ʻO nā mea hānai e hānai i nā hemahema

Nā mea hana e make ai i nā hemahema a pehea e pale ai iā lākou

1. Hōʻikeʻike

ʻO ka mea e make ana he hana hana kūpono a maikaʻi loa e hana i nā hana paʻakikī paʻakikī e hana i nā'āpana metala paʻakikī.

Hoʻohana nuiʻia ma nāʻoihana e like me ka automotive, AerERPPACE, nā leka uila, a me nā huahana waiwai,

ʻO nā mea make e hānai ana i nā makana e like me nā uku hana kiʻekiʻe, ʻO ka pololeiʻokoʻaʻokoʻa, a me ka pauʻana o ka pālima.

Akā naʻe,, ʻOiai ma kahi kaʻina e like me ka mea e like me ka makeʻana, ʻAʻole kūpono nā hemahema.

Hiki i kēia mau hemahema ke hōʻole i ka maikaʻi o nā'āpana, ke alakaʻiʻana i nā hōʻai'ē kālā a me nā mea kūʻai aku o ka mea kūʻai aku.

ʻO ka hoʻomaopopoʻana i nā hemahema o nā mea make, ko lākou kumu, a he mea nui nā kumukūʻai pale e mālama i nā kūlana hoʻolālā kiʻekiʻe.

Ma kēiaʻatikala, Eʻimi mākou i nā hemahema o ka make, Pehea lākou e hōʻike ai i ka hana, a me nā ala kūpono e pale ai iā lākou.

2. He aha ka mea e make ai?

ʻO ka mea makeʻo Die Creing he kaʻina hana kahi i hoʻohālikelikeʻia ai ka metala molten i loko o kahi mū ma lalo o ke kaomi kiʻekiʻe. A laila,ʻaeʻia ka mea hao a hoʻopaʻaʻia i loko o kahiʻano kūpono.

ʻO ka maʻamau maʻamau no ka hanaʻana i nā'āpana me nā geometries intricate e koi ai i ka pololei kiʻekiʻe.

Make-tästing
Make-tästing

Loaʻa nā pono nui:

  • 'Clelo pololei: Make ka mea e hana ai i nā mea hana i hiki ke loaʻa i nā mea paʻa e like me ka mea e like me ± 0.1 mm, Ke kūpono nei i nā'āpana no nā mea e koi ai i nā kiko'ī kiko'ī.
  • Kumukūʻai-kūpono: Hanaʻia nā lulu, He maikaʻi loa ke kaʻina hana a me ke kumukūʻai, ʻO ka nui o nā hana hana kiʻekiʻe.
  • Uku uku uku: Hiki i ka poʻe make ke hana i nā kaukani o nā'āpana likeʻole i kahi manawa pōkole, e lilo ia i mea kaulana no ka hana nui.

Hoʻohanaʻia nā metals maʻamau:

  • Aluminum: Nā helu no ka kokoke 85% o nā huahana make-make, kaulana no kona mau kukui māmā a me ka corrosior, Hoʻohana pinepineʻia i loko o kaʻoihana automotive a me Aerospace.
  • Zinc: Hāʻawi i ka ikaika kiʻekiʻe, ʻO ke kāwele nuiʻana, a me ke kū'ēʻana. Hoʻohana pinepineʻia no ka liʻiliʻi, nā'āpana likeʻole.
  • Magnesum: ʻO keʻano metala māmā, hāʻawi i kahi kiʻekiʻe kiʻekiʻe-kiʻekiʻe, hoʻohana pinepineʻia ma Aerospace a me nā noi Automotive.
  • Nā pāpale keleawe: Kaulana no ka ikaika kiʻekiʻe a me keʻano uila, Hoʻohanaʻia nā mea kūʻai aku no nā'āpana uila.

3. ʻO nā mea hana maʻamau

Hiki i nā mea make-make ke hopena i ka hopena o ka maikaʻi, hana, a me nā mea hoʻopiʻi Aesthetic.

