6061 Aluminim vs 6063 Aluminum

6061 Aluminim vs 6063 Aluminum

1. Hōʻikeʻike

Ua liloʻo Alumini alloys i lilo i mau mea hana hou i ka hana hou, Mahalo i kā lākouʻanoʻokoʻa o ka ikaika, Ke kū'ē neiʻo Corrosionion, a me ke kukui kukui.

Ke kohoʻana i ka allununum aluminum a alloy he mea nui no ka hōʻoiaʻana e hoʻokō ana kāu papahana i kāna hana, durability, a me nā koi kūpono.

E hoʻohālikelike kēia blog iʻelua Apana Apana Aluminum, 6061 a 6063, Keʻimi nei i kā lākou waiwai, noi, a me nā mea nui e kōkua ai e kōkua iāʻoe e hoʻoholo i kahi hoʻoholo.

2. Overview o 6061 a 6063 Apana Apana Aluminum

Ma mua o ka hoʻokaʻawaleʻana i nā kiko'ī, He mea nui ia e hoʻomaopopo i nā hiʻohiʻona core o nā alloysʻelua.

6061 Aluminum

Kaulana no kona ikaika a me kona ikaika kiʻekiʻe, 6061 he mea paʻaʻole a Alluinum, nui loa me ka magnesium a me ka silika.

6061
6061

He ikaika kiʻekiʻe loa ia i hoʻohālikelikeʻia i nā alloys'ē aʻe, Ke kūpono nei i nā noi i kahi e loaʻa ai ka kī.

  • Ka Hoʻolālā: Maki, Aia ia 0.8-1.2% Magnesum, 0.4-0.8% Silikino, a me nā'āpana liʻiliʻi (0.15-0.4%), 'Eron (0.7% max),
    Chromium (0.04-0.35%), zinc (0.25% max), a me nā mea'ē aʻe.
    , Hāʻawi iā ia i kona ikaika a me ke kū'ēʻana.

6063 Aluminum

Ma ka lima ʻē aʻe, 6063 makemakeʻia no kāna hana maikaʻi loa a me ke kiʻekiʻe kiʻekiʻe. Hoʻohana pinepineʻia ia i nā hana extrusion a me nā noi e koi ana i kahi hopenaʻikeʻike.

6063
6063
  • Ka Hoʻolālā: Aia i ia 0.45-0.9% Magnesum, 0.2-0.6% Silikino, a me nā'āpana liʻiliʻi o ke keleawe (0.1% max), 'Eron (0.35% max), mang kāne (0.1% max),
    a me nā mea'ē aʻe.
    , hopena i konaʻanoʻano palupalu a me ka maʻalahi o ka hoʻokumuʻana.

3. 6061 Aluminum: Nā waiwai a me nā noi

Nā mea nui:

  • Ikaika: 6061 ʻO ka ikaika o ka ikaika kiʻekiʻe, ʻO ka maʻamau maʻamau mai 42,000 i 45,000 Psi (paona i kēlā me kēia pahu pahu). ʻO kona ikaika e hāʻawi ai 35,000 i 40,000 Psi.
  • Ke kū'ē neiʻo Corrosionion: Hāʻawi ia i nā pale kū'ē maikaʻi loa, i loko o ka marine a me nā wahi waho, Mahalo i kona pale pale pale.
  • Wawahua: 6061 hiki ke hoʻohanaʻia e hoʻohana ana i nāʻano likeʻole, komo me ka tig, Iaʻu, a me ka hele ana.
    ʻO ka hoʻonuiʻana a me ka mālamaʻana i ka hana wela wela i hoʻonui pinepineʻia i ka maikaʻi a me keʻano kūpono.
  • Markinpalibility: Oiai 6061 he maʻalahi ka mīkini, Pono paha e koi i nā mea hana kūikawā ma muli o kona paʻakikī.
    ʻO ka helu helu match a puni 70-80% ua hoʻohālikelikeʻia i ke keleawe matching manuahi.

Nā'Āpana Hoʻonuiʻia:

  • Nā Māhele kā Aerospace: Hoʻohanaʻia i loko o nā mokulele mokulele, e like me nā'ēheu, Nā Pili, a me ka pae'āina, kahi a me nā ikaika kiʻekiʻe a me nā pono māmā e pono ai nā waiwai.
  • Aitompetitive Nā'āpana: Hoʻohana pinepineʻia i nā poloka mīkini, Nā'āpana i hoʻokuʻuʻia, a me nā'āpana, hoʻolako i kahi kaulike o ka ikaika a me ke kaumaha.
  • Nā hana hana: Kūpono no ka kūkuluʻana a me ke kūkuluʻana, Ma kahi e pono ai ka ikaika kiʻekiʻe a me ka nui o ka ikaika, e like me nā alahaka a me nā scaffolding.
  • Nā lako hanaʻoliʻoli: Hoʻohanaʻia ma nā keke, Nā Wats, a me nā huahana haʻuki, Ma kahi e pono ai ka ikaika a me ka paleʻana.
6061 Nā'āpana aluminum
6061 Nā'āpana aluminum

No ke aha mai 6061 ua koho pinepineʻia no nā noi kiʻekiʻe:

  • ʻO kāna mau mea kiʻekiʻe kiʻekiʻe a me nā ikaika e hāʻawi ai i ka maikaʻi no nā noi i kahi e koʻikoʻi ai ka hoʻonohonohoʻana.
  • ʻO ka hiki ke hana i nā kūlana weliweli a mālama i kāna mau waiwai ma luna o ka manawa e hana ai i kahi koho kūpono no ke koiʻana i nā wahi koi.

4. 6063 Aluminum: Nā waiwai a me nā noi

Nā mea nui:

  • NoMame: 6063 he mea nui loa a hiki ke maʻalahi maʻalahi i loko o nāʻano paʻakikī, e hana ana i ka'āina no ka nui o nā hoʻolālā.
  • Paulapua: He mea maikaʻi loa ia, hopena maikaʻi, Ke kūpono nei ia no nā noi a me nā palapala noi. Hiki i ke anidizing ke hoʻonui hou i konaʻano a me ka nui.
  • Ke kū'ē neiʻo Corrosionion: E like me 6061, 6063 Hāʻawi i ke kū'ē kū'ē, nui i ka wā i loaʻa ai. Hana ia i kahi pale pale pale e pale aku ai i keʻano o ka wai.
  • Wawahua: 6063 hiki ke hoʻopauʻia, akāʻoi aku ka maikaʻi e hoʻopiliʻia i ka 6061. E makaʻala i ka mālamaʻana i nā pale uldings a me ka preheating hiki ke hoʻokō i kēia mau pilikia.

Nā noi maʻamau:

  • Matapili: Hoʻohanaʻia ma nā puka makani, Nā pahu puka, a me nā kaʻa, kahi i maʻemaʻe, Ua makemakeʻo Aesthetically.
  • Nā mea ukana: Maʻamau ma nā wahi waiwai, e like me nā wāwae noho a me nā papa papa, kahi o ka formability a me ka hoʻopauʻana he mea nui.
  • Nā huahana kūʻai: Loaʻa ma nā huahana kūʻai likeʻole, me nā hoʻopili uila uila a me nā kīhini, kahi e pili ana i ka hana a me ka hiʻohiʻona.
  • 'Āpana Noihia: Hoʻohanaʻia ma nā hōʻailona hōʻailona a hōʻike i ka hopena ma muli o kona hoʻopau maikaʻiʻana a me ka formability, E hoʻomaʻamaʻa maʻalahi e hana i nā hoʻolālā hoʻolālā.
6063 Nā'āpana aluminum
6063 Nā'āpana aluminum

No ke aha mai 6063 i makemakeʻia no ka extrusion a me nā kumu aesthetic:

  • ʻO kāna hana maikaʻi loa a me keʻano o ka hoʻopauʻana i ka hana kūpono no ka hoʻokumuʻana i nā hoʻolālā a me nā hoʻolālāʻole.
  • Uaʻae ka maʻalahi o ka extrusion no ka hanaʻana o ka nui o nāʻano ākea a me nā profile, hoʻemi i nā kumukūʻai hana a hoʻomaikaʻi i ka hana.

5. Nā Pīkuhi Propertinies: Kahi wahi e hoʻohālikelike ai

E hoʻomaopopo maikaʻi i nāʻokoʻa ma waena 6061 a 6063, E hoʻohālikelike mākou i kā lākou mau mea hana:

Waiwai 6061 Aluminum 6063 Aluminum
Ikaika ikaika 42,000-45,000 psi 25,000-30,000 PSI
Ka ikaika 35,000-40,000 PSI 21,000-24,000 psi
Ewangantion 10-12% 15-20%
Paʻakikī paʻakikī 95 70
Malting Point 580-650 ° C 615-655 ° C

E like me ka papa hana o kēia papa, 6061 ʻoi aku ka ikaika, aka, 6063 Hāʻawi i kahi kūpono loa a me ka formability, e hana maikaʻi ana i nā noi i nā noi i nā mea hoʻohālikelike a me nā hoʻolālā e pono ai.

6. Nāʻokoʻa ma waena 6061 Aluminim vs. 6063 Aluminum

Ka Hoʻolālā:

  • 6061: Aia nā kiʻekiʻe kiʻekiʻe o ka magnesium a me Silikona, me nā liʻiliʻi liʻiliʻi o nā mea'ē aʻe, Ke hāʻawi nei i kona ikaika kiʻekiʻe.
  • 6063: Aia nā kiʻekiʻe haʻahaʻa o ka magnesium a me Silikona, me nā mea liʻiliʻi likeʻole, e hana hou aku ai iā ia a maʻalahi e hana me.

Ikaika:

  • 6061: Ikaika a ikaika loa, kūpono no nā noi kiʻekiʻe.
  • 6063: Emi iki akāʻoi aku ka nui, Kūpono no nā noi a me nā noi haʻahaʻa haʻahaʻa.

Hana:

  • 6061: ʻOi aku ka paʻakikī e hana me, e koi ana i nā ikaika hou a me nā mea hana kūikawā.
  • 6063: ʻOi aku ka maʻalahi o keʻano a me ka hewa, Me ka hoʻopauʻana, e hana ana i ke kumukūʻai-maikaʻi no nāʻano paʻakikī.

Ke kū'ē neiʻo Corrosionion:

  • 6061: ʻO ke kū'ēʻana o ka corrossion maikaʻi, i loko o nā wahi moana, Ma muli o kona pale pale pale.
  • 6063: Hāʻawi pū i ke kū'ē kū'ē, Akā e koi paha i nā hana hou e like me ka anodicit no ka hana maikaʻi loa.

Wawahua:

  • 6061: Hiki ke hoʻopauʻia, akā,ʻo ka mālamaʻana a me ka hana wela o ka wela e pono ai e hōʻoia i ka hōʻoiaʻana i kahi paʻa ikaika a ikaika.
  • 6063: Welible, akāʻoi aku ka maikaʻi, e koi ana i ka mālama ponoʻana i nā pale o nā mea hana a me ka mua.

Paulapua:

  • 6061: Maikaʻi loa, Akāʻaʻole ia e like me 6063, ʻO ka hanaʻana i nā mea kūpono no ka hana ma mua o nā noi e nānā ai.
  • 6063: Kūpono, me kahi hopena maikaʻi loa a maikaʻi hoʻi, Kūpono no nā noi a me nā noi aesthetic.

ʻO ka wela wela:

  • 6061: Hana wela, ʻO ka mālama wela maʻamauʻo ia kaʻoihana lapaʻau T6, ʻaeʻia no ka hoʻonuiʻiaʻana o nā mea hana mechanically ma o ka hoʻomehanaʻana i nā kaʻina hana.
  • 6063: ʻO ka mea wela i mālamaʻia, Akāʻoi aku ka paʻakikī o ke kaʻina hana no ka loaʻaʻana o nā waiwai i makemakeʻia, e hana pono ana e hana me.

Lihui:

  • 6061: Hiki ke lilo, akā me ka paʻakikī a me nā uku kiʻekiʻe ma muli o kona ikaika kiʻekiʻe.
  • 6063: Luhi nui loa, e hana ana i ke kumukūʻai-kūpono no ka hanaʻana i nāʻano paʻakikī a me nā profile.

Loaʻaʻia:

  • 6061: Loaʻa nui loa i kahi ākea ākea o nāʻano a me nā nui, Ke loaʻa nei iā ia no nā noi likeʻole.
  • 6063: A laila e loaʻa nō hoʻi, nui loa i nāʻano extruded, a ua hoʻohana pinepineʻia ma nāʻoihana he nui.

Nā hoʻohālikelike kumukūʻai:

  • 6061: ʻOi aku ka nui o nā kumukūʻai ma muli o kona ikaika kiʻekiʻe a me nā noiʻi kūikawā.
  • 6063: ʻOi aku ka uku haʻahaʻa, Ke hana nei i kahi koho koho-kūpono no nā noi he nui, ʻO ka mea e koi ai i ka formability a me kahi mea maikaʻi maikaʻi.

7. 6061 Aluminim vs. 6063 Alumini no nā extrusions

I ka hikiʻana mai i nā alumini, ʻO ke koho ma waena 6061 a 6063 hilinaʻi nuiʻia i nā koi o nā noi.

  • 6063 No nā mea hoʻonāukiuki: Me kona kūlana kiʻekiʻe loa a me ka maʻalahi o ka hanaʻana, 6063 ua hoʻohana nuiʻia ma nā mea hana hoʻokūkū hoʻokūkū e like me nā pahu window, Nā mākaʻi, a hui pū me nā provige signage.
  • 6061 No nā mea hoʻonāukiuki: ʻOiai e like me ka mea maʻamau no nā extrusions, 6061 ua hanaʻia ma nā noi e koi ana i nā ikaika hou a me ka nui, e like me nā mea i hoʻohālikelikeʻia i nā mea kanu a me nā mīkini ikaika.

No nā papahana e noi ai i nāʻano paʻakikī a me kahi hoʻopau poli, 6063 ʻo ka maʻamau ka hele. Akā naʻe,, Inā he ikaika ka ikaika, 6061 hāʻawi maikaʻi i ka hana maikaʻi.

8. Ke kohoʻana i ka alloy kūpono: 6061 Aluminim vs. 6063 Aluminum

E hoʻoholo i ka alloy maikaʻi loa no kāu papahana, E noʻonoʻo i nā mea i hala:

E hoʻoholo i ka ikaika i koiʻia a me ke kū'ē:

  • Nā noi kiʻekiʻe kiʻekiʻe: Koho 6061 No kona ikaika ikaika a me ka paakiki, nui loa ma ka aerospace, aitompetitive, a me nā noi kūpono.
  • ʻO nā noi haʻahaʻa haʻahaʻa a me nā'ōlelo hoʻonaninani: Koho no ka 6063 no kona koina a me ka hoʻopauʻana, Ke kūpono nei no ka hoʻolālāʻana, nā mea ukana, a me nā huahana waiwai.

Hoʻoholo i ka hoʻopauʻana:

  • ʻO ka hoʻopauʻana a me Aesthetic hoʻopau: 6063 ʻo ke koho maikaʻi loa no nā noi ma kahi o ka helehelena he mea nui, e like me nā huahana a me nā huahana kūʻai.
  • Hana hana: 6061 he kūpono no nā noi eʻoi aku ka mea nui ma mua o nā aesthetics, e like me ka hoʻohanaʻana a me nā hoʻohanaʻana i kaʻoihana.

E noʻonoʻo i ke kumukūʻai a me ka loaