Ke neʻe nei nā robots humanoid mai nā hale hana noiʻi i ka ʻoihana, Kālepa, a ma hope o nā noi hale, ke koi no ka māmā, ʻO nā mea hana kiʻekiʻe e hana ana i nā manawa hou no ka ʻoihana hoʻoheheʻe make.
ʻO ka magnesium a me nā alumini alumini ʻelua mau mea waiwai nui no kēia mau noi. Hāʻawi nā mea ʻelua i ka castability maikaʻi, haʻahaʻa haʻahaʻa, a me ka hiki ke hana paʻakikī, nā mea hoʻohui.
Akā naʻe,, ʻaʻole lākou hana like, a ʻaʻohe mea kūpono no kēlā me kēia subsystem robotic.
ʻO ke kuhi hewa maʻamau i ke koho ʻana i nā mea waiwai, ʻo ia ka manaʻo e like nā mea i hoʻolei ʻia i loko o kahi robot humanoid i nā mea nui: mea momona haʻahaʻa, ʻoʻoleʻa kiʻekiʻe, lawa ka ikaika, a me ke kumu kuai haahaa.
I ka hoʻomaʻamaʻa, ʻokoʻa nui nā koi e like me ka wahi a me ka hana.
He ʻokoʻa nā mea nui o ka hoʻolālā ʻana o ka hale lima lima ʻeleʻele mai kahi hale hui puʻupuʻu haʻahaʻa a i ʻole kahi mea i kūkulu ʻia kokoke i ke kumu o ka robot..
Nānā kēia alakaʻi i nā ʻokoʻa ma waena o ka magnesium a me nā alumini alumini no hoʻoheheʻe robotics, wehewehe i ka ʻokoʻa o nā koi ma waena o nā subsystem robot humanoid, a kūkākūkā pehea e hiki ai i nā ʻenekinia make make ke hoʻomohala i nā ʻōnaehana hana kūʻai kūpono no kēia mau noi e kū nei.
1. ʻO ke Kumukānāwai Māhele: Nā ʻāpana like ʻole, Nā Koina like ʻole
ʻO ka hana mua i kēlā me kēia papahana hoʻolei robot e hoʻokaʻawale i ka robot ma o ka hana. Hōʻuluʻulu ka papa ma lalo i ke ʻano ākea aʻu i ʻike ai ma nā papahana.
| Wahi Lopako | Koi Kumu | Mānoanoa Pā maʻamau | Manaʻo Kaʻina |
| lima lima, lima lima, hopena hopena | nuipa liʻiliʻi, ʻoʻoleʻa kiʻekiʻe | pā lahilahi, 1.5–2.5 mm | HPDC, hiki i ka paia lahilahi |
| lima luna, Pahu | Luhi, nuipa haʻahaʻa | 2–3 mm me nā iwi ʻaoʻao | HPDC, semi-paʻa |
| Kukū, ʻūhā | Luhi, lawe ukana | 3-5 mm | HPDC, semi-paʻa |
| Base, kino lalo | Kūlākuai, kikowaena haʻahaʻa o ka ʻumekaumaha | Nā'āpana ākea, 5-10 mm | Semi-paʻa, Gravity |
| Nā hale hui | ʻAʻa, hoopau wela | 3-6 mm | HPDC me nā mea hoʻokomo |
| ʻIke ʻia nā panela waho | Aesttheticcs, hoʻopau | 1.5-3 mm | HPDC, poni/anodized |
2. ʻO ka Magnesium vs Aluminum Alloys: Nā ʻokoʻa waiwai kumu
ʻO ka Magnesium a me ka alumini ka mea maikaʻi no nā mea hoʻoheheʻe māmā, akā, ʻo kā lākou mau hiʻohiʻona kino a me ka mīkini e alakaʻi i nā manawa hoʻolālā like ʻole.
Hāʻawi ka magnesium alloys i kahi haʻahaʻa haʻahaʻa, e hoʻohiwahiwa ana iā lākou no ka neʻe ʻana o nā ʻāpana kahi e hōʻemi ai ka hoʻohaʻahaʻa nuipaʻa i ka inertia rotational.
Hāʻawi pū lākou i nā hiʻohiʻona vibration-damping maikaʻi a hiki ke hoʻolei ʻia i loko o nā geometries paʻakikī paʻakikī.
Hāʻawi nā alumini alumini i ka modulus elastic kiʻekiʻe, ʻoi aku ka ʻoi aku o ka ʻoi aku ka ʻoi aku o ka ʻoʻoleʻa ma ka geometry like, a me ka conductivity wela maikaʻi.
Hāʻawi pū lākou i kahi ākea o nā mea hoʻoheheʻe i hoʻokumu ʻia, nā mea kino kino, a me nā hoʻonā mīkini.

Hoʻohālikelike waiwai kī
Hāʻawi ka papa ma lalo nei i nā pae ʻenehana hōʻike. Pili nā kumu waiwai maoli i ka pae alloy, Ke kahua nei, mānoanoa ʻāpana, ʻO ka mālama wela, a me nā kūlana hoʻāʻo.
ʻAʻole pono lākou e pani i ka palapala hōʻoia waiwai a i ʻole ka ʻikepili hoʻolālā pae ʻāpana.
