʻokuʻu.
ʻO ka pūpū seramika (Hāʻawiʻia) hoʻokumu
Kumu: e kūkulu i ka pūpū refractory e hoʻopuka hou i nā kikoʻī kumu a kūʻē i ka hoʻouka ʻana i ka wela a me ke kemika i ka wā e ninini ana.
Ke kaʻina hana:
- ʻaʻahu mua (kapa maka): e hoʻopaʻa i ka lāʻau i loko o kahi slurry refractory maikaʻi (mea hoʻopaʻa koʻikoʻi colloidal a i ʻole ethyl silicate me ka pauka zircon/alumina/silica maikaʻi).
E hoʻopili koke i kahi stucco maikaʻi e hopu i nā kikoʻī. Hoʻopau ke alo o ka ʻaʻahu maka. - Nā ʻaʻahu kākoʻo: e hoʻopili i ka slurry coarser + nā papa stucco e hoʻomohala i ka mānoanoa.
ʻO ka helu ʻana o ka papa e pili ana i ka hapa nui - pono paha nā ʻāpana liʻiliʻi i 6-8 mau kapa, hui nui 10-15. Nā pae mānoanoa o ka pūpū maʻamau 5-15 mm (0.2–0.6 iniha) Ke hilinaʻi nei i ka nui. - Haunaele: maloʻo hoʻomalu (ambient or forced ea) ma waena o nā ʻaʻahu pale i ka hoʻonui ʻana i ka mahu a me ka haki ʻana o ka pūpū.
ʻO ka hoʻomaloʻo nui ʻana ma waena o nā ʻaʻahu he 1-24 mau hola ma muli o ka haʻahaʻa a me ka ʻōnaehana.
Nota mea: no ke keleawe, e hoʻohana i ka zircon a i ʻole nā stuccos alumina kiʻekiʻe no ka ʻaʻahu maka e hōʻemi i ka hopena kemika metala-shell a me nā hemahema alpha-case.
Nā mana & QC: e ana i ka paona pulu a maloo, nānā i ka mānoanoa pūpū, a me ka laʻana i nā pūpū hoʻāʻo no ka ikaika (hoʻāʻo apo) ma mua o ka dewaxing.
Hoomoana (ka wehe ʻana i ke ʻano)
Kumu: e haʻalele i ka wax me ka pōʻino ʻole i ka pūpū.
Nā hana: ka mahu autoclave a i ʻole ka umu dewaxing.
Hoʻohana nā pōʻaiapuni autoclave maʻamau i ka mahu ma 100–150 °C me nā pōʻai kaomi e māhā a hoʻokahe i ka wax; Hoʻohana ka umu dewaxing i kahi ala i hoʻonohonoho ʻia e hoʻoheheʻe i ka wax. E hōʻiliʻili a hana hou i ka wax i hoʻihoʻi ʻia.
Nā mana & QC: e hōʻoia i ka pau ʻana o ka wax (nānā nānā/kaumaha); e nānā no ke koena o ka wax a i ʻole ka pōʻino pūpū. Mālama ʻo dewax maikaʻi i nā hemahema kinoea i ka wā e ninini ana.
Shell Firring / kaka ahi
Kumu: wehe i nā koena mea ola, nā mea hoʻopili volatilized a hoʻopaʻa i ka ceramic no ka ikaika mechanical a me ka paʻa wela.
Hoʻomaʻamaʻa mua i ka pūpū e hōʻemi i ka haʻalulu wela i ka ninini ʻana.
Nā papahana maʻamau: ramp hoʻomalu i 600–900 °C me nā paʻa i lawa no ka hoʻoheheʻe ʻana i nā mea ola a hoʻōla i nā mea paʻa (maʻa mau hola 2-4 ma muli o ka nui o ka pūpū).
ʻO ka wela mua ma mua o ka ninini pinepine ʻana 600-800 ° C.
Nā mana & QC: e nānā i ka ʻike wela kiln, mau manawa a me ka lewa. E ho'āʻo i nā pūpū i puhi ʻia no ka pau ʻana o ka mea paʻa (ke koena kalapona), permeability a me ka pono mechanical.
