ʻO ka pololi (loko, kikowaena kikowaena a me nā micro-shrink) ʻo ia kekahi o nā hewa pinepine a me nā hopena kūponoʻole (nalowale-wax) ʻO nā mea kūʻai aku i nā mea kūʻai aku o nā meaʻili.
ʻO ka hemahema ka meaʻole i hikiʻole ke hoʻopili i ka hoʻoikaikaʻana i nā'āpana (Nā Vilves, Nā kino kino, Nā'āpana kūpono) Ma kahi e lele ai nā leaka a iʻole nā hōʻeha hōʻeha.
ʻO kēiaʻatikala e pili ana i ka pono, ʻO kaʻike ma kaʻenehana-papa inoa a me nā pilikia e hoʻopau ai i nā hana e hoʻopau ai a hōʻemi paha i ka poshity shriklest.
1. Nā kumu kumu - he aha ka mea e hoʻonani ai i nā mea kūʻai aku i hoʻopaʻaʻia?
Shrinkage posterity ma ke kila kila Kālā Pūnaewele ʻaʻole heʻano hana kūʻokoʻa hoʻokahi akā akāʻo ka hopena o kekahi mau hui pūʻana me nā mea hana metallirgical a me nā mea hana.

Nā mea hoʻokele intrinsic (alloy a hoʻoponopono paʻa)
Ka nui o ka hoʻokaʻawaleʻana i ka nui
- Nui nā hōʻailona nui o ka heluʻana i kaʻaeʻana i ka hōʻoiaʻana. ʻO ka shlaintic maʻamau maʻamau no nā austenitic maʻamau aneane 4-6%, ʻoi aku ka nui ma mua o nā alloys he nui.
E hana ana i kahi koi kiʻekiʻe no ka meaʻai wai wai e uku ai i ka loaʻaʻana o ka nui.
Nā Mushy Zone & 'ili'āmiʻili
- Hōʻike pinepineʻo Austentitics Austentitics i kahiʻano liʻiliʻi o ka wai-solidus indeal a iʻole ke kauʻana i kahi kūlana paʻa ".
Hiki i kahi mea paʻa i keʻano ma mua i ka neʻeʻana o ka underface a me nā'āpana interdendritic i loko o ke kikowaena, Ke pale nei i ka hānaiʻana a me ka hanaʻana i ka shriknicage interdendritic.
ʻO ka hoʻoponoponoʻana a me nā micro-segregation
- Nā mea hoʻonā i nā mea i hoʻokaʻawaleʻia i ka wai interdendritic i ka wā hoʻoponopono.
ʻO kēlā mau wahi wai wai hope loa a me nāʻano hana intercondected interdendritic; I ka wā e pau ai ka hānaiʻana, ʻO kēia mau wahi i kauʻia i nā'āpana shlenist.
ʻO ka haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa
- ʻO ka neʻeʻana o Molten maʻamau e holo liʻiliʻi ma mua o ka alumini a iʻole ke keleawe (ʻO ka lōʻihi o ka lōʻihi o nā fridities furelal no ka mea ponoʻole ma ~ 1500 ° C i ke kauoha o 300-350 mm).
Hoʻopilikia ka nui o ka lehulehu i ka hiki ke hoʻopiha i nā'āpana likeʻole a hānai i nā wahi wela.
Nā mea kūʻai aku
- Nā Koho Auli (Mo, I) E hoʻomaikaʻi i ka hoʻomaikaʻiʻana a iʻole ka ikaika e hōʻemi i ka wai a me ka laulā i ka hana manuahi manuahi no kekahi mau mea hoʻohui.
ʻO kekahi mau mea i loaʻaʻole ai i nā chemissitation a iʻole duplex paha i nā neʻe manuahiʻole a me nā pilikia e hoʻopiʻi nui ai i nā pilikia.
Nā mea hoʻokele extrins (Hoʻolālā, mold a me ke kaʻina)
Nā punawai i kohoʻia
- Nā'āpana ākea, Hoʻololi nā helu hoʻopau, nā lua i hoʻopiliʻia a me nā wahi i hoʻokaʻawaleʻia a iʻole e lilo i nā wahi wela.
Ināʻaʻole e hānaiʻia kēia mau'āina, ʻO nā kikowaena kikowaena nui a iʻole ka interdendritic. - ʻO ke kānāwai kūpono: Hoʻopau i nā hoʻokūkū ākea (E.g., 10 → 25 mm ma luna o kahi lōʻihi pōkole) E hoʻomau i ka hopena wela wela.
Hana houʻana a me ke alohaʻana
- Nā'ōlelo / me nā mea i hoʻopiliʻia, waiho hewa, a iʻole ke keleponaʻana o ka mea i hikiʻole ke hāʻawi i nā mea hao wai e uku ai i ka shriknized kūloko.
Ke haʻalele nei i nā ala kūpono (I.e., Pono ka metala e pono ai mai ke ala mamao loa e hiki ai i ka'ōlelo) he kumu kumu kumu.
ʻO Mold Shell a me nā pilikia pili
- ʻO Colley Cold / maikaʻi loa: Hōʻea i ka momona o ka bilill ke kumu i ka hoʻomehana wela wikiwiki a me nā pōkole i ka puka makani.
- ʻO nā mea nui a iʻole nā mea i loaʻaʻole i nā waiwai luhi: hiki ke kumu i ka hoʻoponopono ponoʻole.
- ʻO ka pōʻino a iʻole ka maikaʻiʻole: nā mea i pauʻole, ʻaʻole hiki ke hoʻokaʻawaleʻia aʻaʻole paha e hoʻopili pono i ka hānaiʻana a hana i nā ala i hoʻopaʻaʻia.
ʻO ka meaʻai maikaʻi / Riser Thermal hoʻolālā
- ʻAʻohe leo, liʻiliʻi loa (modulus haʻahaʻa loa), a iʻole ka hemahema o exothermic / insulating i nā hana e pili ana i ka mea kanu i hanaʻia ma mua a iʻole me ka wahi wela (I.e., Hoʻopau nā hānai).
ʻO ka hoʻomaʻamaʻaʻanaʻana
- Lawa ole superheat a iʻole ka haʻahaʻa haʻahaʻa.
- Turbulence nui a iʻole slashing → oxide estanintment (pifilms), ka mea e hoʻopili ai i keʻano metallurgical a hoʻopaʻa i nā mea hana maikaʻi maikaʻi loa.
ʻO ka maikaʻi: ʻO nā hau a me nā incousions
- Nāʻanuʻu (H₂, OAHO) hana i nā pres spical spical; Ke hui pūʻia me ka hoʻololiʻana i ka hoʻoponoponoʻana i ka hana a lākou i hana ai i ka hanaʻole.
- Nā meaʻole-metallic a me nā bifilms hana i nā wahi paʻa a hana e like me nā pūnaewele nuklebation no nā pūnaewele shleinge. ʻAʻole hiki i ka hoʻopiliʻana o ka mea hao i nā mea maikaʻiʻole e hānai i nāʻoihana pūnaewele interdendritic.
Nā mea hana a me ka hoʻopioʻana
- Hoʻopiliʻia (Nohoʻo Wax, Shell Dust, swarf) a iʻole ka hoʻohana ponoʻoleʻana i nā mea hana carbon-kila e hiki ai i nā kiʻi corrossion a iʻole ka posterity i ka wā e hoʻoponopono ai a hiki ke hoʻopauʻia me ka ho'ōlaʻana i nā channels.
ʻO nāʻano hana kūponoʻole - pehea ke kumu o ka launa pūʻana
ʻO nā hopenaʻo Poissity i nā hopena mai lehulehu nā nāwaliwali e hana pū ana: E.g., he wahi wela + ʻO ka hōʻikeʻana + low pour marp + trapd hydrogen. Hiki i kekahi kumu ke ukuʻia no ka mea he ikaika nā mea'ē aʻe; ʻO nā kūlana marginal he nui e hānai ai i ka hiki ke hana a hana i ka pososity.
2. Ke kū pololei nei ka hewa
Ma mua o ka hoʻololiʻana i ke kaʻina hana a hoʻolālā paha, E hōʻoia i ka mea āu eʻike nei.