Ua hāʻule kēia mau hopena i nā'āpanaʻehā: 'Ōlao'ōmaʻomaʻo, hewa kūloko, nā hemahema, a me nā hemahema e pili ana i nā mea.

A. 'Ōlao'ōmaʻomaʻo

DEAD-CASTING DECTTS DECTTS DIG TRAGS
DEAD-CASTING DECTTS DECTTS DIG TRAGS
  • Pū uilani
    E hele mai ka Flash i ka wā e pakele ai ka nui o nā mea hao mai ka'ōpū, maʻamau ma muli o ka lawaʻole o ka hoʻoikaikaʻana i ka paʻakikī a iʻole he mismatch i nā'āpana mold.
    Hopena i ka lahilahi, unwantd itad fins a puni ka pā, i mea e hoʻokaʻawaleʻia ai.
  • Ua anuanu
    ʻO kahi pani anuanuʻo ia ka hopena o ka moltental i keʻano o ka molten i hikiʻole ke hoʻopili piha i ka wā o ke kaʻina hana ma muli o ka nui o ka wela.
    ʻIkeʻia he seam a iʻole ka laina ma luna o ka papa o ka mea lawe a hiki ke loaʻa i ka'āpana.
  • Kuni i nā māka
    Burn Marks he mau pōkoleʻeleʻele a iʻole ka carbon e kūkulu ana i luna o ka pā hale.
    ʻO kēia ka mea maʻamau i ka laweʻana i ka mea hao a iʻole ka hōʻike nui loa i ka wela i ka wā o ka make.
  • Aniani wai
    Nā hualoaʻa o nā pohomisty i nā lua liʻiliʻi a iʻole nā ​​leo i hōʻikeʻia ma kaʻaoʻao o ka hale kūʻai.
    ʻO kēia hewa pinepineʻia e ka lewa a iʻole ke kīʻana i ka hau ma keʻano molten i ke kaʻina hana.

Na B. Hewa kūloko

'Āʻia wela
'Āʻia wela
  • Loko
    ʻO ka lāʻau lapaʻau kūloko e pili ana i nā pihi Air i hoʻopaʻaʻia i loko o ka hale kūʻai, Ke hana nei i ka mea nāwaliwali a me ka hikiʻole ke loli i ka hikiʻole ke hoʻopau i ke kaumaha.
    Ke hele pinepine nei kēia mau leo ​​i ka wā e hoʻopiliʻia ai ka mīkini i ka wā o ke kaʻina hana.
  • Shrinkage
    Nā hemahema o ka shrink i ka wā e pau ai nā mea kūʻai aku a me nā kuʻikahi, Ke hana nei i nā hana i loko o ka'āpana.
    ʻO kēia ka mea maʻamau i hanaʻia e nā mea maikaʻiʻole a iʻole ke kūʻaiʻana i nā lako metala molten.
  • 'Āʻia wela
    E ulu ana ka wela wela i ka wā e kau ana i nā pōpoki, pinepine i nā'āpana'āpana i nā'āpana i kahi o ke kaumaha i ka wā e pau ai ka hoʻololiʻana i ka hiki ke pale.

C. Nā hemahema

  • Kauoha
    Ke hele neiʻo SoulPage i ka wā o nā'āpana e koi ai ma muli o keʻano o nāʻano kaulikeʻole a iʻole ke kaumaha kūloko.
    ʻO kēia mau mea maʻamau i nā'āpana nui a iʻole nā'āpana paʻakikī kahi e hele ai nā kumukūʻai e like me nā'āpana likeʻole.
  • Morliengente
    ʻO ka Misnalignment e kū pono ana i ka wā e hoʻokaʻawale ponoʻia, e pili ana i nā hewa ma ka'āpana geometry.
    Hiki i kēia ke kumu i hanaʻia e nā hoʻolālā maikaʻiʻole a iʻole kūponoʻole i ka hoʻopiliʻana i ka wā injection.
  • ʻO nā'āpana kūponoʻole
    Nā kūlana kūponoʻole, e like me keʻano kūponoʻole a iʻole ka wela, hiki ke hopena i nā'āpanaʻaʻole e hoʻokō i nā kiko'ī hoʻolālā.

D. Nā mea e make ai nā mea i nā hemahema

ʻO nā hewa pili-pili i piliʻia e nā hewa, paio, a iʻole nā ​​mea hana kūponoʻole.

Hiki i kēia mau hemahema ke hopena i nā hemahema, Potiwale, a he hapaʻole paha.

4. Nā kumu o ka makeʻana o nā mea kūʻai aku

Hiki i nā hana Die-Casting Defens ke kū mai nā mea likeʻole i ka wā o ke kaʻina hana.

ʻO ka hoʻomaopopoʻana i kēia mau kumu ke koʻikoʻi no kaʻikeʻana i ke kumu o ka pilikia a me ka laweʻana i nā hana hoʻoponopono.

Ma lalo o nā kumu nui o nā mea make-make:

Nā pilikia pili pili

  • Palau: Nā mea haumia a iʻole nā ​​mea haumia i loko o ka metala, e like me nā merites a iʻole ka lepo, hiki ke hoʻokaʻawale i keʻano o ka mālamaʻana.
    Hiki i nā mea waiwai ke hopena i nā hemahema e like me ka poosity a iʻole nā'ūhā anu.
  • ʻIkeʻia kaʻike: ʻO ka nui o ka mistiture i loko o ka metala a iʻole mold ke kumu i ka steam e hana i ke kaʻina hana injection.
    Hiki i kēia ke alakaʻi i nā bubbles, nā pahu hau, a me nā hemahema e like me ka poosity a iʻole ka pākuʻiʻana.
  • NA KAKU ANA LOA: Ināʻaʻole i kāwiliʻia ka metala metal, Hiki iā ia ke hana i ka shrink a iʻole ka politika kūloko.

Kāohi i ke ana: Ke hoʻohana nei i ka maikaʻi kiʻekiʻe, hoomae, a me nā mea i hoʻomākaukauʻia, a hōʻoiaʻiʻo e hoʻomākaukauʻia ka mea metal a ua hana pololei i hiki ke hoʻoikaika i kēia mau pilikia.

Ka hoʻolālāʻana a me ke kūlana

  • Indeducquate: Pono kūpono ke kiʻi kūpono eʻae i ka lewa i pakele i ka pakele i ka wā o ke kaʻina hana injection.
    ʻAʻole hiki ke hoʻokaʻawale i keʻano o ke komoʻana i ke kino, e hana ana i nā hemahema e like me ka poosity a iʻole nā ​​hōʻailona.
  • ʻO ka lole a me ka waimaka: Ua holo ʻoi aʻe ka manawa, Hiki i nā Molds ke kau i waho aʻeha paha i nā hewa, e alakaʻi ana i nā hemahema e like me nā liʻiliʻi o ka uila a iʻole nā'āpana.
  • ʻAʻole kūpono i nā'ōnaehana hana: Inā hoʻokomoʻia ka'ōnaehana o ka mold a ke kālaiʻia a kauʻia paha,
    Hiki iā ia ke kumu i ke kahe waiʻole, e alakaʻi ana i nā hemahema e like me nā shuts anuanu, morliengente, a iʻole ka hoʻopiha pihaʻana.

Kāohi i ke ana: Ka mālama maʻamau o nā molds, ʻO nā'ōnaehana'ōnaehana, a me ka mālama ponoʻana i nā'ōnaehana geting a me nā'ōnaehana e hiki ke pale i kēia mau pilikia.

Kaʻina hana

  • Ka Hoʻopumia a ka Ola: Ka mālamaʻana i kahi mahana kūlike no ka metalaʻelua a me ka'ōpū he mea nui.
    Inā wela loa ka metala a wela paha, Hiki iā ia ke alakaʻi i nā hemahema e like me nā hōʻailona wela, nā'ōpū anuanu, a i ole.
    Like me, Hiki i keʻano o ka maffistlast moll i keʻano o ka hoʻomaʻamaʻaʻana a iʻole nā ​​mea i hanaʻoleʻia.
  • ʻO ka wikiwiki a me ke kaomi: ʻAʻole lawa i ka wikiwiki o ka wikiwiki a iʻole ka hopena e hopena i ka hoʻopiha pihaʻana, e alakaʻi ana i nā shuts anuanu a iʻole nā ​​hale kūʻaiʻole.
    Like, Hiki i ke kaomi nui ke kumu i nā flash a me nā mea waiwai.
  • ʻO nā uku hoʻomehana: ʻO nā kumukūʻai maikaʻi loa i wikiwiki a lohi paha i ka lohi, Kauoha, a iʻole ka wela wela. Hiki i keʻano maʻalahi ke alakaʻi i nā kaumaha o loko a me nā makemake.

Kāohi i ke ana: Ke nānā pinepine nei a hoʻoponopono i ka mahana, Ka paipai, a me ka maikaʻiʻana i nā kumukūʻai e hōʻoia i ka maikaʻi o ka hana.

Mīkini a me nā mea hana

  • Make make: Ua holo ʻoi aʻe ka manawa, ʻO nā make i hoʻohanaʻia no ka makeʻana e lilo ai i nā mea kūʻai aku, e alakaʻi ana i nā hemahema e like me nā uila a iʻole nā ​​intaccuracies ma nā'āpana'āpana.
    Ua hanaʻo Fan i ka hanaʻana i keʻano o keʻano kūʻokoʻa, e hopena paha i nā hemahema.
  • Nā Mahele mīkini: Hiki i nā mīkini hoʻoheheʻe make hewa a i ʻole calibrated kūpono ʻole ke kōkua i ka paʻi like ʻole,
    keka ao, a me ka wikiwiki i ke kaʻina hana injection, alakai i na hemahema.
  • Pono ʻole nā ​​hoʻonohonoho Mīkini: Ke hoʻohana ʻana i nā hoʻonohonoho hewa no ka mīkini hoʻoheheʻe make, e like me ka wikiwiki ʻole o ka injection a i ʻole ke kaomi,
    hiki ke hana i nā pilikia e like me ka pani anu, ʻilihune hoʻopiha, a i ʻole ka uila nui.

Kāohi i ke ana: E hōʻoia i ka calibrated mau nā mīkini, pani ʻia a mālama ʻia paha nā make, a me ka hoʻonohonoho ʻana i nā mīkini hiki ke pale i kēia mau ʻano hemahema.

Hana hewa

  • Ka lawelawe pono ole: ʻO nā mea hana i hoʻomaʻamaʻa ʻole ʻia a ʻaʻole i hahai i nā kaʻina hana kūpono hiki ke hana hewa e alakaʻi i nā hemahema.,
    e like me ka hoʻouka ʻana i ka poʻi kūpono ʻole a i ʻole ka wela metala like ʻole.
  • Nānā kūpono ʻole: Inā ʻaʻole ʻike nā mea hoʻohana i nā hōʻailona mua o nā hemahema a i ʻole hahai ʻole i nā kaʻina hana hoʻomalu maikaʻi,
    Hiki i nā hemahema ke hele iʻikeʻoleʻia, e alakaʻi ana i nā pilikia nui ma hope o ka hanaʻana.
  • Nele o ka hana hoʻoponopono: I kekahi mau hihia, ʻAʻole hiki ke hoʻololiʻia nā mea hana e hoʻoponopono i nāʻano kaʻina hana i ka wā e hoʻomaka ai nā hemahema, ʻaeʻia i nā pilikia i ka leʻaleʻa.

Kāohi i ke ana: Hoʻomaʻamaʻa kūpono a me ka hōʻoiaʻana i nā mea hana, me nā kaʻina hana loiloi, he mea koʻikoʻi no ka paleʻana i nā hala a me ka mālamaʻana i ka mana maikaʻi.

Nā meaʻikeʻole

  • ʻO ka haʻahaʻa a me keʻano like: ʻO nāʻano likeʻole i ka haʻahaʻa a me ke aniani e pili ana i ka kaheʻana o keʻano o ka mea hao,
    e alakaʻi ana i nā hopena kūponoʻole a me nā hemahema e like me ka pososity a iʻole keʻano.
  • Maʻemaʻe: Lepo, lepo, a iʻole nā ​​mea'ē aʻe i loko o kaʻoihana hana hiki ke hoʻohālikelike i nā mea hao a iʻole nā ​​mold,
    ke alakaʻiʻana i nā hemahema e like me ka nui o ka pā a iʻole ka hoʻopauʻana.

Kāohi i ke ana: Mālama i kahi mana, ʻO ka hoʻomaʻemaʻe hoʻomaʻemaʻe me ka mahana kūlike a hiki i nā kūlana haʻahaʻa ke kōkua i ke kōkuaʻana i kēia mau pilikia.

5. Nā hoʻonā maʻamau no ka poʻe e make i nā hemahema

ʻO ka heluʻana i nā hana make make-e nānā i kahi ala i kohoʻia e pili ana i keʻano o nā kumu o kēlā me kēia pilikia.

Iiiai, Mālama mākou i nā hoʻonā kūikawā no nā hemahema maʻamau, Kākoʻoʻia e kaʻikepili a me nā meaʻike pono e kōkua i nā mea hana e hoʻomaikaʻi i kā lākou kaʻina hana.

ʻO nā mea make e hānai ana i nā hemahema
ʻO nā mea make e hānai ana i nā hemahema

Pū uilani

Hopena: Hoʻoponopono i ka makeʻana i ka pohōʻana, ʻO ka hoʻomaikaʻiʻana i ka hoʻolālā Mod, a hōʻoiaʻiʻo e hōʻoia i nā hana kūpono kūpono e hōʻemi ai i nā flashgies e hōʻemi i ka flash.

  • Make slamping spemping: Ka hoʻonuiʻana i ka ikaika o ka clamping e hiki ke hōʻemi i ka hopena o ka flash e a i 25%.
    Ke hōʻoiaʻiʻo nei e paʻa paʻa ana nā pale mold.
  • HoʻolālāʻOi loa: Ka hoʻopiliʻana i nā mea kanu lāʻau i ka hoʻolālāʻana i ka hoʻolālāʻana e hiki ke hōʻemi i ka flash e like me ka nui 40%.
    Hoʻopili kēia i ka hana pololei a me nā loiloi mālama maʻamau e hōʻoia ai no ka hikiʻoleʻana i nāʻano o nā'āpana ma waena o nā'āpana mold.
  • Kūhewaʻi: Loaʻa i ka hana kūpono e hoʻopau i ka ea e pakele ai mai ka chevity a me kaʻaeʻana i nā mea hao molve e hahai ai.
    Hiki i ka hoʻonohonoho kūpono kūpono ke hōʻoki i ka hana uila e pili ana i 30%.

Ua anuanu

Hopena: Ka hoʻonuiʻana i ka mahana kila a iʻole hoʻoponopono i ka wikiwiki o ka wikiwiki e hōʻoia i ka hoʻopiha piha piha piha a me ka hoʻopili kūponoʻana o nā kahawai hao.

  • Oihana kila: E hāpai i keʻano o ka mahana o ka metala molten ma 10-20 ° C hiki ke hoʻoikaika i ka wai a pale i nā pilikia.
    Hiki i nā kiʻekiʻe kiʻekiʻe ke hoʻonui i ka hopena o ke kūleʻa kūleʻa e hiki mai ana 35%.
  • Ka wikiwiki: Hiki ke hoʻomaikaʻi i ka wikiwiki i ka wikiwiki e hoʻomaikaʻi i ke kaʻina hoʻopiha, e alakaʻi ana i kahi hōʻemi ma keʻano o ke anuanu ma kahi o ka a puni 40%.
    Hiki i nā wikiwiki ke kōkua i nā wikiwiki i hiki ke kōkua e hōʻoia e hoʻopiha i nā'āpana āpau i mua o ka hoʻomakaʻana o ka metala.

Kuni i nā māka

Hopena: Ka hoʻemiʻana i ka mahana molld a me ka hoʻomaikaʻiʻana i keʻano o ka curle cycle hiki ke pale aku i ka paleʻana a me nā hōʻailona ma hope o nā hōʻailona.

  • Kaohiʻana o ka mahana wela: Ka hoʻohaʻahaʻaʻana i ka mahana o ka mū ma ka 10-15 ° C hiki ke hōʻemi nui i ka hopena o nā hōʻailona puhi.
    Hiki ke kāohi i ka holoiʻana i ka pīhoihoi a me nā hemahema o nā wahi.
  • ʻO ke kāheaʻana i ka cycle optimization: Ke kauʻana i ke kaheʻana o ka mea kūʻai aku e pale i ka hoʻolahaʻana i ka wela e hiki ke wela ke hoʻopau i nā hōʻailona e nā 20%.
    E hōʻoia i ka hoʻokele kālā e pono ai i ka'āpana maʻamau.

Potiwale (Ahaolelo a me ka loko)

Hopena: Ke kāohi nei i ka helu hoʻoliʻiliʻi a me ka noiʻana i nā hana deginanging i hiki ke hoʻoikaika i nā pilikia poosity.

  • ʻO ka hoʻokele waiwai: Hiki ke hoʻokōʻana i nā kumukūʻai i mālamaʻia e hōʻemi i ka poosity kūloko e ka 30%.
    Kōkuaʻo ka mālie wikiwiki e kōkua i nā mea i hōʻoleʻia i nā kīwī, hopena i nā hale kūʻai denser.
  • ʻO nāʻenehana hana: Ke hoʻohana nei i nā ala e like me nā mea i kōkuaʻia e kōkuaʻia a hoʻohuiʻia paha i nāʻoihana a me ka hoʻonuiʻana i nā mea hoʻokele e hiki ai ke hoʻopau i 90% nā hewa pili i nā poster.
    Ua hoʻolaha kēia mau hana i ka weheʻana o nā kīwī i hoʻokaʻawaleʻia mai ka mea molte ma mua o ka hoʻoponoponoʻana.

ʻO ka wela a me ka wela wela

Hopena: Ke hoʻohālikelike nei i nā kumukūʻai hoʻomehana a me ka hoʻohuiʻana i nā alaloa e hiki ke kamaʻilio i nā chevinis shniknisity a me nā wela wela wela.

  • ʻO ka nānāʻana i ka hōʻoiaʻana: Keʻano maikaʻi i ke kaʻina hana e hōʻoia ai e hiki ke hōʻemi i keʻano o ka lole e hiki ai ke hōʻemi i nā hemahema shfink e 20%.
    Hoʻololiʻo Uniform i nā leʻaleʻa koʻikoʻi i keʻano o ke kaumaha e alakaʻi ai i ka wela wela.
  • Nā malihini a me nā mea hānai: Hiki i ka hoʻonohonohoʻana o nā mea hōʻike e hāʻawi i nā mea kilokilo hou e hāʻawi i nā mea molten e ukuʻia no kaʻohiʻana, e hōʻemi ana i nā uku detect e a hiki i 35%.
    ʻO nā'ōnaehana kūpono kūpono e hōʻoia ai e noho mau nā wahi koʻikoʻi mai nā lanakila i ka wā e hoʻoponopono ai.

Kauoha

Hopena: Ke hoʻokele nei i nā kumukūʻai maloʻo a me ka ho'ēmiʻana i nā pilikia kūloko i hiki ke pale i ka hanaʻana.

  • ʻO ka holoiʻana i ka hoʻomaʻemaʻe: Ka hanaʻana i nā channels e hoʻolōʻihi ana i ka hōʻoluʻolu e hiki ke hōʻemi i ka hoʻoponoponoʻana e 25%.
    ʻO nā mea hoʻonaninani haʻahaʻa liʻiliʻi e hōʻemi ana i nāʻano likeʻole a me nā kaumaha o loko.
  • ʻO ke kaumaha koʻikoʻi: Ka hoʻohuiʻana i nā hoʻomaʻamaʻa kaumaha kaumaha e like me keʻano e hiki ai ke hōʻemi i keʻano o ka hoʻoponoponoʻana e 40%.
    Hoʻomaʻamaʻa i nā kūlana koʻikoʻi e hōʻoia i ka pono o ka dimensional.

Morliengente

Hopena: Hoʻopili i nā hoʻolālā hoʻolālā mold.

  • Hoʻolālā'Oiwith maʻamau: Hoʻohana pono i nāʻenehana SAND / Camnlogies cam / cam e hoʻomaikaʻi i ka pololei, hoʻemi i nā hewa hewaʻole e 50%.
    Mālama pololeiʻia nā molds pololei i kahi kiko'ī.
  • ʻO keʻano'ōnaehana'ōnaehana: Hoʻolālā e hoʻolālā pono i nā'ōnaehana maikaʻi e kū pololei ana i ke kahe molten i ke kaheʻana i ke kahe 30%.
    ʻO ka hoʻopiliʻana i nā kākoʻo kūpono kūpono e hoʻopihapiha ana a me nā hōʻemi liʻiliʻi.

ʻO nā'āpana kūponoʻole

Hopena: Hiki i nā kūlana o nā kūlana hana a me nā kumu o nā mea i hoʻopaʻaʻia i keʻano o ka mana.

  • Nā kūlana hoihoi: Ka mālamaʻana i nāʻano hana hana kūpono e like me ka mahana, Ka paipai,
    a hiki i nā kumukūʻai hōʻoluʻolu ke hoʻokō i ka pololei o ka dimensional i loko o nā mea paʻa paʻa, ho'ēmi i nāʻano likeʻole e 20%.
  • Honua mālamalama: Hiki i ka hoʻokōʻana i nā protocols reporcols reporcols hiki ke hoʻomaopopo a hoʻoponopono i nā intaccuracies likeʻole ma keʻano o ka hanaʻana.
    Hiki i ka mana kūpono ke hoʻokaʻawale i nā helu rejection rejection e 15%.

6. Ka hopena o ka makeʻana i nā hemahema ma luna o ka hana a me ke kumukūʻai

  • Hoʻonui i nā kumukūʻai scrap: ʻO nā kumukūʻai kiʻekiʻe kiʻekiʻe e hoʻonui i nā mea waiwai a me nā uku hana.
    ʻO kēlā me kēia pākēneka e hoʻonui ai i ka helu scrap hiki ke hoʻohui 5% No nā uku hana.
  • Nā hana hana i hoʻonuiʻia: ʻO nā delays ma muli o nā hemahema ke hoʻonui i nā timoline a hoʻonāukiuki i nā papa hana.
    Hiki i nā mea hana hana ke kūʻai aku i nāʻoihana he nui o $10,000 I kēlā me kēia lā.
  • Ka mana kūpono a me ka hana hou: Ke kumukūʻai o ka hana houʻana i nā'āpana hemahema a iʻole e huki hou ana iā lākou.
    Hiki i nā mea paʻahana ke hoʻopaʻaʻia e hiki ai i ka 15% o nā kumukūʻai hana nui.
  • ʻO kaʻoluʻolu o ka mea kūʻai aku: Hiki i nā hale kūʻai maikaʻi-maikaʻi hiki ke hōʻemi i ka hana huahana a me ka hilinaʻi o ka mea kūʻai aku.
    Hiki i ka leʻaleʻa mea kūʻai aku ke alakaʻi i kahi poho o kaʻoihana, me nā haʻawina e hōʻike ana i kēlā 80% ʻAʻole hoʻi e hoʻihoʻi nā mea kūʻai aku ma hope o kahiʻike maikaʻiʻole.

7. Pehea e pale ai i ka makeʻana i nā mea kūʻai aku

Ke hoʻohālikelikeʻana i ka hoʻolālā mold:

He koʻikoʻi ka hoʻolālāʻana o ka molld no ka hōʻemiʻana i nā hemahema. E hoʻohana i nā'ōnaehana kūpono kūpono, Hoʻoponopono i ka gating no ke kahe pono kūpono,
A e hōʻoia pono i ka hoʻoponoponoʻana i ka mold a me ka hoʻemiʻana i ka hopena o ka flash a me ka pasosity.

Ke kāohi nei i nā hiʻohiʻona kaʻina hana:

Mālama i ka wela kūlike, Ka paipai, a me ka hoʻomaʻemaʻeʻana i nā kumukūʻai e hōʻoia ai i nā mea molt i hoʻopihapiha i hoʻopiha pono i ka meld kūpono a me nā mea paʻaʻole me kaʻoleʻole.

Koho kūpono a me ka laweʻana:

Ke hoʻohana nei i ka maikaʻi kiʻekiʻe, hoʻemiʻia nā mea i hoʻonuiʻia a me nā hemahema. ʻO ka mālama kūpono a me ka laweʻana i ka mea pono e pale i nā pilikia e pili ana i nā pilikia.

Hana maikaʻi a me nā hana mālama pono:

Hana maʻamau a me ka calibration o nā make, Nā Max, a me ke kōkua e kōkua i ka hōʻoiaʻana i ka maikaʻi maʻamau a hōʻemi i nā hemahema.

Hoʻomaʻamaʻa a me kaʻike:

Pono nā mea hana i hoʻomaʻamaʻa maikaʻiʻia no ka nānāʻana i nā hemahema kūpono a me ka laweʻana i nā hana hoʻoponopono kūpono.

Pono lākou e hoʻomaopopo i nā intricacies o ke kaʻina aʻike pehea e hoʻoponopono ai i nā parameter e pono ai.

8. Hopena

ʻO ka mea make e noho mau ana i kahi kaʻina hana hanaʻole, Eia nō hoʻi e hele mai me nā pilikia inherent i manaʻoʻia e hoʻokō i nā hopena maikaʻi loa.

Ma ka hoʻomaopopoʻana i nāʻano o nā hemahema, e hoʻomaopopo ana i ko lākou kumu, a e hoʻokō nei i nā ana pale,

Hiki i nā mea hana ke hoʻonui nui i ka maikaʻi a me ka hoʻoponoponoʻana o kā lākou huahana.

Ka hoʻoliloʻana i nāʻenehana loea holomua, ʻO nā kaʻina hana, A e hōʻoiaʻiʻo ana i ka hoʻomaʻamaʻaʻana i ka hana hana e hōʻemi i nā hemahema a me ka hōʻoiaʻana i kahi kūpono hanaʻaiʻai.

 

Hoa me ka deze e pale aku ai i ka makeʻana i nā drawbuby i kāu fabrication

Ma ka haʻiʻana me kēia, loaʻa iāʻoe ke komo i kaʻike a me nā hoʻololiʻana o nā kihi e kōkua ai iāʻoe e pale aku i nā hemahema a hoʻonui i kāu kaʻina hana hana.

Inā paha e ponoʻoe i nā mea kūʻai aku a paʻakikī paha, Mālama mākou i nā'āpana āu i hanaʻole ai, Ke mālama nei iāʻoe i ka manawa, Kālā kālā, a me nā kumuwaiwai i ka holo lōʻihi.

E hanaʻo Deze i kāu mea hana i hilinaʻiʻia, a hui pū pū, E lawe mākou i kāu mau hana hoʻolālā i ka pae aʻe, manuahi mai nā pilikia maʻamau maʻamau.

E hōʻea i kēia lā e aʻo pehea e hiki ai iā mākou ke kōkua iāʻoe e kūleʻa ana i kāu hana e make ai.

Kāhea iā mākou i kēia lā!