Hoʻomākaukau metala - hoʻoheheʻe, lapaʻau a me ka hoʻoheheʻe ʻana
Kumu: hana i ka maemae, pololei ka haku mele, ʻO ke keleawe hoʻoheheʻe haʻahaʻa haʻahaʻa i mākaukau no ka ninini ʻana.
Nā Pono Hana: He mea maʻamau ka induction or resistance crucible furnaces; graphite a i ʻole nā lining crucible seramika.
Kaʻina hana:
- Ka mana hoʻopaʻa: hoʻohana i nā hui ʻōpala/ingot i hōʻoia ʻia e hoʻokō i ka haku mele (e kuhikuhi i nā mea tramp ʻae ʻia).
- Ka wela wela: e lawe i ka huila i loko o ka puka makani wela nui; no nā keleawe maʻamau liquidus ≈ 900-940 ° C, laula ninini pono 950-1,050 ° C ma muli o ka hao a me ka pūpū.
E hōʻalo i ka wela nui e hōʻemi i ka hoʻohuhū zinc. - Kālā wailua / kākina: e hoʻohana i nā kahe kūpono e wehe i nā oxides a me ka lepo.
- Keila: kinoea inert bubble (Aron, nitrogen) a i ʻole e hoʻohana i nā degasser rotary e hōʻemi i ka hydrogen a me ka oxygen.
- Kapalakula: e ninini i loko o nā kānana huʻa seramika e hoʻopili i nā hoʻokomo.
Nā mana & QC: hoʻopaʻa hoʻoheheʻe kemika (Poina), No ke kauwela, nā kaʻina flux a me nā degas. Laʻana a me ka palapala MTR no ka huli ʻana o ka hailona.
Ka ninini a hoʻopiha i ka pūpū
Kumu: e hoʻopiha i ka lua pūpū i hoʻomaʻemaʻe ʻia me ke keleawe hoʻoheheʻe maʻemaʻe ma lalo o nā kūlana i mālama ʻia e pale i nā hemahema.
Nā hana: ka ninini ʻana o ka umekaumaha a i ʻole ke kaomi haʻahaʻa/riser-kōkua ʻia no nā ʻāpana paʻakikī. Hoʻolālā ʻia ka nui o ka ninini ʻana a me ka trajectory e hōʻemi i ka turbulence a me ka entrainment.
Nā mana & QC: e mālama i ka mahana wela i loko o ka pahu pahu; e nānā i ka manawa hoʻopiha a me ka hana hoʻoheheʻe ʻike; hoʻohana i ka kānana a me ka hoʻopaʻa ʻia ʻana.
No nā hoʻolei koʻikoʻi, hoʻopaʻa hoʻopaʻa wikiō a me nā moʻolelo wela.
Kūpuia, hooluolu a lulu
Kūpuia: emi ke keleawe ma ka paʻa (hōʻemi laina maʻamau ≈ 1-2%); pono e uku ka gating a me ka risers.
E paipai i ka hoʻopaʻa ʻana mai ka ʻāpana lahilahi a kaumaha.
Ho'ōla: e ʻae i ka ʻoluʻolu e hoʻemi i ke koʻikoʻi wela - mākaukau paha nā ʻāpana liʻiliʻi no ka lulu ʻana 24 Nā hola hola; ʻoi aku ka lōʻihi o nā ʻāpana nui (a i 72 Nā hola hola).
Hiki i ka ho'opio wikiwiki ke ho'oulu i ka pohā a i 'ole ka ha'iha'i.
Ka Haakauaoha / Shell lawe: e hoʻoneʻe i ka keramika me ka haʻalulu mechanical, hopena pneumatic, ka pahū wai a i ʻole ka hoʻoheheʻe kemika inā kūpono.
Hopu a hana hou i nā ʻāpana pūpū a hoʻomalu i ka lepo lele (pale hanu a me ka kānana).
Nā mana & QC: e nānā no ka pili ʻana o ke koena pūpū, ili ili (pahu alpha), nui ka porosity a i ʻole holo hewa.
Hoʻopau a hoʻopau i nā hana
Nā hana mua: ʻoki i nā ʻōpuʻu a me nā kukini (bandsaw, ʻoki ʻoki abrasive), wili puka, a hui pū i nā ʻili.