Nā Diagnostics maʻalahi:
- Nānā'ōwaho & PAUKU: Keʻoki nei i ka hukiʻana ma o kaʻaoʻao o ka mea i hōʻike pinepineʻia i kahi lua nui (Lohi) a iʻole he pūnaewele o nā microbavities (michiposoity).
- Hoʻoili pūnaewele / Ct: Hōʻike nā radiographs i ka nui o ka nui a me kahi wahi; Maikaʻi loa ka ct no ka paʻakikī o nā geomex kūloko.
- Hoʻolālā Metal: Hiki i ke microscopy ke hoʻokaʻawale i ka shninkritic interdendritic mai keʻano o ke kino (ʻO nā PREAR PREARICS PRESS vs. Nā kāpena incontendritic Brand).
- Kekau & Hōʻike Hōʻike Pūnaewele: E nānā i nāʻike hydrogen, Melt maʻemaʻe, e ninini superheat, nā lāʻau lāʻau a me nā hoʻolālā hoʻolālā.
ʻO ka lula wehewehe: Inā he mau kaʻa kaʻa me nā ala i halaʻole a hōʻike i nā pā dendritic → e hānai i nā hemahema. Inā he mau leka uila a me nā mea e hoʻokaʻawaleʻia.
3. Hoʻolālā (ʻO ka laina mua a me ka hapa nui)
ʻO ka hapanui o nā pilikia shriknika i hoʻoponoponoʻia ma mua o ka hoʻolālāʻana ma mua o ke kaʻina ahi.

Hoʻolau i ka hoʻoponopono hoʻonohonohoʻana
- E kau i ka hānai (nā mea hānai / nā mea kanu) No laila e holomua ana kēlā paʻaʻana mai ke ala mamao loa i ka mea hānai.
I ka nalowale-wax, E noʻonoʻo i ka hoʻonohonohoʻana o nā kiʻi wela o waho, nā mea kanu i hoʻopaʻaʻia a iʻole exothermic moe i nā wahi koʻikoʻi. - Maʻalahi ke kauʻana: E hōʻemi i nā wahi wela wela (nāʻeke e kū pono ai) Ma ka hoʻololiʻana i nā geometry, hoʻohui i nā thimmal thermal a iʻole nā passicages kūloko e hana ana i nā mea hānai.
Hōʻalo i nā hoʻololi i ka pauku e loli a me nā wahi wela
- E hana i nā pā pōhaku kahi i kūpono; ʻO nā'āpana o nā wahi ākea he nui a me nā mea e pono ai e hānai.
- E hoʻohui i nā kīʻaha, Nā unuhi kiko'ī a me nā radii ʻaʻole ma mua o nā kihi koʻikoʻi e hōʻemi ai i ka wela wela i ka kahe wela a hoʻomaikaʻi i ke kaheʻana o ka aila i ka wā e hoʻopiha ai.
Hāʻawi i ka hānaiʻana i ka momi no nā lua kūloko
- Hoʻolālā i nā mea hānaiʻole-pale waho a iʻole kaʻili, Hoʻopau i nā hoʻonui i kahi e hikiʻole ai ke hānai i loko.
No nā kumulāʻau kūloko, E hoʻohana i nā mea hānai cemic (insround) a iʻole hoʻolālā e hoʻopili ai i nā plugs liʻiliʻi liʻiliʻi. - Nā Kūlana Kīpela & kūhewaʻi: e hōʻoia i kākoʻoʻia nā code chemic akāʻaʻole i luna; Pono e hoʻolālāʻia nā chalapts no lailaʻaʻole lākou e hana i nā mea paʻa paʻa i ka shrik.
4. Hānai i ka hoʻolālā'ōnaehana - hānai i nā pono o ka hale kūʻai
ʻO ka hānaiʻana ka naʻau o ka paleʻana i ka paleʻana.
- Chilulus (KBVorinV) kānāwai: ʻO ka nui o ka nui o kā lākou modulus M_rister ≈ 1.2-1.5 × m_casting (wahi wela nui loa). E hōʻoiaʻiʻo i ka mea i hoʻopaʻaʻia ma hope o keʻano o ka mea kūʻai aku e hānai ai.
- Nāʻano pōhaku & Ka ana: E hoʻohana i nā kiʻi kiʻi kiʻekiʻe no nā wahi wela; ʻO nāʻaoʻao hema no nā wahi wela wela. E kau i nā mea e hānai pololei ai i nā helu koʻikoʻi.
- Exothermic and insulated rentiers: ʻO Exothermic Ringers e hoʻonui i ke ola wai e 30-50%; ʻO nā moe i hōʻoleʻia e hōʻemi i ka nalowale wela.
- ʻO nā mea kaulike he nui: No nā'āpana cylindrical a iʻole symetric paha, E hoʻohana i ka 3-4 mau mea i hōʻehaʻia i ke kaheʻana i ke kahe a hōʻemi i nā ala lōʻihi lōʻihi.
- Hoʻolālā Rlaner: Hoʻopiliʻia nā mea holo kaʻa i paʻiʻia; Hōʻalo i nā koina a me nā hōʻemi wikiwiki. No nā mea liʻiliʻi e mālama i nā'ōmole runnener ≥ 8 mm E like me ka liʻiliʻi liʻiliʻi.
5. ʻO nā hana hana hanana
Nā loli liʻiliʻi i nā hopena hana he nui nā hopena nui.

- Hill Preheat: no ka mea austetetic (E.g., 316/316L) preheat sheell to 800-1000 ° C; No ka hoʻohanaʻana o nā hale kūʻai artness / pr 600-800 ° C.
Ua hoʻolōʻihiʻiaʻo Prenaat Pretaat i ka liloʻana i ka momona a hoʻonui i ka manawa hānai. Pale aku i luna (>1100 ° C). - Ka nininiʻana & superhaeat: Kaukai ~ 100-150 ° C ma luna o ka wai ma luna o ka alloy a me ka'āpana. Hoʻoloholo: 316L nininiʻia ma ~ 1520-200-00 ° C (± 5 ° C ka mana no nā'āpana koʻikoʻi).
Hoʻonui ka nui o ke kino kiʻekiʻe (Kōkua i ka hoʻopiha a hānai) Akā e hoʻonui i nā kaulike-kaulike. - Kāohiʻia hōʻoluʻolu: No nā'āpana kaumaha, ka hoʻoweliweliʻana i kaʻili ('ōwili) No 2-4 mau hola ma hope o ka hoʻonuiʻana i ka pour i ka nui o ka gradient a me nā mea kōkua i ka hānaiʻana. Pono e paleʻiaʻo Rapid Quech.
- Geting a hoʻopiha i ka mana: hoʻokūpaʻa, Hoʻopiha nā laminar i ka hōʻemiʻana i nā laps maloʻo a hōʻemi i keʻano o ka hoʻokaʻawaleʻana i nā ala nui.
6. ʻO ka maikaʻi a me nā mettallurgy - wehe i nā pūnaewele nukle
ʻO nā kīwī a me nā meaʻoleʻole-metallic invousens in molten i kahi mea kila kila e like me nuclei no ka bhclei no ka bhching, No laila, he mea pono keʻano o ka mana o Molten Chelat maikaʻi loa:
- E hōʻoluʻolu i ka hoʻolālāʻana: E hoʻohana i ka hoʻopaʻapaʻa argon-oxygen (Aod) a iʻole ka paleʻana o ka oxygen oxygen (Vod) e hoʻoponopono hou i nā kila kila, Ka hōʻemiʻana i ka kalapona, Sulfur, a me nā meaʻona (H₂ ≤ 0.0015%, O nana.≤ 0.002%).
No ka hana liʻiliʻi-batch, E hoʻohana i kahi'ōkuhi e hōʻole i ka hulu (Lrf) me nā slags synthetic (Cako-al₂o₃-sio₂) e wehe i nā incusions non-metallic. - ʻO ka degusing a me Deslagging: Hana i ka pana pua (kahe kahe 0.5-1.0 l / min per i kēlā me kēia o ke kila) No 5-10 mau minuke ma mua o ka nininiʻana e wehe i ka hydrogend hydrogen.
Skim slag slag maikaʻi loa mai ka papa papa e pale ai i ke komoʻana i ka slag, e kumu ana i ka pololi a me na manao. - Kāohi i nā hoʻohui alloy: Hōʻalo i ka hoʻohui nui o nā mea'ē aʻe (E.g., Mo, I) e hōʻemi i ka wai. E hoʻohana i nā lako hana kiʻekiʻe kiʻekiʻe (hoʻomaʻemaʻe ≥ 99.9%) e hōʻemi i ka hōʻoiaʻana.
7. Ke koho nui & Nā koho post-hoʻoiho
Inā hikiʻole i nā ana ke hoʻopau i ka hoʻopauʻana i ka shrink i ka wā a iʻole ke koiʻana o ka beroosity:
- ʻO ke kaomiʻana o ka wela wela (Hip): ʻO keʻano maʻamau o ka hip o ka hip 1100-1200 ° C a 100-150 mpa no ka 2-4 hola.
Ua hoʻohuliʻo Hip i nā leo kūloko kūloko, hoʻokō i nā huaora ≥ 99.9%, a hoʻihoʻi hou i ka hōʻeha a me ka hoʻokōʻana. ʻO ka hip ka go-to sults no ka aerospace a me nā'āpana koʻikoʻi. - Kaomi / centrifugal e kāhea ana: ka hōʻoia paʻaʻana (Ke noi nei i ke kaomi i ka wā hoʻomaha) a iʻole nāʻano variafugal ke hōʻemi i ka poosity no kekahi mauʻano, ʻOiai ke koiʻia nā loli a me nā loli.
- Nā hoʻoponopono kūpono: Hiki i ke Gtaw me Er316L Filler e hoʻoponopono hou i ka heleʻana o ka heleʻana ma hope o ka nānāʻana a me ka hana wela wela; ʻaʻole kūpono no nā hemahema o loko i nā'āpana ikaika.
- Hoʻohuiʻia: ʻO Recast nā ponaʻo Hip i kekahi manawa ke ala wale nō eʻaeʻia no nā'āpana me nā'āpana me ka hoʻihoʻiʻana i loko.
8. Honua mālamalama, Manaʻo & 'opau
E hoʻonohonoho i nā loiloi kūpono a hōʻoia i ka hoʻokō.
- Ndt: radiography no nā hana kūloko kūloko, Ct no nā geometus paʻakikī, Uti no nā hemahema nui. E wehewehe i kaʻaeʻana (E.g., ʻaʻohe leo > X mm, ʻO ka polomity kiʻi < Y%).
- ʻO ka nānāʻana o ke metallographic: E hōʻoia i ka morphology Pore (interdendritic vs gas) Ke pilikia nei.
- Nā hōʻike hoʻokolohua hoʻokolohua: tersele, hua, ewangantion, a me ke kaomi / Leak e hōʻike ana i nā'āpana paʻakikī; Pono pinepine ka hip i ka hoʻomehanaʻana a iʻole ka hōʻoiaʻana i ka hōʻoia.
- Ke kaʻina hana & Spc: E kākau i ka stiret preheat, mea ' & No nā wela, ʻO nā manawa hana, nā'āpana a me nā wahi; ʻO nāʻano kiko'ī statistically e hoʻokaʻawale i nā mea e pono ai.
9. Kālā Kū'ē Manaʻo (hoʻomālamalama): Hoʻopau i ka shlening Valve-noho i ka lā 316l Valve kino
Pilikia: 316L valve kino (ka helu ikaika 10 Mpa) hōʻikeʻia i nā kāhiko shlik i hōʻikeʻia ma ka noho Valve (22 mm Wall), kumu 15% Andivage.
Nā hana
- Hoʻokaʻawale i ka 22 mm wela i loko oʻelua mau'āpana x x mm me a 3 MM RIB a me kahi hoʻololiʻana.
- Hoʻohui i kahi kiʻi kiʻi exothermic kiʻekiʻe me Modulus 2.0 cm a me nā mea hou i hoʻopaʻaʻia e hānai i ka wahi wela.
