Lost Foam Casting Services

DEZE provides comprehensive Lost Foam Casting Services for rapid prototyping and full-scale production. Our process produces complex, high-quality components with excellent dimensional accuracy and smooth surface finishes.

What Is Lost Foam Casting?

Lost foam casting is a metal casting process that uses an expendable foam pattern to form the shape of the desired casting. The foam pattern is coated with a refractory material, and then the mold is surrounded by unbonded sand. Once the molten metal is poured into the mold, the foam evaporates (hencelost foam”), leaving behind a perfectly cast metal part that mirrors the original foam shape.

The foam pattern was first used in metalworking in 1958. Although this mold casting technique is not as popular as other methods such as sand mold casting or permanent casting, it maintains outstanding advantages, especially in casting complicated and precise molds.

Lost foam castings

The Lost Foam Casting Process

The lost foam casting process, similar to investment casting, is a highly efficient method used to produce complex metal parts with precise shapes. Here’s a brief overview of how it works:

casting with Lost Foam Coating

1、Stvaranje uzorka

The process begins by creating a pattern made from expandable polystyrene (EPS) foam. This foam pattern is a replica of the final part and is produced either by molding or machining the foam into the desired shape.

3、Premazivanje

The foam pattern is coated with a refractory ceramic material to provide a barrier between the foam and the molten metal. This coating ensures the casting’s dimensional accuracy and surface finish.

5、Ulijevanje

Molten metal is poured directly onto the foam pattern, causing the foam to vaporize. As the foam evaporates, the molten metal fills the void left behind, forming the final shape of the casting.

2、Montaža uzorka

If the part is complex, several foam pieces can be glued together to form a complete pattern. Sprues and gates (channels for the metal to flow through) are also added to the foam pattern.

4、Molding

The coated foam pattern is then placed into a container and surrounded by unbonded sand, which supports the foam and helps maintain the shape during the metal pour.

6、Cooling and Removal

Once the metal has solidified and cooled, the casting is removed from the sand mold. Minimal post-processing is required, as the lost foam method produces smooth, near-net-shape castings.

Lost Foam Casting Materials

Na ovom, proizvodimo složene dijelove od širokog spektra metala. Naš tim je predan kvalitetnom preciznom lijevanju, i radimo s raznim metalima kako bismo proizveli komponente prema vašim točnim specifikacijama. Neke opcije materijala od legura za precizno lijevanje uključuju:

Završna obrada glatke površine

The refractory coating applied to the foam pattern helps create a smooth surface finish on the final part, reducing the need for additional surface treatments.

Kompleksna geometrija

One major advantage of lost foam casting is its ability to produce intricate shapes and geometries, uključujući unutarnje šupljine, tanki zidovi, and fine details, which are challenging to achieve with traditional methods.

Minimal Machining

The precision of the foam pattern and the quality of the surface finish means that the cast parts require very little finishing work. This reduces the need for expensive post-casting machining processes and lowers overall production costs.

Cost-Effective for Large Parts

This method is especially cost-effective for large parts or high-volume production runs, where the cost savings from reduced machining and material usage add up.

Advantages of Lost Foam Casting

Lost foam casting offers several key advantages that make it a preferred method for producing metal parts with high precision and intricate details.

Lost Foam Casting Services

Custom Lost Foam Casting Parts

DEZE offers lost foam casting services, proizvodnja visokokvalitetnih metalnih komponenti po narudžbi. Korištenje raznih metala i legura, stvaramo složene i detaljne dijelove koji su isplativi i imaju visoke performanse, dizajniran da zadovolji vaše specifične zahtjeve.

Applications of Lost Foam Casting

Lost foam castings are highly valued across industries due to their ability to produce intricate shapes, smooth surfaces, and precise dimensions. It is especially useful for creating components with internal cavities, tanki zidovi, and complex structures that traditional casting methods struggle to achieve.

Zrakoplovna industrija

kao što su okviri zrakoplova, dijelovi stajnog trapa, komponente interijera, itd.

Automobilska industrija

Komponente motora, slučajevi prijenosa, kotači, strukturne komponente, itd.

Roba široke potrošnje

kao što je posuđe, Elektroničke kućice, ukrasni predmeti, itd.

Mornarica

kao što su oprema za čamce, propeleri, i brodski hardver, itd.

Završnica površine na jednom mjestu

Poboljšajte performanse svog dijela odabirom visokokvalitetnih površinskih završnica koje povećavaju hrapavost, tvrdoća, kemijska otpornost, i kozmetičke značajke vaše gotove komponente.

Lost Foam Casting Products Display

Na ovom, we specialize in lost foam casting services for industries such as automotive, zrakoplovstvo, i proizvodnja. Our advanced techniques and equipment ensure precision-cast components that meet your exact specifications. Whether you need intricate parts with complex geometries or high-quality castings for demanding applications, we have the expertise to deliver outstanding results.

Aluminum Casting Oil Filter Parts
Aluminum Casting
Al Die Casting automobile
Alu casting dz
Alu die casting dz
Al die casting
Alu die casting
Alu die casting

Stavite svoje dijelove u proizvodnju danas!

Pomaknite se na vrh