Nā lāʻau abrasive a me ka mechanical: pana, ʻO ka hoʻopau ʻana i ka haʻalulu a i ʻole ka haʻalulu e hoʻoneʻe i ke koena seramika a maʻemaʻe.
Hana wela: stress-relief anneal maʻamau ~250–450 °C e hoemi i ka hoolei ana; Pono paha nā keleawe i koho ʻia i nā mea hoʻohui homogenization - e hahai i nā papa kuhikuhi kikoʻī. E hōʻalo i ka wela nui e hoʻoikaika i ka nalowale o ka zinc.
Machimen: e hana i ka mīkini hope loa kahi e koi ʻia ai nā hoʻomanawanui (ke huli, MilightʻAʻole, hoʻomālamalama); koho i nā mea hana a me nā meaʻai kūpono i ka pae keleawe (ʻO nā keleawe alakaʻi ʻole ke koi aku i nā ʻāpana hoʻololi).
Nā mea kino kino: Kāleka, Wehe (nickel, chrome), nā lacquers a i ʻole passivation e like me ka mea i ʻōlelo ʻia. E hōʻoia i ka hoʻomaʻemaʻe mua ʻana e hōʻoia i ka pili ʻana o ka uhi.
Nā mana & QC: Ke nānāʻole neiʻo Dimensonal (Cmm, Nā Buke), ana hoopau ili (Ra), nā ho'āʻo paʻakikī a me ka ʻae ʻana i ka ʻike.

ʻO ka nānā hope a me ka hoʻāʻo
Huahuai & nānā'ōwaho: Cmm, nā mea hoʻohālikelike optical, 3D ka nānā ʻana, a me ka ʻike no nā hemahema o ka ʻili.
Ndt: mea komo wai no nā māwae ili, radioography a i ʻole ultrasonic no ka porosity kūloko ma nā ʻāpana koʻikoʻi; eddy au no nā ʻāpana lahilahi.
Nā Hōʻike Manaʻo: tersele, hua, nā ho'āʻo elongation a me ka paʻakikī ma luna o nā hōʻailona hōʻailona a i ʻole nā mea hoʻohālike.
ʻO ka loiloi Chemical: OES/spark spectroscopy e hoʻopaʻa i ka hoʻohui ʻana i ka alloy e kūʻē i ka UNS/ASTM spec.
Nā palapala palapala: MTRs, papa hana (mea ', E ninini, kiʻi pū), mālama ʻia nā moʻolelo nānā a me ka traceability i kēlā me kēia ʻōnaehana maikaʻi (E.g., Iso 9001).
E hōʻole a palapala i nā mea like ʻole; hoʻopili i nā hana hoʻoponopono kumu.
5. Nā hemahema hoʻolei maʻamau, nā kumu kumu a me nā hopena
Potiwale (kinoea a me ka emi)
- Nā kumulā: nā kinoea hoʻoheheʻe (H₂, olio), ka piʻi kūpono ʻole, ka ninini ʻino, ea paa.
- Nā koho: Keila, Kālā wailua, kānana, ʻO ka hoʻolālā gating/riser kūpono, maikaʻi loa ninini wela, ka hoʻoheheʻe ʻia ʻana o ka vacuum inā pono.
Nā Hoʻohui / hoʻopaʻa paʻa
- Nā kumulā: ka hoʻomaʻemaʻe maikaʻi ʻole a i ʻole ka skimming kūpono ʻole.
- Nā koho: hoʻohana i ka uku maʻemaʻe, ka holo pono, nā kānana seramika a me ka hoʻoheheʻe ʻia ʻana o ka wai.
Poino / nā'ōpū anuanu
- Nā kumulā: lawa ole ka wela ninini, kahe maikaʻi ʻole i nā ʻāpana lahilahi.
- Nā koho: hoʻonui i ka wela (i loko o nā palena), revise gateting, e hoʻopaʻa pono i ka paʻa o ka pūpū.
Waimaka wela / Kāle Uhiʻi
- Nā kumulā: kaohi ʻana, hoʻololi ʻāpana ʻoi, nā māhele interdendritic palupalu i nā ʻāpana alpha-beta.
