Ma hope o ka ʻoi aku 20 makahiki i ka mālama ʻana i ka ʻili - holo anodichiz Nā LESE, hoʻoponopono pilikia i nā ʻāpana hemahema, a me ka hoʻopaʻapaʻa ʻana me nā mea hoʻolālā hoʻolālā e koi nei "he alumini wale nō, pono e anodize e like me 6061" - Hiki iaʻu ke haʻi iā ʻoe i ka nīnau aʻu e lohe pinepine ai ʻo ia kēia: "Hiki iā ʻoe ke anodize i ka alumini make-cast?"
ʻO ka pane pōkole he ʻae. ʻO ka pane pololei: ʻaʻole me kāu kaʻina hana anodizing maʻamau, a ʻaʻole me ka ʻike ʻole i ke kumu e ʻokoʻa ai ka hana ʻana o die castings mai nā extrusions wrought.
Ua ʻike au i nā hale kūʻai he nui e hoʻāʻo e holo i nā ʻāpana make ADC12 ma o kahi laina anodizing maʻamau, e puka mai me ka pipili, hinahina, nā ʻāpana like ʻole i uhi ʻia i ka smut, a haʻi aku "ʻaʻole hiki ke anodized ka alumini make."
He hewa kēlā. Hiki ke anodized - akā pono ia i kahi kaʻina hana hoʻolaʻa mua, nā manaʻolana kūpono e pili ana i ka maikaʻi o ka ʻili, a me ka ʻike maopopo i kahi o nā palena kaʻina hana.
Ua kākau ʻia kēia alakaʻi mai ka papahele laina anodizing.
Ua wehewehe pono i ke kumu Die-shold ALuminum kū'ē i ka anodizing maʻamau, he aha ka pilikika me ia, he aha nā hoʻololi mua e pono ai, he aha nā pilikia i koe ma hope o ka desiliconization, a he aha nā kaʻina hana hoʻopau ʻē aʻe e noʻonoʻo ai inā ʻaʻole kūpono ka anodizing.
1. Ka Pane Pololei: ʻAe — ʻAʻole me ka hana maʻamau
E hāʻawi mua wau i ka hopena, ma mua o ko mākou ʻeli ʻana i ka kemika:
- Hiki ke anodized ka alumini die-cast.
- Hoʻopuka ka hana anodizing maʻamau i nā hopena maikaʻi ʻole ma ADC12.
- ʻO kahi desiliconizing i hoʻolaʻa ʻia (hoʻopaʻapaʻa) pono ke kaʻina hana mua.
- ʻOiai me ka desiliconization maikaʻi loa, mau pilikia porosity a me kala.
Ma kā mākou hale kūʻai ponoʻī, ua holo mākou i kahi ho'āʻo hoʻomalu: ʻelua mau ʻāpana make-cast ADC12, ʻaʻohe lāʻau lapaʻau kūikawā, holo ma ko mākou laina anodizing maʻamau. Ua maopopo kekahi (kūlohelohe) anodized, ʻeleʻele kekahi.
Ua wānana ka hopena: kūlike ʻole, kala ʻulaʻula, ʻāʻī ʻōpala, a me kahi papa o ka smut hina ma ka ʻili i holoi ʻia ma kou manamana lima.
ʻAʻole kēia he hemahema i kā mākou laina. ʻO ia ka hopena i manaʻo ʻia ke ʻanodize ʻoe i kahi huila die-cast kiʻekiʻe-silikona e like me ke ʻano āu e hana ai 6061 Kuhi.

2. No ke aha e paʻakikī ai ka Die-Cast Aluminum e Anodize?
ʻO ka pilikia mai nā kumu ʻekolu: kiʻekiʻe kiʻekiʻe silika maʻiʻo, hoʻoheheʻe porosity, a me nā palena o ka hana maʻamau.
Hoʻopilikia ka maʻiʻo Silicon kiʻekiʻe me ka Anodizing
Nui nā mea hoʻoheheʻe make i loaʻa ka nui o ka silika e hoʻomaikaʻi i ka wai, hoemi i ka hoemi solidification, a kākoʻo i ka hana ʻana i nā paia lahilahi, Nā'āpana paʻakikī.