- Hoonui hou i ka stream rat mai 750 → 900 ° C a hoʻonohonoho i ka nininiʻana 1540 ± 5 ° C.
- Ua hōʻoleʻo Vod + ʻO Argon Tenging (8 min) e hōʻemi h₂ ≤ 0.001%.
Hopena: Ua hāʻule i kahi kūlana shrink 2%, Hoʻokuʻuʻiaʻo Leakage, Nā Kūlana Kūlana Kūlana ~ 8-10% - Hana Hou a me ka Hana Kūʻai Kūʻai a me nā Mea kūʻai aku.
10. ʻO nā kumu nui a me nā hana maikaʻi loa no ka paleʻana i ka poosiny
ʻO kēia'āpana'āpana i nā lula o kaʻenehana, ʻO nā papa hana a me nā hana hana a me nā hana e pale pū ai i ka paila shrink i loko o nā hale kūʻai waiwaiʻole.
Nā Kūlana Coripers (ka "kumu" ma hope o nā hana a pau)
- Hoʻolālā e hānai, ʻaʻole e nānā maikaʻi. ʻO ka pahuhopu mua o ka geometry e hiki ai i keʻano o ke aniani a me ke kahe waiʻole i loko o ka wai.
Inā hoʻokumu ka hoʻolālā i nā wahi wela, ʻO nā mea hoʻohālike e mālama ponoʻole i ka paleʻana. - E hoʻohālikelike i ka hana hānai e koi i ka noiʻana. E hoʻohana i ka modulus (KBVorinV) Keʻano o nā ala nui e hōʻike ai i nā mea e hānai ai i ka wahi wela a lākou e hānai ai (rula maʻamau: M_rister ≈ 1.2-1.5 × m_casting).
- E kāohi i ka Timmal Timeline. Ka manawa paʻa (Hill Preheat, No ke kauwela, esulation /ʻoluʻolu) E wehewehe i ka puka makani.
Hoʻokele i kēlā mau hiʻohiʻona i manaʻo maikaʻiʻia e mālama ai i kahi e pono ai. - E hoʻopau i nā pūnaewele nussity Plclesity ma ka Melt. ʻO nā helu hydrogen haʻahaʻa a me nā mea haʻahaʻa haʻahaʻa e hōʻemi ai i ka hopena o keʻano o ka wai incondendritic.
- Ana, simulate a metate. E hoʻohana i ka Simonition Simulation i mua a me nā pahuhopu ndt & metallirgy ma hope o nā hoʻokolohua e hoʻopili wikiwiki ai i kahi subus robus.
- E piʻi i ka wā e pono ai. I ka wā e koi ai nā koina a me nā pono palekana a palekana paha e pili ana i keʻano o keʻano (nā'āpana ikaika, AerERPPACE), E hoʻokae i nāʻoihana waiwai o ka hopena holomua (Hip a iʻole ka hoʻololiʻana) ma mua o kaʻaeʻana i ka scrap recurrent.
11. Hopena
ʻO keʻano o ka pohō i loko kila kohu ʻole ʻO ka mea kūʻai aku i ke kūʻai akuʻana he mea paʻakikī i ka mea paʻakikī e nā mea hoʻoponopono kūpono, ke kauʻana, a me nā kaʻina hana.
Hoʻoholo e pono ai i kahi'ōnaehana, ʻO ka hoʻomakaʻana o keʻano o ka hoʻopiliʻana i ka hoʻohālikelikeʻana, Hoʻolālā Hoʻomaluhia Pūnaewele, Ke kaʻina hanaʻana, a me ka hoʻomaikaʻiʻana i ka hoʻomaikaʻiʻana i keʻano maikaʻi o Moolten.
Ma ka piliʻana i nā loina o ke kuhikuhiʻana i ka hoʻoponopono hoʻonohonohoʻana, ho'ēmi i nā wahi wela, a me ke kūponoʻana i ka hana e pono ai e koi i ka koi, Hiki i nā mea hana ke hōʻemi nui i ka poshity shrinkistage a hoʻomaikaʻi i ka maikaʻi.
Lākahi, ʻAʻoleʻo ka hoʻonāʻana o keʻano o keʻano o ka pôpeku maikaʻi.