- Nā koho: hoʻolālā hou i nā hoʻololi mānoanoa-ʻiʻihi, E hoʻohui i nā kīʻaha, hoʻololi i ke ala paʻa me ke anuanu a i ʻole ka puka ʻē aʻe.
Pane ʻeleʻele metala (hoʻouka kemika)
- Nā kumulā: mea ʻeleʻele reactive (silika manuahi), superheat nui, hoʻohaumia i ka pūpū.
- Nā koho: hoʻohana i ka zircon/alumina stucco no ke keleawe, hoʻomalu i ke kī ʻana i ka pū, e hoemi i ka wela nui, hōʻoia i ka maʻemaʻe o ka pūpū.
Hoʻokaʻawale a me ke koʻikoʻi koena
- Nā kumulā: ka hoʻolili ʻole ʻana a i ʻole ka lawelawe ʻana i ka mīkini i ka wā wela.
- Nā koho: kāohiʻia hōʻoluʻolu, stress-relief anneal, nā mea hoʻoponopono kūpono.
6. Nā Pōmaikaʻi o ka hoʻolei ʻana i ke keleawe nalowale-wax
- ʻO nā kikoʻī kiʻekiʻe a me ka maikaʻi o ka ʻili: hoemi i ka pau ana o ke kumu kuai a hiki i ka waiwai waiwai kiko'ī.
- Ka pololei a me ka hana hou: pono no na hui, nā hiʻohiʻona male a me nā paʻi paʻi.
- Hiki i nā geometries kūloko paʻakikī: nā pāʻili, undercuts a me nā ʻaoʻao kūloko me ka ʻole o nā cores i kekahi mau hihia.
- Mea kūponoʻole: ʻO nā ʻano ʻupena kokoke e hōʻemi i ka nui o ka ʻōpala a me ka mīkini.
- Hoʻololi i ka nui hana: hiki ke hoʻokele waiwai no nā prototypes ma o nā holo hana waena; ʻoi aku ka liʻiliʻi o ke kumukūʻai o nā mea paahana no ka hoʻoheheʻe ʻana i ka wax ma mua o ka make no ka hoʻoheheʻe nui ʻana.
7. Nā Hana Hana Hana o ke keleawe nalowale-wax
Hoʻohana ʻia ka hoʻolei kālā keleawe ma kahi o nā aesthetics, ka pololei a me ka hana corrosion:

- Plumbing & nā mea hoʻomaʻemaʻe: Nā Vilves, kino paipu, demirative trim (nā ʻano ʻokoʻa alakaʻi ʻole i koi ʻia i nā noi inu).
- Lako hoohiwahiwa & ʻOihana HoʻolālāʻAmelika: nā mea kāhiko, Ke kukui uila, nā kahu hānai.
- Nā mea kani & nā mea kani: nā ʻano bele paʻakikī a me nā pono kūpono.
- Nā mea hoʻohui uila a me ka uila: pololei geometric tolerances a maikaʻi conductivity.
- ʻO nā ʻāpana mīkini pololei: Gear Blanks, Ke hali nei, nā'āpana pā liʻiliʻi liʻiliʻi.
- Nā ʻāpana kūikawā: Mary Ples, nā mea hana pono kahi e pono ai nā ʻano paʻakikī a me ka ikaika haʻahaʻa.
8. Hoʻohālikelike i nā Kaʻina hana hoʻolei keleawe
| Loko | Nalowale-wax (Waiwai kūʻai) Kauhi | Sand cread |
| Nānā kaʻina hana | Wax kumu(S) → kūkulu ʻia ka pūpū seramika (mau kapa komo) → dewax → puhi ʻana i ka pūpū → ninini → lulu → hoʻopau. Hoʻomalu nui ʻia, kaʻina hana he nui. | Kākau (lāʻau/metala/pepa) i loko o ke one mold → hoʻokahi ninini → shakeout → hoʻomaʻemaʻe/hoʻopau. Hāhao, ʻoi aku ka maʻalahi o ka hoʻomākaukau ʻana. |
| Nā noi maʻamau | Liʻiliʻi–waena, nā'āpana likeʻole: Nā Vilves, hana hanohano, Nā'Āpana Pūnaewele, mea mele, Hoʻohui kūpono kūpono. | Nā ʻāpana geometry nui a maʻalahi paha: Nā Hale Hōʻikeʻike, nā lako nui, hoolei kalakala, nā prototypes a me nā mea hoʻokahi. |
Kiko'ī & paʻakikī geometric |
Kiʻekiʻe loa - kikoʻī maikaʻi, nā pāʻili, nā undercuts, Nā hiʻohiʻona o loko (me nā kaula). | Loli - maikaʻi no nā ʻano maʻalahi a paʻakikī; Pono nā ʻoki a me nā kikoʻī maikaʻi i nā cores a i ʻole ka paʻakikī o nā kumu. |
| Paulapua (maʻamau e like me-lawe, Ra) | Kūpono: ~0.8–3.2 µm (hiki ke ʻoi aku ka maikaʻi me nā ʻaʻahu maka maikaʻi). | Coarser: ~6–25 µm (pili i ke one a me nā mea hoʻopaʻa). |
| Dimensional pololei (MAKAINA WAU) | High: ± 0.1-0.5 mm (pili ka nui hapa). | Haʻahaʻa: ±0.5–3.0 mm (hiʻona & Ka hilinaʻi nui). |
| ʻO ka liʻiliʻi liʻiliʻi o ka pā | Kope: ~ 1.0–1.5 mm hiki ke loaʻa; 1.5-3.0 mm i ʻōlelo ʻia no nā hiʻohiʻona lawe ukana. | mānoanoa: ʻO ka maʻamau ≥3–5 mm i ʻōlelo ʻia no ka hoʻopiha pono a me ka ikaika. |
ʻO ka nui o ka ʻāpana kūpono / Ke kaumaha |
Liʻiliʻi–waena: maʻa mau a hiki i ~20-50 kg no ka hoʻolei ʻana i ka hana maʻamau (hiki ke nui me ka lawelawe kūikawā). | Nui: ʻO nā ʻāpana mai kahi liʻiliʻi kilokani a hiki i nā tona he nui. |
| TOLECE & lawehala | Hiki ke hoʻihoʻi hou i nā holo ma muli o ka mea hana i hoʻomalu ʻia a me ke kaʻina hana shell. | Maikaʻi no nā hiʻohiʻona nui; ʻO ka hoʻihoʻi hou ʻana ma muli o ke ʻano a me ka mana one. |
| Potiwale / PūNea ma loko | E emi ka pilikia ke hoʻoheheʻe ka mana, hoʻokō pono ʻia ka kānana a me ke kī ʻana i ka pūpū; ʻoi aku ka maikaʻi no nā ʻāpana paʻa paʻa. | ʻOi aku ka nui o ka pilikia o ke kinoea a me ka shrinkage porosity inā ʻaʻole koʻikoʻi nā hana hoʻokele / hānai a hoʻoheheʻe.. |
Nā Pīkuhi Propertinies (maʻamau e like me-lawe) |
ʻO nā ikaika pili i ka alloy like (E.g., 200–450 MPa no ke keleawe) aka, ʻoi aku ka maikaʻi pinepine ma muli o ka microstructure ʻoi aku ka maikaʻi mai ka hoʻopaʻa ʻia ʻana. | ʻOi aku ka ikaika o ka huila like ʻole akā ʻoi aku ka nui o ka microstructure i nā ʻāpana mānoanoa; ʻokoʻa nā ʻano mechanical me ka pauku a me ka nui o ka hoʻoilo. |
| Hoao / ʻO ke kumukūʻai kumu | Loli: mea paahana kila no na poni wax (ʻoi aku ka kiʻekiʻe ma mua o nā kumu lāʻau hoʻokahi / plastik akā haʻahaʻa ma mua o ka mea hana make). Maikaʻi no ka holo waena. | Hoʻohaʻahaʻa: ʻO ke kumukūʻai kumu (lāʻau/pepa/metala); he haʻahaʻa ke kumukūʻai paahana no nā ʻāpana one - kūpono no nā ʻāpana nui/hoʻokahi. |
ʻO ke kumu kūʻai o ka ʻāpana |
Maikaʻi ke kumu kūʻai no ka ʻāpana liʻiliʻi; ʻoi aku ka maikaʻi o ka hoʻonui ʻana i nā mea hana ma nā puʻupuʻu liʻiliʻi. | Kūʻai maikaʻi loa no nā ʻāpana nui a i ʻole nā puke haʻahaʻa loa; ʻO ka hoʻopau ʻana i kēlā me kēia ʻāpana hiki ke hoʻonui i ke kumukūʻai no nā koi pololei. |
| Ka manawa o waena o ka hoʻomaka a i ka wā pau | ʻOi aku ka lōʻihi ma muli o ke kūkulu ʻana i ka pūpū, dewaxing a me ke kī ʻana (nā lā a i nā pule e pili ana i ka papa hana a me ka shell). | ʻOi aku ka pōkole no nā ʻāpana maʻalahi - ka lā hoʻokahi a i kekahi mau lā maʻamau. |
| Pono ka hana hope | Pono ka mīkini liʻiliʻi / hoʻopau; pinepine kokoke-upena, hoemi i ka huina hoopau koina. | ʻOi aku ka hana machining/hoʻopau i mea maʻamau e hiki ai i nā ʻae like ʻole/ka pau ʻana o ka ʻili. |
ʻAno & pono waiwai |
Maikaʻi waiwai kiʻekiʻe - ʻo nā ʻano ʻupena kokoke e hōʻemi i ka ʻōpala a me ka ʻōpala mīkini. Loaʻa nā kahawai hoʻoheheʻe a me ka pūpū akā pono e mālama ʻia. | Hiki ke piʻi aʻe ka ʻōpala waiwai (nā haʻawina mīkini, 'Anaʻa); Hiki ke hoʻohana hou ʻia ke one akā pono ka mālama ʻana a me ka hoʻoponopono hou ʻana. |
| Kaiualoa & Nā noʻonoʻo palekana | Hoʻoponopono i ka lawelawe ʻana i ka wax, Shell Dust, kiln emissions, a lilo i mau mea paa. Pono e hoʻomalu i ka lepo/huhū a me ka hana hou ʻana i ka wax. | Mālama i ka lepo silica/sani (pilikia silica respirable), nā hoʻokuʻu hoʻopaʻa; koʻikoʻi ka hoʻihoʻi ʻana i ke one a me ka mālama ʻana i ka lepo. |
| Loaʻa (kahi e oi ai) | ʻOi loa no nā kikoʻī kiʻekiʻe, Nā Paukū Kuhi, ʻoi loa ka hoʻopau ʻana i ka ʻili a me nā hoʻomanawanui paʻa; liʻiliʻi post-machining; maikaʻi no nā holo hana waena. | Maikaʻi loa no ka nui, nā'āpana maʻalahi, haʻahaʻa haʻahaʻa haʻahaʻa, huli wikiwiki no nā prototypes a me nā ʻāpana hoʻokahi; scalable i nā mea nui loa. |
PAHUI |
ʻOi aku ka paʻakikī o ke kaʻina hana ma kēlā me kēia ʻāpana a lōʻihi ka manawa pōʻai; ʻoi aku ka maikaʻi no nā ʻāpana nui a i ʻole nā puke kiʻekiʻe loa kahi e ʻoi aku ka maikaʻi o ka hoʻolei ʻana. | Ua kaupalena ʻia ka hoʻopau ʻana a me ka pololei; ʻaʻole kūpono no nā ʻāpana lahilahi a i ʻole nā kikoʻī paʻakikī; kiʻekiʻe hoʻopau hana haʻahaʻa. |
| I ka manawa e koho ai | E koho i ka geometry/detail, ʻO ka hoʻopau ʻana i ka ʻili a me ka pololei o ka dimensional nā mea hoʻokele mua, a i ʻole he mea nui ka hoʻokō waiwai no ka nui o ka hana ʻana. | E koho i ka nui o ka ʻāpana, ʻoluʻolu ka hoʻomanawanui, a i ʻole ke koi ʻia ke kumukūʻai haʻahaʻa haʻahaʻa haʻahaʻa a me ka huli wikiwiki ʻana. |
| ʻO ka laʻana alakaʻi ʻelele | 7-21 mau lā maʻamau no nā pūʻulu hana (ʻokoʻa ma muli o ka hiki ke hana). | 1–7 mau lā maʻamau no nā ʻano maʻalahi/holo pōkole. |
9. Nā hopena
keleawe nalowale-wax hoolei (Kāhaka kūʻai kūʻai) he kanaka makua, ʻano hoʻolei pololei e hāʻawi ana i ka maikaʻi o ka ʻili, ʻO ka pololei o ka dimensional a me ka hiki ke hana i nā geometries paʻakikī.
Hoʻohana nui ia i ka paipu, ka manuahi, nā mea kani a me nā mea pololei.
Pono ka holomua i nā hoʻoholo pili: ke koho ʻana i ka ʻohana keleawe kūpono (alpha vs alpha-beta vs lead-free), hoʻolikelike i ke kemika pūpū me ke keleawe e pale aku ai i ka ʻae ʻana o ka ʻili metala, e hoʻomalu i ka hoʻoheheʻe a me ka ninini ʻana i nā ʻāpana e pale i ka porosity a i ʻole ka nalowale Zn, a me ka hoʻolālā ʻana i ka mālama ʻana i ka wela ma hope o ka hoʻolei ʻana a me ka hoʻopau ʻana.
No nā noi i hoʻoponopono ʻia (wai wai) e kuhikuhi i nā palena alakaʻi a noi i nā MTR.
Ke ʻāpana geometry, ʻoi aku ka nui o ka hoʻopau a me ka pololei ma mua o ke kumu kūʻai maʻalahi, hāʻawi ka hoʻolei kālā ʻana i kahi ala hoʻohua kūpono.
FaqS
He aha ka liʻiliʻi o ka mānoanoa o ka pā e hiki ke hoʻolei ʻia i ke keleawe e ka hoʻolei kālā?
Hiki i nā hiʻohiʻona liʻiliʻi loa a hiki i ~ 1.0-1.5 mm no nā kikoʻī non-loadbearing; no nā mea hoʻolālā hana ʻenehana hilinaʻi e kuhikuhi maʻamau i ka ≥1.5–3.0 mm ma muli o ka nui a me ke kaumaha.
He mea ma'amau no ka ho'olei 'ana i ke keleawe?
Hoʻopaʻa paʻa nā ala keleawe ma kahi o ~900–940 °C. ʻO nā mahana ninini maʻamau i hoʻohana ʻia e nā foundries ~950–1,050 °C, i hoʻopaʻa ʻia no ka ʻōnaehana alloy a me ka shell.
Pono e pale i ka wela nui e kaupalena i ka hoʻohuhū zinc.
Pehea wau e hōʻemi ai i ka porosity i nā hoʻolei keleawe keleawe?
Degas ka hehee, e hoʻohana i ka fluxing kūpono a me ka skimming, hoʻopili i ka kānana keramika, hoʻolālā i nā ʻōnaehana gating/riser kūpono, hoʻomalu ninini wela a me ka wikiwiki, a noʻonoʻo i ka hoʻolei ʻana i ka lewa a i ʻole inert lewa no nā ʻāpana kūpaʻa kiʻekiʻe.
He pilikia nā keleawe alakaʻi?
Ke alakaʻi i hoʻomaikaʻi ʻia ka machinability ma ka mōʻaukala, akā, no ka wai inu a me ka nui o nā noi i hoʻoponopono ʻia ua kaupalena ʻia ke alakaʻi. E hoʻohana i nā mea ʻē aʻe me ke alakaʻi ʻole a i ʻole ke alakaʻi haʻahaʻa a loaʻa i nā hōʻike hoʻāʻo mea i hōʻoia ʻia.
ʻO ka manawa hea e makemake ai au i ka hoʻolei ʻana i ke one no ke keleawe?
E koho i ka hoʻolei kālā inā makemake ʻoe i nā kikoʻī maikaʻi, nā pāʻili, ʻoi aku ka maikaʻi o ka hoʻopau ʻana i ka ʻili; koho i ka hoolei one no ka nui, nā ʻano maʻalahi kahi e hoʻemi ʻia ai ke kumukūʻai o nā mea hana.