Adoc12 he ʻelele Al-Si-Cu make-casting alloy.
Akā naʻe,, He ʻokoʻa ke ʻano o ke silika mai ka alumini i ka wā o ka hoʻomaʻamaʻa mua a me ka anodizing.
Ma kahi kaʻina hana etching alkaline maʻamau, hiki wawe ka alumini, ʻoiai e mau ana nā ʻāpana waiwai silika ma ka ʻili.
Ma muli o ka hui ʻana o ka alloy a me nā kūlana kaʻina, Hiki i kēia mau koena ke hana i kahi papa hina hina a ʻeleʻele paha.
Inā lawa ʻole ke kaʻina hana hoʻopau hope, ʻO ke koena mea waiwai silika a me nā koena alloying-element hiki ke hoʻopilikia i ka hoʻokumu ʻana o ka oxide-film a me ke ʻano..
Hōʻike kēia i nā hemahema i ʻike ʻia ma ka hoʻāʻo ADC12:
- ʻAno ʻōniʻoniʻo: ʻOkoʻa ka pane ʻana o nā wahi like ʻole o ka hoʻolei ʻana i ka pretreatment a me ka anodizing.
- kala like ole: ʻO nā ʻano like ʻole o ka microstructure o ka ʻili a me ka papa oxide e hoʻopuka i ka ʻae ʻana o ka māmā a me ka lawe ʻana i ka wai..
- ʻAhinahina hina: Ke waiho nei nā koena o ka ʻili ma hope o ka hoʻomaʻemaʻe ʻole ʻana a i ʻole ka hoʻopau ʻana.
- ʻAʻohe kala ʻeleʻele: ʻAʻole hiki ke kākoʻo ʻia ke ʻano o ka oxide a me ke ʻano o ka ʻili i ka hoʻomoʻa ʻana o ka wai.
ʻO ka mea nui, ʻo ka pilikia ʻaʻole wale ka hele ʻana o ke silika i loko o ka hui nui. ʻO ia ka pilina ma waena o ka microstructure alloy, ʻoihana hoʻomākaukau, a me ka hana kiʻiʻoniʻoni anodic.
Hoʻokumu ka hoʻolei ʻana i ka Porosity i nā hemahema hou aʻe
Hiki i ka alumini make ke komo i ka porosity kinoea, Nāʻuala, a me nā mea ʻē aʻe o lalo o ka honua.
ʻO kā lākou hāʻawi ʻana ma muli o ka hoʻolālā make, metala wela, nā ʻāpana injection, kūhewaʻi, a me nā kūlana paʻa.
Paʻakikī loa kēia mau hemahema i ka wā anodizing no ka mea ʻo ka hoʻomaʻamaʻa mua ʻana a me ka waihoʻoluʻu ʻana e hōʻike i ka hoʻolei ʻana i nā hoʻonā kemika wai..
Hiki ke hāʻawi i ka porosity:
- ʻO ka wehe ʻana o ka ʻāina a me nā kikoʻeleʻele.
- ʻO ka hoʻopaʻa ʻana o ka wai kala ʻole.
- ʻO ka paʻa ʻana o ka waikawa a me ka ʻili ʻana ma hope.
- ʻO nā pinho o ka ʻili a me ke ʻano like ʻole.
- Hoʻemi ʻia ka pale ʻana i ka corrosion kahi i hoʻopau ʻia ai ka uhi ʻana a i ʻole ke kīnā o ka hoʻolei lalo..
ʻAʻole ʻike ʻia nā porosity āpau ma ka ʻili like-cast. ʻIke ʻia kekahi mau hemahema ma hope o ka mīkini, etgian, aiʻole anodizing.
Mai kahi hiʻohiʻona hana, ʻo ia hoʻi, ʻaʻole hiki i ka hoʻopau ʻana i ka ʻili ke uku no ka maikaʻi ʻole o ka hoʻolei ʻana.
Inā makemake kekahi mea i ka hoʻopau anodized ʻeleʻele like ʻole, Pono e hoʻomaka ka mana porosity i ka hoʻomohala ʻana i ka hoʻolei ʻana ma mua o ka hiki ʻana o ka ʻāpana i ka laina hoʻopau.
3. No ke aha ʻaʻole hoʻonā ʻo Desmutting i kēlā me kēia pilikia anodizing
He hoʻomaikaʻi koʻikoʻi ka wehe ʻana i nā koena ili waiwai nui, akā ʻekolu mau pilikia nui e hiki ke noho.
| Hewa ole | Ke kumu nui | Nā Hana Mana Mana |
| ʻAhinahina a i ʻole ke koena pauda | ʻAʻole lawa ka wehe ʻana i nā koena waiwai nui o ke silikoni a me nā waihona mea hoʻohuihui ʻē aʻe | E hoʻonui i ka hoʻomaʻemaʻe a me ka holoi ʻana |
| ʻAʻohe kala ʻulaʻula a ʻeleʻele paha | Nā ʻano like ʻole o ka microstructure alloy, hoʻokumu ʻana i ka oxide, kūlana pae, a iʻole e hoʻopau ai | E hoʻomaikaʻi i ka hoʻomaʻamaʻa mua ʻana a hōʻoia i ke kaʻina kala |
| Nā kiko keʻokeʻo a i ʻole ka waiho ʻole ʻana o ka waihoʻoluʻu kūloko | Potiwale, paʻa kemika, nā hemahema ili kūloko, a i ʻole ka hoʻokumu ʻana o ka oxide | E hoʻomaikaʻi i ka maikaʻi o ka hoʻolei ʻana, drainage, holoi ʻana, a me ke kaʻina hana |
| Pinho a me nā lua ili | ʻO ka pololi, nā hemahema hōʻemi, Nā Hoʻohui, a i ʻole ka etching nui | E hoʻomaikaʻi i nā ʻāpana hoʻolei a hoʻopaʻa i ka paʻakikī o ka hoʻomaʻamaʻa mua ʻana |
| Kūlike ʻole ka mānoanoa kiʻiʻoniʻoni | Nā ʻano like ʻole o ka geometric, pili uila, hāʻawi i kēia manawa, a i ʻole ka pane alloy kūloko | E hoʻonui i ka hoʻopili, pili uila, a me nā ʻāpana anodizing |
Porosity a me ka hoʻopaʻa ʻana i ka ʻakika
Hiki ke hoʻoheheʻe ʻia me nā pores hāmama i ka hoʻoponopono mua ʻana a i ʻole ke kala kala. Inā ʻaʻole i lawe pono ʻia kēia mau mea kemika, hiki iā lākou ke hoʻomau i ka hana ʻana ma ka ʻāina a hoʻoulu i ka ʻili, nā kiko keʻokeʻo, a i ʻole nā hemahema ʻē aʻe.
ʻAʻole wale ka hoʻonā e hoʻolōʻihi i ka manawa desmutting. Hiki ke hoʻouka hou i ka ʻili me ka ʻole e hoʻopau i ka porosity lalo.
Kahi e koi ai ka helehelena, ka hoolei ana, kūlike loa ka helehelena, hoʻolālā wai, a pono e loiloi pū ʻia ka pono o ka holoi ʻana.
Nā kala kala
ʻOi aku ka koi ʻana o ka anodizing ʻeleʻele ma mua o ka hopena kūlohelohe a ʻulaʻula paha no ka mea hiki ke ʻike ʻia nā ʻano liʻiliʻi liʻiliʻi o ke ʻano o ka ʻili..
ʻO ka hiʻohiʻona hope e pili ana i ka alloy, hoʻolei microstructure, hana mua, oxide-film hiʻona, kemika kala, a me ka hana hoʻopaʻa ʻana.
ʻAʻole hiki i ʻelua mau ʻāpana i hana ʻia mai ka huila inoa like ʻole i nā hopena like inā ʻokoʻa ko lākou kūlana hoʻolei ʻana a i ʻole nā moʻolelo o luna.
No kēia kumu, Pono nā ho'āʻo hōʻoia e hoʻohana i ka hoʻoheheʻe ʻana i nā mea hoʻolaha ma mua o nā kākika hale hana hoʻonani wale.
ʻO ke ʻano o ka ʻili me ka hana hana
Hiki ke ʻae ʻia kahi mea anodized ʻoiai ʻaʻole e hoʻokō i kāna mānoanoa kiʻiʻoniʻoni i koi ʻia a i ʻole nā kumu kūʻē corrosion.
Like, Hiki ke hoʻokō ʻia kahi uhi ʻike ʻole i kekahi mau koi hana, ma muli o ke kiko'ī.
No laila, pono e hoʻokaʻawale nā pae hoʻoholo i waena:
- ʻO nā koi hoʻonaninani, me ke kala, aolama, a me nā hemahema i ʻike ʻia.
- Nā koi hana, me ka mānoanoa kiʻiʻoniʻoni, Ke kū'ē neiʻo Corrosionion, E kāʻei i ke kū'ē, a me ka hanaʻana i ka hana.
Pono e ʻae ʻia kēia mau koi ma mua o ka hoʻomaka ʻana o ka hana.
4. ʻO ka ADC12 Anodizing Reality Check
E haʻi pololei iaʻu e pili ana i kāu mea hiki a hiki ʻole ke manaʻo.
| Kālā | Hana aluminum (6061/6063) | Die-Cast ADC12 (Kaʻina Hana maʻamau) | Die-Cast ADC12 (Me ka Desiliconizing) |
| Hoʻolikelike kiʻiʻoniʻoni | Kūpono | ʻAhune - splotchy, hoʻopau ʻole | Maikaʻi - akā ʻaʻole like me ka hana ʻana |
| ʻIke ʻili | Metala maʻemaʻe, makei | ʻAhinahina hina, pulupulu | Hoʻomaikaʻi ʻia, akā ʻike ʻia ka micro-porosity ma kahi kokoke |
| kala like | Maikaʻi loa - ʻaʻahu pūʻulu | ʻilihune loa - ʻaʻole like ka lawe ʻana i ka wai | ʻAno haʻahaʻa - ʻike mau nā kala ʻeleʻele i ka ʻokoʻa |
| Smut / ke koena hina | Nookahi | Kaumaha - holoi i nā lima | Ka liʻiliʻi - wehe ʻia e HF desmut |
| Pale pale | Maikaʻi loa | Hoʻololi - hoʻopau ke kiʻiʻoniʻoni | Maikaʻi loa, aka, e mau ana na pores ma ke ano nawaliwali |
| Hua maʻamau (ʻāpana maikaʻi) | 95%+ | 30-50% | 70–85% |
He aha ke ʻano o kēia ma ka hoʻomaʻamaʻa
Inā 'oe anodize ADC12 me ka desiliconizing, manaʻo ʻia ma kahi o ka hapalua o kāu mau ʻāpana he mea hōʻole ʻia.
Me kahi hana desiliconizing kūpono, ʻoi aku ka maikaʻi o ka hua - akā ʻaʻole ʻoe e kūlike me ka maʻemaʻe, ili kīnā ʻole o kahi i hana ʻia 6063 hānehi.
ʻO ka mea e hoʻohiki i ka "extrusion-quality" anodizing ma kahi hoʻoheheʻe make he wahaheʻe a hoʻohana paha i kahi huila kūikawā haʻahaʻa-silikona..
5. Nā Kaʻina Hana Hoʻopau ʻokoʻa a me ka hoʻokūkū
No ka mea, paʻakikī ke anodize i ka alumini kiʻekiʻe-silikona make-cast, Pono e noʻonoʻo ʻia nā lāʻau lapaʻau ʻē aʻe inā ʻaʻole hiki i ka anodizing maʻamau ke hoʻokō i ke ʻano i makemake ʻia, Ke kū'ē neiʻo Corrosionion, a i ʻole ke kumukūʻai hana.
| Puni Ke hoʻopauʻana Ke kaʻina hana | Helehelena | Kuupuiawi Kū kū'ē | ʻAʻa Kū kū'ē | Pili pili Kālā | MAKAINA WAU Noi |
| Kuʻuna Anodichiz | Hoʻopau hoʻonaninani like ʻole ma nā ʻāpana kūpono; pinepine inconsistent ma kiʻekiʻe-silikona make castings | Maikaʻi ke hoʻokumu pono ʻia ke kiʻi anodic a hoʻopaʻa ʻia | Maikaʻi loa, ma muli o ka mānoanoa kiʻiʻoniʻoni a me ke ʻano | Kūpono | ʻO nā ʻāpana alumini i hana ʻia a me nā hoʻoheheʻe make kūpono e koi ana i kahi kiʻiʻoniʻoni anodic |
| Anodichiz me Kaawe | Hoʻomaikaʻi like ʻole, ʻoiai e mau ana ka hoʻololi ʻana i pili i ke silika | Maikaʻi inā hoʻomalu pono ʻia ka pretreatment a me ke kiʻi anodic | Maikaʻi loa, e pili ana i nā kikoʻī uhi | Equium-High | ʻO nā ʻāpana make-cast hana pono e koi ana i ka anodizing me nā koi hoʻonaninani haʻahaʻa |
| Micro-Arc Oxiyan (Mao) | ʻili like-ceramic; ka waihoʻoluʻu a me ke kinona ma luna o ka huila a me ka hana | Maikaʻi e maikaʻi, ma muli o ka hoʻopili ʻana a me ka hoʻopaʻa ʻana | Maikaʻi no nā pale lole pale kūpono | High | Nā ʻāpana e koi ana i ka paʻakikī o ka ʻili kiʻekiʻe, E kāʻei i ke kū'ē, a me nā'ōlelo uila |
Ka Hoʻololi Kemika |
Kope, ʻO ka maʻamau maʻamau a i ʻole ka hoʻopau kala iki | Maikaʻi loa i ka maikaʻi, ma muli o ka ʻōnaehana hoʻololi | Paʻa | Hoʻohaʻahaʻa | Nā ʻāpana e koi ana i ka pale ʻino kumu a i ʻole ka hoʻomaʻamaʻa mua ʻana no ka pena |
| Electrostatic Pauda Pāpale | ʻO ka waihoʻoluʻu kūlike me kahi ākea o nā pae ʻoniʻoni a me nā ʻano | Maikaʻi a maikaʻi loa me ka hoʻomaʻamaʻa mua ʻana a me ka mānoanoa o ka uhi | Maikaʻi loa, ma muli o ka hana pauda a me ka ho'ōla | Haʻahaʻa-medium | Urowing, nā brackets, nā'āpana automotive, a me nā pā ʻoihana e koi ana i ka pale hoʻonaninani lōʻihi |
| Pena Baki (ʻO ka uhi wai i kālua ʻia) | Hoʻopau hoʻonaninani maʻemaʻe me ka waihoʻoluʻu a me ka nani | Maikaʻi ke hoʻopili pono ʻia ka uhi a hoʻōla ʻia | Maikaʻi loa i ka maikaʻi, ma muli o ke kemika pena a me ka mānoanoa kiʻiʻoniʻoni | Kūpono | Nā mea kanu make, nā huahana kūʻai, nā'āpana automothetive, a me nā ʻāpana e pono ai ke ʻano o ka ʻili maʻemaʻe |
Pehea e koho ai i ke kaʻina hana pono
- E koho i ka anodizing me ka desiliconizing i ka wā e pono ai ka ʻāpana i kahi papa anodic oxide a ʻoi aku ka nui o kāna hana hana ma mua o ka hoʻopau hoʻonaninani ʻaʻahu.
- E koho i ka micro-arc oxidation (Mao) i ka wā e hoʻohana ai i ke kūʻē a me ka paʻakikī o ka ʻili ka mea nui.
Pono e hōʻoia ʻia kona kūpono no nā alloys kiʻekiʻe-silicona a me ka hana corrosion i koi ʻia ma o ka hoʻāʻo ʻana. - E koho i ka pauka inā ʻoi aku ka nui o ka waihoʻoluʻu a me ka uhi o ka ʻili ma mua o ka mālama ʻana i ke ʻano metala o ka alumini anodized.
Hiki iā ia ke hūnā i nā ʻokoʻa liʻiliʻi o ka ʻili, akā ʻaʻole hiki iā ia ke hoʻopau pono i nā hopena o ka porosity koʻikoʻi a i ʻole outgassing. - E koho i ka uhi hoʻololi kemika a i ʻole ka pena pulu inā ʻaʻole pono kahi kiʻi ʻoniʻoni anodic hoʻonaninani a ʻo nā koi mua he pale corrosion, hoʻopili pena, a i ʻole nā koho kala maʻalahi.
ʻO ke kaʻina hana maikaʻi loa e pili ana i ke kaiapuni lawelawe o ka mea, nā pono helehelena, a me nā kikoʻī hana.
No nā ʻāpana ADC12 e koi ana i ka pau ʻeleʻele like ʻole, ʻoi aku ka maikaʻi o ka uhi ʻana i ka pauka ma mua o ka anodizing maʻamau.
6. Ke koho ʻana i ka Alloy Die-Cast Pono no ka Anodizing
ʻAʻole nā mea alumini alumini die-cast i hana i nā hopena anodizing like. HōʻikeʻIke, pae haumia, moloka, a me ka maikaʻi o ka hoʻolei ʻana i nā hopena a pau i ka hoʻokumu ʻia ʻana o ka oxide-film a me ke ʻano o ka ʻili.
Hāʻawi ka papa ma lalo i ka hoʻohālikelike mua ʻana o nā alumini alumini i kamaʻilio maʻamau.
Hōʻike ʻia nā pae haku mele a pono e hōʻoia ʻia e pili ana i ka maʻamau kūpono a me ka palapala hoʻolako.
| Alloy | Maʻiʻo Silicon maʻamau | Anodizing Paʻakikī | Nā manaʻo nui |
| Adoc12 (A383) | 9.6–12.0% | High | Hoʻohana nui ʻia no ka hoʻolei ʻana; Hiki i ka maʻiʻo silika kiʻekiʻe ke kumu i ka anodizing ʻole a me ka smut ʻili |
| Yl102 (AlSi12) | 10.5–13.5% | High | Pili nā hopena anodizing i nā pae haumia, ʻōlelo hoʻohālikelike, a me ka maikaʻi o ka hoʻolei ʻana |
AlSi9Mg (A360) |
Ma kahi o 9.0–10.0% | ʻO ke kiʻekiʻe kiʻekiʻe | Hiki ke hāʻawi i ka hiki ke anodizing i hoʻomaikaʻi ʻia ma lalo o ke ʻano hana a me nā kūlana kaʻina kūpono |
| A413 / AlSi12(na B) | Ma kahi o 11.0–13.0% | High | Kākoʻo ka ʻike silika kiʻekiʻe i ka hoʻoheheʻe ʻana i ka wai akā hoʻopili i ka anodizing hoʻonaninani like ʻole |
| Huhū 6063 (kuhikuhi) | Ma kahi o 0.2–0.6% | Hoʻohaʻahaʻa | ʻO ka hōʻailona maʻamau no ka anodizing hoʻonaninani like ʻole |
Nānā: ʻOkoʻa nā inoa Alloy a me nā palena haku mele e like me ka maʻamau a me ka mākeke.
Yl102, A360, ʻAʻole pono e hoʻololi ʻia nā mea hoʻohui like ʻole me ka nānā ʻole ʻana i kā lākou haku mele a me nā koi mechanical.
Manao Hooikaika
Inā he koi hoʻolālā koi ʻia ka anodizing a ʻaʻole koho ke alumini hana, e loiloi i ka AlSi9Mg a i ʻole kahi mea hoʻoheheʻe haʻahaʻa haʻahaʻa haʻahaʻa i hoʻohālikelike ʻia ma mua o ka hana ʻana i ka hana..
Hiki i kēia mau mea ke hāʻawi i ka ʻoi aku ka maikaʻi o ka ʻili ma lalo o nā kūlana kūpono, akā, ʻaʻole lākou e loaʻa i ke ʻano like me ka anodized 6063.
No kēlā me kēia huila moho, hoʻopaʻa i ka silikoni a me ka hao, maikaʻi hoʻolei, Pono nā mea iʻikeʻia, a me ka launa pū me ke kaʻina hana mua i manaʻo ʻia.
Pono e hana ʻia ka anodizing hoʻāʻo ma nā ʻāpana hana-makaʻāinana e hōʻoia i ka like ʻole o ka waihoʻoluʻu, maikaʻi kiʻiʻoniʻoni, a me ka hana corrosion.
Lākahi, Pono e noʻonoʻo pū ʻia ke koho ʻana i ka alloy a me ka hoʻomohala ʻana i ka mālama ʻana i ka ʻili.
Hiki ke hoʻomaikaʻi i ka hopena i ke koho ʻana i kahi alloy anodizable, akā, ʻaʻohe inoa alloy wale nō e hōʻoiaʻiʻo i kahi hoʻopau anodized hala ʻole.
7. Hopena
Hiki iā ʻoe ke anodize i ka alumini die-cast? ʻAe, akā, pono ka noʻonoʻo pono ʻana i nā mea hao silicon kiʻekiʻe e like me ADC12.
ʻO ka anodizing maʻamau me ka hoʻomaʻamaʻa ʻole ʻana i ka alloy-specific pretreatment hiki ke hana i ka waihoʻoluʻu mottled, ilihune kiʻi like ʻole, a hina hina.
ʻO kahi kaʻina hana hoʻopau kūpono - i kekahi manawa me ka hoʻohana ʻana i kahi hopena i loaʻa i ka HF ma lalo o nā kūlana ʻoihana i hoʻomalu ʻia - hiki ke hoʻomaikaʻi nui i ka ʻili ma ka wehe ʻana i nā koena waiwai nui..
Akā naʻe,, ʻAʻole hoʻopau ka desmutting i ka porosity, hōʻoiaʻiʻo i ka hoʻoheheʻe ʻana i ka waiʻaʻahu like ʻole, a i ʻole nā hemahema i hoʻokumu ʻia e ka paʻa ʻole a me ka hoʻomākaukau ʻana i ka ʻili.
Pono kēia mau pilikia i ka mana hoʻonohonoho o ke koho ʻana i ka alloy, maikaʻi hoʻolei, hana mua, anodichiz, a me ke kala.
He maʻalahi ke kānāwai kūpono: ʻAʻole hiki ʻole ke anodize ka alumini make-cast, akā, ʻaʻole pono ke anodized me he mea lā he alumini alumini hana maʻamau.
I ka wā e pono ai ka hoʻopau ʻana i ke kāhiko like ʻole, e hoʻokō i ke kaʻina hana piha me ka hoʻohana ʻana i nā ʻāpana hana-representative a hoʻohālikelike i ka anodizing me nā mea ʻē aʻe e like me ka uhi pauka a i ʻole micro-arc oxidation ma mua o ka hana ʻana i ka hana nui..
FaqS
No ke aha e puka mai ai ka anodizing make-cast i ka hina a me ka maʻemaʻe?
Maʻiʻo silika kiʻekiʻe (9–12% ma ADC12) e waiho ana i ke silika elemental ma ka ili ma hope o ke etching.
Hoʻopilikia kēia smut silika i ke kiʻiʻoniʻoni oxide a hana i ka hina, ʻano like ʻole. Hoʻopau ka desiliconizing i kēia papa.
He aha ke koho maikaʻi loa i ka anodizing no ka alumini die-cast?
ʻO ka uhi ʻana i ka pauka ka mea kaulana loa - uhi ia i ka porosity, hāʻawi maikaʻi i ke kala like ʻole, a hāʻawi maikaʻi i ka pale corrosion.
No ka pale ʻana i ka ʻaʻahu, micro-arc oxidation (Mao) hana maikaʻi ma ka kiʻekiʻe-silikona make castings.
E like me ka desiliconizing i kaʻu mau ʻāpana make 6063 anodized?
ʻAʻole. Hoʻoponopono ka desiliconizing i ka smut a me ka pau ʻole, akā, ʻo ka porosity make-cast ke kumu i nā hemahema ʻike ʻia a me nā kiko wai.
He maikaʻi ka hopena no nā ʻāpana hana, akā ʻaʻole like me ka anodize alumini hana.
Pono au i ka impregnation vacuum no nā ʻāpana make-cast anodized?
No nā mea hoʻomaʻemaʻe a i hoʻopaʻa ʻia paha kahi e hoʻokahe ai ka waika, ʻAe.
Hoʻopaʻa ʻia ka impregnation vacuum i ka porosity subsurface ma mua o ka anodizing, ka pale ʻana i ka ʻakika i paʻa ʻia mai ka lele ʻana ma hope o ka pau ʻana.