| Waiwai | MAKENESIM ALLOYS | Apana Apana Aluminum | Pili i nā lopako |
| Huakai | Ma kahi o 1.74–1.85 g/cm³ | Ma kahi o 2.65–2.80 g/cm³ | Hiki i ka Magnesium ke hoʻemi i ka nui o nā ʻāpana ma ke ʻano 30% hoʻohālikelike ʻia me ka alumini ma ka nui like. |
| Modulus elastic | Aneane 45 GPA | Ma kahi o 69–72 GPa | Hāʻawi ka alumini i ka ʻoʻoleʻa ʻoi aku ka nui ma ka geometry like. |
| ʻoʻoleʻa kikoʻī (E/r) | Ma kahi o 24–26 GPa/(g / cm³) | Ma kahi o 25–27 GPa/(g / cm³) | ʻOi aku ka liʻiliʻi o ka pono ʻoʻoleʻa o ka alumini ke hoʻohālikelike ʻia e ka density. |
| Ka HōʻaʻO Kokua | Ma kahi o 50–100 W/(m · ALOHA Kina), alloy-hilinaʻi | Ma kahi o 90–220 W/(m · ALOHA Kina), alloy-hilinaʻi | ʻOi aku ka maikaʻi o ka alumini no nā hale hoʻolaha wela. |
| Kuʻi haʻalulu | ʻOi aku ka kiʻekiʻe | Haʻahaʻa haʻahaʻa | Hiki i ka Magnesium ke kōkua i ka hōʻemi ʻana i ka hoʻoili ʻana i ka haʻalulu i nā hui neʻe. |
| Pūnaewele kūleʻa | Pono ka pale alo a me ka pale ʻili | ʻO nā koho pale corrosion maʻamau | Pono e noʻonoʻo ʻia ka mālama ʻana i ka ʻili a me ka ʻike ʻana i ke kaiapuni. |
Whola |
Maikaʻi no ka pā lahilahi, ʻāpana māmā me ka mana kaʻina hana kūpono | Maikaʻi no ka paʻakikī, nā mea hoʻohui; alloy-hilinaʻi | Hiki iā lāua ke kākoʻo i nā geometries die-cast paʻakikī. |
| Markinpalibility | Ka mea maikaʻi, akā, he mea nui ka mana puʻupuʻu a me ke ahi | Ka mea maikaʻi, me ka ʻike ʻoihana nui | Kākoʻo lāua ʻelua i ka mīkini pololei o nā noho halihali a me nā pilina. |
| Ke hoʻopauʻana | Pono ke kaʻina hana-specific pretreatment a me ka pale | Nui nā koho hoʻopau i hoʻopaʻa ʻia | He mea nui no nā hale robot i hōʻike ʻia a me nā panela waho. |
He ʻokoʻa koʻikoʻi: ʻAʻole hiki i ka haʻahaʻa haʻahaʻa o Magnesium ke hoʻomaʻamaʻa i ka hoʻolei ʻana i ka magnesium i kāna noi hoʻolālā hope.
No ka mea, loaʻa i ka magnesium ka modulus elastic haʻahaʻa, makemake paha nā ʻenekinia i nā pā mānoanoa, iwi ʻaoʻao hohonu, a i ʻole ka hoʻoikaika hou ʻana e hoʻokō i ka ʻoʻoleʻa pono.
No laila, pono e loiloi ʻia ka pono kaumaha hope ma hope o ka hoʻolālā ʻana, ʻaʻole mai ka nui wale.
3. Makana māmā: No ke aha e ʻoluʻolu ai ka Magnesium no ka neʻe ʻana i nā ʻāpana Robot
I nā lopako humanoid, ʻO ka hoʻemi ʻana i ke kaumaha o nā ʻāpana neʻe he mea koʻikoʻi loa ia no ka mea e pili pono ana ko lākou nuipa i nā ukana actuator a me ka hoʻohana ʻana i ka ikehu..
Ke hohola ka lopako i kona lima, ʻoi aku ka lōʻihi o ka ʻāpana mai ka hui poʻohiwi, ʻoi aku ka nui o kāna hāʻawi ʻana i ka inertia rotational.
Ma ka hopena, ʻoi aku ka nui o ke kaumaha o ka forearm ma mua o ka manaʻo o kona nui wale.
Pono nā poʻohiwi a me nā kuʻekuʻe e kākoʻo ʻaʻole i ke kaumaha o ka lima wale nō akā i nā ikaika hou i hana ʻia i ka wā o ka wikiwiki., hoʻoemi, a me ka lawelawe ʻana i ka ukana.
ʻO ka hoʻohaʻahaʻa ʻana i ka nui o ka hana lima hiki ke hoʻohaʻahaʻa i nā koi actuator, hoʻomaikaʻi i ka neʻe ʻana, a i ʻole e hoʻonui i ka hiki ke loaʻa ka uku uku o ka robot.
ʻO kēia kahi e lilo ai nā mea hoʻoheheʻe magnesium a me ka hoʻoheheʻe ʻana i nā paia lahilahi. Kōkua ka haʻahaʻa haʻahaʻa o Magnesium e hōʻemi i ka nui o nā mea, ʻoiai ke kiʻekiʻe-press die casting (HPDC) hiki ke hana i nā hale paʻakikī me nā paia lahilahi, Hoʻopili i nā iwi, a me nā hiʻohiʻona kau ʻana.

Nā Manaʻo Hoʻomaʻamaʻa no ka HPDC Paʻa Māmā
Pono ka hoʻolālā ʻana i ka pā lahilahi e kaulike i ka hoʻemi ʻana i ke kaumaha me ka hiki ke hoʻolei ʻia a me ka hana hoʻolālā:
- Hoʻopiha i nā palena:Ka mānoanoa o ka pā ma lalo 1.5 mm hiki ke paʻakikī ke hoʻopiha pono, ʻoiai ke hele lōʻihi ka metala i hoʻoheheʻe ʻia ma o ka lua make.
- ʻOoleʻa kūpilikiʻi:ʻO ka hoʻohaʻahaʻa ʻana i ka mānoanoa o ka pā e hōʻemi ana i ka ʻoʻoleʻa. Pono ka hoʻoikaika ʻana i nā iwi ʻaoʻao a me ka topology optimization e hoʻomalu i ka deformation.
- Rapid holoi:Hoʻomaʻalili koke nā ʻāpana lahilahi, hoʻonui i ka pilikia o nā pani anu, hoʻopiha piha, a maikaʻi ʻole ka maikaʻi o ka ʻili inā ʻaʻole mālama pono ʻia nā ʻāpana hana.
- Ejection a me ka lawelawe ʻana:ʻOi aku ka maʻalahi o ka hoʻoheheʻe ʻana i ka paia i ka deformation i ka wā ejection a me ka lawelawe ʻana ma hope, e koi ana i nā hoʻolālā ejector i hoʻolālā maikaʻi ʻia a me nā mea kākoʻo.
No nā hoʻolei lima robotic he nui, ʻO ka mānoanoa o ka pā ma kahi o 1.5-2.5 mm hiki ke lilo i mea kuhikuhi no ka hoʻolālā mua, pili i ka hao, Goody, lōʻihi kahe, a me ka mana make-casting.
He mea koʻikoʻi ke ʻano o ka iwi ʻaoʻao i hana pono ʻia.
He māmā paha ka pā lahilahi palahalaha akā ʻaʻole lawa ka rigidity; hiki i ka pā lahilahi i hoʻoikaika ʻia i ka iwi ʻaoʻao ke hāʻawi i kahi kaulike ʻoi aku ka maikaʻi ma waena o ka nuipa a me ka ʻoʻoleʻa.
4. Okoa ke Kumu: Paʻa ma luna o ka māmā māmā
ʻAʻole like me nā mea hoʻoneʻe e like me nā lima robotic, ʻO ka hoʻoheheʻe ʻana ma kahi kokoke i ke kumu o ka robot e hoʻokumu i ka paʻa ma mua o ka hoʻemi kaumaha.
ʻO ka nuipa kūpono ma ka hopena haʻahaʻa o ka hale e kōkua i ka hoʻohaʻahaʻa i ke kikowaena o ka umekaumaha, e hoʻemi i ka pilikia o ka ʻoki ʻana, a hoʻomaikaʻi i ke kūpaʻa i ka wā e hele ai, ke huli, a me nā neʻe ikaika ʻē aʻe.
ʻO ka māmā māmā ma kēia mau wahi hiki ke hoʻopilikia i ke koena o ka robot a me ke kūpaʻa haʻalulu.
NOEHUI, Hiki i nā ʻāpana kumu ke hoʻohana i nā pā mānoanoa a me nā ʻāpana i hoʻoikaika ʻia i ka wahi kahi e koi ai nā ukana kūkulu.
ʻO ka semi-solid rheocasting kahi koho kūpono no ia mau mea, ʻoiai ke hoʻohui ʻia kahi hoʻolei hoʻokahi i nā haku mānoanoa, wahi e kau ana, a me nā pūnaewele pili lahilahi.
ʻO nā pōmaikaʻi koʻikoʻi o ka rheocasting semi-solid no nā hoʻolei kumu lopako:
- ʻO ka politika haʻahaʻa:ʻO kona poʻo honua, hiki i ka microstructure non-dendritic a me ke kahe metala ke hoʻemi i ka porosity i hoʻohālikelike ʻia me ka HPDC maʻamau.
- ʻOi aku ka maikaʻi o ka mānoanoa kūpono:Hāʻawi ia i nā hoʻololi ma waena o nā ʻāpana mānoanoa a lahilahi, ke kākoʻo ʻana i ka hoʻoikaika kūloko me ka hana ʻole ʻana i ka ʻāpana holoʻokoʻa i ke kaumaha pono ʻole.
- Hoʻonui i ka hana mechanical:Hiki i ka hana ʻana i hoʻomalu pono ʻia ke hāʻawi i nā waiwai mechanical maikaʻi, me ka elongation a me ka luhi luhi.
- Hoʻemi ʻia ka hoʻopaʻa ʻana o ka oxide:ʻO ka hana hoʻopihapiha haʻahaʻa haʻahaʻa e kōkua i ka hoʻopaʻa ʻana i ka oxide-film entrainment a hoʻomaikaʻi i ka pono o ka hoʻolei ʻana.
He mea waiwai kēia hui ʻana o nā ʻano kaʻina hana no nā kūkulu kumu robot, kahi e makemake pinepine ai nā mea hoʻolālā i nā hiʻohiʻona haʻahaʻa haʻahaʻa ma ka ʻaoʻao o nā ʻāpana lahilahi e hoʻomalu i ka nuipa holoʻokoʻa a mālama i ka paʻa o ke kūkulu..
5. ʻO ka hoʻoheheʻe wela he hana hoʻolālā
Loaʻa i nā robots Humanoid nā mea hana he nui, nā pila, a me nā ʻāpana hana AI, ʻo ia mau mea a pau e hoʻoulu i ka wela i ka wā e hana ai.
ʻO nā hui haʻahaʻa kiʻekiʻe, pili loa i nā kuli a me nā pūhaka, hiki ke loaʻa i nā ukana wela nui.
Hoʻohui kekahi mau hoʻolālā robot i nā paipu wela kokoke i nā hui kuli e hāʻawi i ka hoʻoluʻu i manaʻo ʻia no nā mea hana kiʻekiʻe..
Ma ka hopena, ʻoi aku ka nui o ka hoʻolei ʻana ma mua o ke kumu hoʻolālā. Hiki i nā hale hui a me nā mea kākoʻo ke hana ma ke ʻano he ʻāpana o ka ʻōnaehana hoʻokele wela o ka robot.
No laila, lilo ka thermal conductivity i mea koʻikoʻi no ke koho ʻana i nā mea me ka ikaika, luhi, a me ka nui.
Hoʻokumu kēia koi i nā manawa hou no ka hoʻomohala ʻana i ka alloy.
Pono e kaulike nā alloys i ka wā e hiki mai ana no nā noi robotics, Ka HōʻaʻO Kokua, a me ka castability ma mua o ka nānā wale ʻana i ka ikaika a me ka ductility.
ʻO ka hoʻohālikelike hoʻohālikelike o ka alumini a me ka magnesium
| Alloy | Ka HōʻaʻO Kokua (W / m · c · k) | Nā hiʻohiʻona koʻikoʻi |
| A380 (Al-Si-Cu) | ~96 | Mea hoʻoheheʻe make maʻamau |
| A360 (Al-Si-Mg) | ~113 | ʻOi aku ka maikaʻi o ka pale ʻana i ka corrosion |
| A413 (Al-Ae) | ~121 | Ke alakaʻiʻana i ka thermal, ikaika haʻahaʻa haʻahaʻa |
| Am60 (Mg) | ~62 | ʻOi aku ka haʻahaʻa haʻahaʻa ma mua o nā alumini alumini |
| AZ91 (Mg) | ~51 | ʻOi aku ka haʻahaʻa haʻahaʻa ma mua o nā alumini alumini |
Hōʻike ka hoʻohālikelike i kēia mau alumini alumini e hāʻawi maʻamau i ka conductivity thermal kiʻekiʻe ma mua o nā alloy magnesium i helu ʻia.
ʻO kēia ka mea i kūpono i ka alumini no nā hale hui a me nā pā actuator e pono e hoʻoneʻe i ka wela mai nā kaʻa a me nā uila uila..
Noho maikaʻi ka Magnesium ma kahi o ka hoʻemi ʻana i ka neʻe nui ka pahuhopu nui, akā, ʻo ka haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa paha e koi aku i nā ana hoʻomaha hou ma nā wahi wela.
No nā ʻāpana me ka koi ʻana i nā koi wela-dissipation, ʻO ka alumini ka mea maʻamau ke koho kūpono; ʻoi aku ka maikaʻi o ka magnesium i ka wā e hoʻemi ʻia ke kaumaha a hiki i ka hoʻolālā wela ke hoʻokō i kona mau palena.
6. ʻOi aku ka rigidity ma mua o ka ikaika loa
ʻO kahi ʻokoʻa koʻikoʻi ma waena o ka hoʻoheheʻe robot humanoid a me ka hoʻolei ʻana o ka automotive maʻamau, ʻo ia ka manaʻo nui i ka rigidity structural ma mua o ka hoʻonui ʻana i ka ikaika waiwai..
Manaʻo nā mea hana ʻoihana i kēlā, no kekahi mau mea lopako, i ka manawa e hiki ai ka ikaika tensile i ka liʻiliʻi loa o ka noi 200 Mpa, ʻO ka hoʻonui ʻana i ka ikaika hiki ke hāʻawi i ka pōmaikaʻi liʻiliʻi ma mua o ka hoʻomaikaʻi ʻana i ka rigidity.
ʻO ka koi ikaika maoli e pili ana i nā kūlana hoʻouka o ka mea, Goody, a me ka mea palekana.
Hoʻoholo nui ʻia ka rigidity e ka hoʻolālā hoʻolālā. Hoʻoikaika i nā iwi ʻaoʻao, nā ala hoʻouka ʻoi ʻia, hoʻolālā hana, a hiki i ka topology optimization ke hoʻomaikaʻi i ke kūʻē ʻana i ka deformation me ka hilinaʻi wale ʻana i nā alloys ʻoi aku ka ikaika..
Hiki i kekahi mea ikaika kiʻekiʻe i loko o kahi hale hana maikaʻi ʻole ke hoʻohuli nui ʻia, ʻoiai ʻo kahi huila ikaika ikaika me kahi geometry i hoʻopaʻa ʻia e hāʻawi i ka ʻoʻoleʻa kūpono a me ka paʻa ʻana o ka dimensional..
Hāʻawi ka hoʻoheheʻe make i ka maʻalahi hoʻolālā ma kēia ʻano. Nā pūnaewele iwi ʻaoʻao paʻakikī, ʻano mānoanoa pā pā, a hiki ke hoʻohui pū ʻia nā haku kau i hoʻokahi ʻāpana, e ho'ēmi ana i ka pono no nā ʻāpana he nui a me nā hana hui lua.
ʻO ka luʻi koʻikoʻi e hōʻoia i ka hana ʻana o ka geometry i hoʻopaʻa ʻia a hiki ke hoʻokele waiwai i ka nui o ka hana i koi ʻia..
Nā Manaʻo Hoʻolālā Nui
- Hoʻolālā no ka hoʻolei ʻana mai ka hoʻomaka ʻana:E hōʻalo i ka hoʻololi wale ʻana i kahi mea mīkini i ka hoʻolei ʻana. Mānoanoa pā, Nā kihiʻihi, Nā Kūpono, a e noʻonoʻo ʻia nā laina hoʻokaʻawale i ka wā o ka hoʻolālā mua.
- E hoʻohana i nā iwi ʻaoʻao a me nā gussets:E hoʻoikaika i nā wahi koʻikoʻi e hoʻomaikaʻi i ka ʻoʻoleʻa me ka hōʻemi ʻana i nā mea hou aku.
- E hoʻopili i ka loiloi topology:E hoʻopaʻa i nā mea ma nā ala hoʻouka maikaʻi a wehe iā ia mai nā wahi i hāʻawi liʻiliʻi i ka hana hoʻolālā.
- E ʻimi i ka hoʻolālā generative:E hoʻomohala i nā geometries ʻē aʻe e hoʻohana pono i ka hiki o ka die casting e hana i nā hiʻohiʻona paʻakikī.
- E hōʻoia me FEA:E loiloi i ka deformation, ʻO ka hoʻokaʻawaleʻana, a me ka hoʻokō ʻana i ka haʻahaʻa ma o ka nānā ʻana i nā mea i hoʻopau ʻia ma mua o ka hoʻopau ʻana i ka hoʻolālā a me nā mea hana.
No nā papahana robotics, pono e kōkua ka mea hoʻolako make-casting i ke koho mea, manao hoolei, a me ka loiloi hana hana — ʻaʻole hāʻawi wale i kahi ʻōlelo i hoʻokumu ʻia ma ke kaumaha ʻāpana.
7. Kū'ē i ka hopena a me ka Ductility: Hoʻolālā no ka wailele ʻaʻole i manaʻo ʻia
No nā lopako humanoid bipedal, ʻAʻole lawa ka rigidity kūkulu wale nō. ʻAʻole like me nā lako paʻa, Pono kēia mau robots e mālama i ke kaulike i ka wā e hele ana, ke huli, a me ka lawelawe ʻana i nā mea, ʻo ia hoʻi, ʻo ka hāʻule ʻana a me ka hāʻule ʻana i kekahi manawa he mau manaʻo hoʻolālā hiki ʻole ke pale ʻia.
Hiki i kahi lopako ke kaupaona ʻana he 80-100 kg ke hoʻohua i nā haawe nui i ka wā e pā ai i ka lepo., e waiho ana i kona mau mea hoolei ma lalo o ka hoouka ana ma mua o ka hana maʻamau.
Hana kēia i ka elongation a me ka hopena i nā waiwai waiwai. Hiki i ka ho'ohehe'e ha'aha'a ke pale i nā haawe hana ma'amau akā nahā a nahā paha ma lalo o ka hopena hikiwawe.
ʻAʻole lawa ka elongation o 0.5% wale nō no nā ʻāpana i ʻike ʻia i nā pilikia hoʻokūkū nui.. Pono ka mea e hāʻawi i ka ductility kūpono e komo i ka ikehu hopena a pale aku i ka pōʻino pōʻino.
ʻAʻole hiki i nā mea hoʻoheheʻe make maʻamau ke hoʻokō i kēia mau koi.
Hoʻohana nui ʻia ʻo AlSi9Cu3 no nā ʻāpana die-cast alumini ma muli o kona castability maikaʻi a me ka ikaika, akā hiki i kāna elongation liʻiliʻi a me ka paʻakikī ke hoʻopaʻa i kona hoʻohana ʻana i nā ʻōnaehana robot koʻikoʻi.
Nā Manaʻo Alloy no ka Paʻa ʻana i ka hopena
| Alloy | Hooloihi maʻamau | Hopena paʻakikī | Kupono no na Hana Lopako |
| Ali nisri9pu3 | 1-3% | Loli | Ua kaupalena ʻia no nā ʻāpana koʻikoʻi hopena |
| A356-T6 | 5-10% | Maikaʻi loa | He kūpono i kahi e pono ai nā waiwai i mālama ʻia i ka wela |
| A360 | 3-5% | Maikaʻi loa | Hāʻawi i ka ductility maikaʻi ma mua o AlSi9Cu3 maʻamau |
| Am60 (Mg) | 6-12% | Maikaʻi loa | ʻO ka elongation maikaʻi, aka, oolea haahaa |
| AZ91 (Mg) | 3-5% | Loli | ʻO ka elongation haʻahaʻa ma mua o AM60 |
Nānā: ʻOkoʻa ka hoʻonui ʻana a me ka hana hopena me ka hui ʻana o ka alloy, Ke kahua nei, Potiwale, ʻO ka mālama wela, hōʻano hoʻohālike, a me nā kūlana hoʻāʻo.
ʻO nā waiwai ma luna nei he mau hoʻohālikelike hōʻike, ʻaʻole i hōʻoiaʻiʻo ʻia nā waiwai ʻāpana.
No nā noi koʻikoʻi hopena, ʻoi aku ka maikaʻi o nā alloys me ka elongation kiʻekiʻe a me ka paʻakikī.
ʻO ka hana wela, e like me T6 no nā alumini alumini kūpono, hiki ke hoʻomaikaʻi i ka hana mechanical.
Akā naʻe,, hoʻonui ia i ke kumukūʻai hana a hiki ke hoʻololi i ka hoʻoheheʻe ʻana i ka paia lahilahi, ka hoʻolilo ʻana i ka mana dimensional i mea koʻikoʻi.
Lākahi, ʻO ka hoʻoheheʻe ʻana o ka robot humanoid e koi i kahi hui pū ʻana o ka ikaika, kūkaha, kumaikalua, hopena kū'ē, a me ka pā.
Pono e hōʻike ʻia ke koho ʻana i nā mea waiwai i ka ʻike maoli ʻana o ka ʻāpana i nā ukana hoʻokūkū ma mua o ka hilinaʻi wale ʻana i nā kikoʻī make-casting maʻamau..
8. Nā Alloy Magnesium no Robotics: Loaʻa a me nā palena
MAKENESIM ALLOYS ʻOi aku ka maikaʻi inā ʻo ka pahuhopu nui e hoʻemi i ka nui o nā hale neʻe.
ʻOi aku ka haʻahaʻa ma mua o ka alumini, a hiki ke hoʻohana ʻia ko lākou mana vibration-damping kiʻekiʻe i nā mīkini robotic.
Eia nō naʻe, ʻAʻole ʻo ka magnesium kahi pani ʻakomi no ka alumini. ʻO kona modulus elastic haʻahaʻa, Pūnaewele kūleʻa, nā koi hoʻomalu-luna, a me nā manaʻo palekana machining pono e hoʻoponopono ʻia.
Nā Pōmaikaʻi Nui o nā Alloy Magnesium
Haʻahaʻa haʻahaʻa: Hiki i ka Magnesium ke hoʻemi i ka nuipaʻa o kahi mea ma kahi kokoke 30% hoʻohālikelike ʻia me ka hoʻolei alumini o ka leo like.
Hiki ke waiwai kēia no nā lima, lima lima, nā mea hoʻopaʻa lima, a me nā hale hoʻoneʻe ʻē aʻe.
ʻO ka haʻalulu haʻalulu maikaʻi: Hāʻawi ka magnesium alloys i ka hoʻoheheʻe haʻalulu maikaʻi ma mua o nā alumini alumini.
Hiki i kēia ke kōkua i ka hōʻemi ʻana i ka hoʻoili ʻana i ka haʻalulu i kekahi mau hui neʻe, ʻoiai e pili ana ka hopena hope i ka geometry, Nā Mīkini, a me ka damping pae ʻōnaehana.
Hiki ke hoolei i ka paia lahilahi: Hiki i nā mea hoʻoheheʻe make magnesium kūpono ke hana paʻakikī, nā ʻāpana pā lahilahi me nā iwi ʻaoʻao i hoʻohui ʻia, Nā Wawa, a me nā hiʻohiʻona kau ʻana.
Palapala maikai: Hiki ke hoʻohana maikaʻi ʻia nā alloys Magnesium. Akā naʻe,, nā ʻāpana mīkini, ʻohi chip, koho wai hooluu, a me nā kaʻina hana e pale ai i ke ahi e koi i nā mana kūikawā no ka mea hiki ke ʻā nā ʻāpana magnesium maikaʻi a me ka lepo.
Nā palena e noʻonoʻo ai nā ʻenekinia
'Āuhae haʻahaʻa: ʻOi aku ka haʻahaʻa o ka modulus elastic o Magnesium ma mua o ka alumini. Pono paha kekahi mea magnesium i nā paia mānoanoa a i ʻole ka hoʻoikaika hou ʻana e hoʻokō i ka palena deflection like.
Pale pale: Hiki ke maʻalahi nā mea hao magnesium i ka ʻino galvanic ke hoʻohui ʻia me nā metala like ʻole i mua o kahi electrolyte..
Nā mea paʻa, nā mea pili pili, Nā pāpale, a pono e noʻonoʻo pū ʻia ka hoʻolālā ʻana i ka wai.
Ke hoʻopauʻana: Pono ka Magnesium i ka mālama mua ʻana a me ka hoʻopau ʻana. ʻAʻole hiki ke hoʻololi pololei ʻia nā ʻōnaehana pale i hoʻohana ʻia no ka alumini i ka magnesium me ka ʻole o ke kaʻina hana.
Palekana mīkini: Pono ka mīkini hana magnesium i ka hoʻokele chip kūpono, mālama hale, nā hana pale ahi, a me nā kaʻina hana.
ʻOi aku ka pōʻino o ke ahi ma mua o ka waihona metala nui maʻamau.
Pono waiwai a me ka hana: Pono e noʻonoʻo ke koho ʻana i ke kaʻina hana hoʻoheheʻe ʻia, mānoanoa ʻāpana, Nā Pīkuhi Propertinies, ʻike ʻino, a me nā koi palekana pili.
I ka wā e pono ai ka Magnesium e noʻonoʻo
| Mea a noi | Loaʻa ka pōmaikaʻi o ka magnesium | Manaʻo manaʻo nui |
| Nā hale lima lima | Hoʻemi ʻia ka neʻe ʻana a me ka inertia | ʻOʻoʻoleʻa a me ke kū'ē i ka hopena |
| Nā uhi mea hana māmā | Ke kaumaha haʻahaʻa a me ka haʻalulu haʻalulu | Ka ikaika kau kau wahi |
| Hoʻopaʻa lopako | Hoemi hope-effector mass | Hoʻouka hou ʻia a ʻaʻahu ʻia ma nā interface |
| Ke neʻe nei i nā pā hui | Inertia hoʻololi haʻahaʻa | ʻO ka paʻakikī o ka noho ʻana a me ka luhi |
| Nā hale uila māmā | Hoʻemi nui a me ka hiki ke pale electromagnetic | ʻO ka mālama wela a me ka pale ʻino |
9. Aluminum Alloys no Robotics: Ikaika, Luhi, a me ka hana Versatility
Apana Apana Aluminum e hoʻomau i ka hana no ka hoʻoheheʻe robotic no ka mea hoʻohui lākou i ka haʻahaʻa haʻahaʻa me ka ʻoʻoleʻa kiʻekiʻe, maikaʻi maikaʻi thermal, a me kahi kaiaola hana makua.
Ua kūpono lākou no kahi ākea o nā mea hana a me nā mea hana, me nā hale hana actuator, hale hui, nā pā kaʻa, ʻāpana kumu, a me nā pua uila.
Nā Pōmaikaʻi Nui o nā Aluminum Alloys
ʻO ka modulus elastic kiʻekiʻe: Loaʻa i nā alumini alumini ka modulus elastic ma kahi o 69-72 GPa, i hoohalikeia me ka roughly 45 ʻO GPa no nā huila magnesium maʻamau.
He mea maikaʻi kēia i ka alumini ma kahi e koʻikoʻi ai ka mana deformation.
Maikaʻi maikaʻi thermal: Hāʻawi ka nui o nā alumini hoʻoheheʻe alumini i ka hoʻoili wela maikaʻi, mea waiwai no ka moto, pākaukau, a me nā hale uila.
Hoʻokumu ʻia ka ʻenehana make-casting: Hoʻohana nui ʻia ka hoʻoheheʻe kiʻekiʻe alumini no nā ʻāpana paʻakikī a kākoʻo i kahi ākea o ka nui o ka hana, nā mea hana hoʻonohonoho, a me nā hana lua.
Hiki ke hoʻopau i ka ʻili: Hiki i nā hoʻolei alumini ke komo i ka pauka, Kāleka, uhi hoʻololi, anodizing kahi i ʻae ʻia ai ka maikaʻi o ka alloy a me ka hoʻolei ʻana, a me nā hana hoʻopau ʻē aʻe.
ʻO nā koho machining makua a hui pū: Hiki ke hoʻohana ʻia nā ʻāpana alumini CNC e hoʻokō i nā noho lawe pololei, nā lua nui, nā papahele e ana ana, a me nā pilina hui.
Ka palena o na Aluminum Alloys
ʻOi aku ke kaumaha o ka alumini ma mua o ka magnesium, hiki ke hoʻonui i ka inertia o ka neʻe ʻana i nā ʻāpana robotic. He mea koʻikoʻi kēia no nā lima lōʻihi a me nā hopena hopena.
ʻO kekahi mau alumini die-cast kiʻekiʻe i hoʻoheheʻe ʻia he elongation palena ʻole, ʻoi aku ka nui o ka porosity, Nā kiʻi kiʻi, a i ʻole nā hemahema hoʻolei ʻē aʻe.
Pono e hōʻoia ʻia ko lākou kūpono no nā hale i hoʻouka ʻia ma o ka hoʻāʻo ʻana i nā mea a me ka hōʻoia ʻana o nā mea.
He ʻokoʻa nō hoʻi ka hoʻoili wela ma muli o ka alloy. ʻAʻole hiki i kahi alumini alumini i koho ʻia no ka ikaika a me ka hoʻoheheʻe ʻana i ka conductivity wela kiʻekiʻe loa.
Nā Koho Aluminum Aluminum maʻamau
Eia nā laʻana o nā alumini alumini i hoʻohana ʻia i nā noi make-casting. ʻO ko lākou kūpono no ka robotics e pili ana i ka mechanical o ka mea, thermal, a me nā koi hana.
| Alloy | Nā hiʻohiʻona maʻamau | Nā polokalamu robotics hiki |
| Ali nisri9pu3 | Maikaʻi maikaʻi, ikaika, a me ke kūpaʻa kiʻekiʻe; hoʻohana nui ʻia i ke kaomi ʻana i ka make | Nā mea hana hana, Nā Mālama Poole, nā pā hale |
| A380 | Maikaʻi maikaʻi, hiki ke paʻa paʻa, a me ka hana make-casting kumu nui | Nā hale paʻakikī, nā pā uila uila, nā hale hana mechanical |
| Adoc12 | Maikaʻi castability a me ka hana maʻamau i ka kiʻekiʻe-volo make make | Nā hale paʻa, uhiʻehā, a me nā mea i hoʻohuiʻia |
| AlSi10Mg | Hiki maikaʻi ka ikaika-i-kaumaha; hilinaʻi nui nā waiwai i ke ala hoʻolei a me ka mālama wela | Nā ʻāpana hoʻolālā i mea nui ka hana mechanical |
| AlSi12 | Kiʻekiʻe silika maʻiʻo a me ka maikaʻi castability, no nā geometries paʻakikī | ʻO nā hale pā lahilahi a me nā mea hoʻoheheʻe paʻakikī |
10. Ke koho ʻana i ke kaʻina hana hoʻolei kūpono: Kiekie-Pressure Die Casting vs Semi-Solid Casting
Pono e hoʻomohala pū ʻia ke koho ʻana i nā mea waiwai a me ke kaʻina hana hoʻolei.
Hiki i kahi huila kūpono ke hana i kahi mea kūpono ʻole inā ʻaʻole hiki i ke kaʻina hana ke hoʻokō mau i ka mānoanoa pā i makemake ʻia, Nā Pīkuhi Propertinies, dimensional pololei, a i ʻole ka maikaʻi o loko.
ʻO keʻano nui o ke koʻikoʻi
ʻO keʻano nui o ke koʻikoʻi (HPDC) ua kūpono i ka paʻakikī, nā hale robotic pā lahilahi a me nā mea e pono ai ka hana kiʻekiʻe.
ʻO kāna mau pono nui:
- Kiʻekiʻe kiʻekiʻe hana a me ka repeatability.
- Geometry paʻakikī a me nā hiʻohiʻona i hoʻohui ʻia.
- ʻO ka hoʻopau ʻili maikaʻi ke hoʻohālikelike ʻia me nā kaʻina hana hoʻoheheʻe maʻamau.
- Hiki i ka pā lahilahi me ka hoʻolālā kūpono a me ka hoʻolālā make.
- Hoʻemi ʻia ka mīkini a me ka hui ʻana ma o ka hoʻohui hana.
Akā naʻe,, Hiki i ka wikiwiki o ka injection ke hoʻokomo i ka hoʻopili kinoea a me nā hemahema pili i ka turbulence. Hiki i kēia mau hemahema ke kaupalena i ka hana mechanical a me nā koho mālama wela o kekahi mau mea.
No ka hoolei robotics, pono nā mea ʻenekinia e nānā pono i ka hoʻokele vacuum, hoʻolālā ʻīpuka a me ke kukini, kūhewaʻi, paʻa kūloko, a me kahi o nā ʻili mīkini koʻikoʻi.
Semi-Solid Die Casting: ʻO kahi koho no nā ʻāpana me nā mānoanoa pā like ʻole
Nā hana hoʻolei semi-solid, me ka rheocasting, e hoʻohana i ka slurry metala me ka hakina paʻa i hoʻomalu ʻia ma mua o ka metala wai piha.
Holo ka mea i loko o ka make ma lalo o ke kaomi ʻoiai e mālama ana i kahi microstructure semi-solid.
Hiki ke nani kēia kaʻina hana no nā ʻāpana robotic me nā ʻāpana lahilahi a me ka mānoanoa, ʻoi aku ka maikaʻi o ka hoʻopiha piha ʻana a me ka hoʻohaʻahaʻa ʻana i ka haunaele.
Loaʻa nā pono kūpono:
- ʻOi aku ka mālama ʻana i ke kahe metala.
- Hoʻemi ʻia ka haunaele a me ka hoʻopaʻa kinoea ma lalo o nā kūlana kūpono.
- Hiki ke hoʻonui ʻia no ka hana ʻana i nā ʻāpana me nā mānoanoa pā like ʻole.
- Loaʻa nā manawa kūpono e loaʻa ai ka maikaʻi o loko a me ke kūlike mechanical.
- Hoʻohālikelike me nā geometries paʻakikī e koi ana i nā paia lahilahi a me nā ʻāpana hoʻoikaika kūloko.
No ka hale lima robot, ʻo kahi laʻana, hiki ke hoʻolālā ʻia ka pūpū nui me nā paia lahilahi e hōʻemi i ka nuipaʻa, ʻoiai ʻo ka mea hoʻokomo i nā kiko a me nā kākoʻo e koi ana i nā ʻāpana mānoanoa.
Hiki i ka hoʻolei ʻana semi-solid ke hāʻawi i kahi ala kaʻina hana pono no kēia hui ʻana.
Akā naʻe,, ʻAʻole kūpono ka hoʻolei semi-solid no kēlā me kēia ʻāpana.
Hoʻomākaukau slurry, hakina paʻa, Ka Hoʻopumia a ka Ola, ka hoopiha ana, a me ke kaʻina hana hou e pono ai ka mana kokoke. Pono e loiloi ʻia kona pono waiwai e kūʻē i ka mea hana, Nā Pono Hana, manawa manawa, a me ka hana hana.
11. Hoʻopau i ka ʻili a me ke ʻano
ʻAʻole like me nā mea hoʻolei automotive he nui, i hūnā ʻia i loko o ka hale kaʻa, ʻike ʻia ma waho ka helu nui o nā hoʻoheheʻe robot humanoid.
ʻAʻole pili ka maikaʻi o ko lākou ʻili i ka pale corrosion akā ʻo ka hiʻohiʻona holoʻokoʻa a me ka maikaʻi i ʻike ʻia o ka robot i hoʻopau ʻia..
Pono nā mea hoʻolako die-casting e nānā pono i ka maikaʻi as-cast, ʻoihana hoʻomākaukau, a me ka hoʻopau ʻana i ke kūlike.
Nā hemahema ʻike ʻia e like me nā kaha kahe, nā'ōpū anuanu, porosity ili, a hiki i nā ʻano like ʻole ke ʻae ʻole i ka ʻāpana ʻoiai ke hoʻokō ʻo ia i kāna mau koi mechanical.
Ma muli o ka hoʻolālā, pana pua, anodichiz, ʻO ka paleʻana, a i ʻole ka polishing e pono ai e hoʻokō i ka helehelena i makemake ʻia.
Akā naʻe,, ʻokoʻa nā koi corrosion no ka nui o nā robots i loko o nā ʻāpana kaʻa i ʻike ʻia i ka paʻakai alanui, kaiwa, a me ka hoʻololi ʻana i nā kūlana o waho.
Nā lopako e hana ana ma nā hale hana, Waremouse, a hiki i nā hale ke kau i ka manaʻo nui i ka helehelena, maʻemaʻe ʻili, a ʻaʻahu i ke kūpaʻa ma mua o ka hana paʻakai paʻakai.
Pono nā koi palekana maoli e hōʻike i ke kaiapuni hana o ka robot.
Nā koho hoʻopau ʻili no ka hoʻolei ʻana i ka robot
- ʻIli hoʻolei ʻia: Pono ka maikaʻi kūlike, me nā kaha kahe ʻole ʻae ʻia, nā'ōpū anuanu, a i ʻole porosity ʻike ʻia ma nā wahi koʻikoʻi.
- Pana pua: Hoʻokumu i kahi ʻano matte like ʻole a hoʻoneʻe i nā mea haumia o ka ʻili a me nā koena.
- Anodichiz: Hāʻawi i nā mea hoʻolei alumini me kahi papa oxide lōʻihi a, e pili ana i ka huila a me ka hana, he laulā o nā koho kala. Pono ka Magnesium i nā kaʻina hana lapaʻau kūikawā.
- ʻO ka paleʻana: Hāʻawi i kahi koho ākea o nā kala, Nā uhi uhi uhi, a me ka lōʻihi o ka ʻili maikaʻi.
- Kāleka: Hoʻomaikaʻi i ka maʻalahi a me ka maikaʻi ʻike no nā mea i hōʻike ʻia me nā koi hiʻohiʻona premium.
Pono pū ka hoʻolālā pili. ʻAʻole like me nā hale kaʻa kaʻa e hoʻohana i ka hoʻopaʻa paʻa paʻa, ʻO nā hui robot humanoid e hilinaʻi maʻamau i nā bolts, Aia, a me nā pilina mekini.
Nā hiʻohiʻona hoʻolei e like me nā flanges, Nā Wawa, a no laila, pono e hā'awi nā ili male i nā wahi kūpono, hoʻopili pili, a me ka pololei ana e hōʻoia i ka hui pono.
Lākahi, pono e noʻonoʻo ʻia ka hoʻopau ʻana i ka ʻili a me ka hoʻolālā pili i ka wā o ka hoʻolālā hoʻoheheʻe ʻana, ma mua o ka mālama ʻia ʻana ma ke ʻano he hana lua ma hope o ka hana ʻana.
12. No ke aha e hoʻomaka ai ka hoʻonā hoʻoheheʻe robotics maikaʻi me ka subsystem
ʻO ka hoʻomohala ʻana o nā robots humanoid e hana nei i kahi manawa hou no nā mea hana hoʻoheheʻe make, akā, hoʻololi i ka pono o nā mea hoʻolako e hoʻokokoke i ka hoʻomohala ʻana.
Hoʻomaka pinepine nā papahana hoʻolei kuʻuna me ke kaha kiʻi, he ʻōlelo hoʻohālikelike, a me ke kumu kuai. Pono nā papahana Robotics i kahi kūkākūkā ʻenehana ākea.
Pono ka mea hoʻolako hoʻolei e hoʻomaopopo i kahi i hoʻokomo ʻia ai ka ʻāpana, he aha ka haawe ana, pehea e neʻe ai, pehea e hoʻopili ai i nā mea ʻē aʻe, a inā pono e hoʻoneʻe i ka wela a i ʻole e pale i nā hopena ulia.
ʻo kahi laʻana, Hiki i ka hale lima mua ke hana mua i ka nui haʻahaʻa a me ka hoʻemi ʻana i ka inertia rotational. Pono paha ka ʻoi aku o ka ʻoʻoleʻa i ka hale hui kuli, ʻO ka paleʻana o ka momona, a me ka hoʻomanawanui hopena.
Pono paha ka pā kaʻa i ka hoʻoili wela kūpono, ʻoiai ʻoi aku ka pōmaikaʻi o kahi ʻāpana kino haʻahaʻa ma muli o ka rigidity a me ka hoʻohele nui ʻana.
No laila, pono e hā'awi ka mea hana ho'ohehe'e make ma mua o ka hao ma'amau a me ka hua'ōlelo hana.
Pono e noʻonoʻo ka hoʻonā hana:
- ʻO ke koho ʻana i nā mea ma muli o nā kūlana hana maoli o ka mea.
- Hoʻolālā hoʻolālā hale no ka ʻoʻoleʻa, ikaika, a he kaumaha.
- Alloy a me ka hoʻolei ʻana-ka hana hoʻohālikelike.
- Hoʻolālā make, Hoʻopihaʻana, Kūpuia, a me ka pale ʻana i nā hemahema.
- ʻO ka mīkini CNC o nā pilina pololei.
- ʻO ka hoʻopau ʻana i ka ʻili a me ka pale ʻana i ka corrosion.
- Huahuai, puiahuhu, a me ka nānā pono kūloko.
A ʻO kēia, hiki ke hoʻokokoke i ka hoʻomohala ʻana i nā mea hoʻolei maʻamau ma ke ʻano he kaʻina hana hoʻohui e pili ana i ka hiki ke hoʻolei, loiloi waiwai, mea hoʻolālā, Cnc iching, a hoʻopau.
ʻO ka pahuhopu ke kōkua i nā mea kūʻai aku e hoʻohuli i nā hoʻolālā ʻāpana robotic paʻakikī i nā ʻāpana hana me ka maikaʻi kūlike.
13. Hopena
ʻAʻole hoʻokahi mākeke hoʻokahi me nā koi hoʻokahi. He hōʻiliʻili ia o nā subsystem me nā pono like ʻole-i kekahi manawa.
Pono ka lima e māmā e like me ka hiki; hiki i ke kumu ke pōmaikaʻi mai ka nuipa hou; pono ka hale hui e hoopau i ka wela; pono e nana pono ka panel ike; pono ka lopako hāʻule i ka paʻakikī, aole ikaika wale.
Loaʻa ka alumini a me ka magnesium i kēia ʻāina, akā, ʻaʻole hoʻi he hopena honua. Hāʻawi ka alumini i ka ʻoʻoleʻa maikaʻi, Ka HōʻaʻO Kokua, a hoʻopauʻia.
Hāʻawi ka Magnesium i ka haʻahaʻa haʻahaʻa a ʻoi aku ka maikaʻi o ka damping, aka, ma ke kumukuai o ka oolea, Holo Maʻaleʻa, a me ka hana paʻakikī.
He ākea ka wahi hoʻolālā no nā hoʻolei robot. Pono nā lopako i ka māmā, kiʻekiʻe rigidity, paʻakikī ka paʻakikī, hoopau wela, dimensional pololei, a me ka maikaʻi o ka helehelena—akā ʻaʻole pono kēlā me kēia ʻāpana i kēia mau mea i ka manawa hoʻokahi.
ʻO ka manawa kūpono e hoʻomohala i nā hāʻina hoʻolei i kūpono i kēlā me kēia hana. He luʻi hoihoi loa ia ma mua o ka hoʻokūkū ma ke kumu kūʻai no ka kilo.
FaqS
Ua ʻoi aku ka maikaʻi o ka magnesium ma mua o ka alumini no nā hoʻoheheʻe robot humanoid?
ʻAʻole i kēlā me kēia noi. He haʻahaʻa haʻahaʻa haʻahaʻa ka Magnesium a ʻoi aku ka maikaʻi o ka haʻalulu haʻalulu, hoʻonanea i nā mea hoʻoneʻe.
Hāʻawi ka alumini i ka ʻoʻoleʻa kiʻekiʻe ma ka geometry like a ʻoi aku ka maikaʻi o ka conductivity thermal.
ʻO ke koho e pili ana i ka ukana o ka mea, palena deformation, pono wela, a me ka hana ana i nā mea'āpono.
No ke aha he mea nui ka ʻoʻoleʻa no ka hoʻolei ʻana i ka robot humanoid?
Mālama ka ʻoʻoleʻa i ka nui o ka hoʻololi ʻana o kahi mea ma lalo o ka ukana. Hiki i ka deformation nui ke hoʻopili i ka alignment bearing, ka hoʻopili ʻana i nā mea hana, hoʻonohonoho hoʻonohonoho, a me ka pololei o ka neʻe ʻana.
No nā hale robotic pololei, ʻO ka hoʻomalu ʻana i ka deflection hiki ke lilo i mea nui e like me ka loaʻa ʻana o ka ikaika tensile lawa.
No ke aha i hoʻohana pinepine ʻia ai ka alumini no nā hale kaʻa robot?
Hoʻohui ka alumini i ka haʻahaʻa haʻahaʻa me ka ʻoi aku o ka ʻoʻoleʻa ma mua o ka magnesium a me ka conductivity thermal maikaʻi maʻamau.
Kūpono kēia mau waiwai i nā hale kaʻa a me nā mea hoʻokele e pono e kākoʻo i nā ukana mechanical ʻoiai e kōkua ana i ka hoʻoneʻe ʻana i ka wela mai nā ʻāpana kūloko..
He kūpono paha ʻo AlSi9Cu3 no ka hoʻolei ʻana i ka lopako humanoid?
ʻO AlSi9Cu3 kahi alumini i hoʻohana nui ʻia me ka hoʻoheheʻe kiʻekiʻe kiʻekiʻe me ka castability maikaʻi a me nā waiwai mechanical pono..
Akā naʻe,, ʻo kona kūpono e pili ana i ka ʻoʻoleʻa i koi ʻia, ewangantion, hana hopena, maikaʻi kūloko, a me nā kūlana hana.
ʻAʻole pono e mālama ʻia ma ke ʻano he hopena honua no kēlā me kēia hale robotic.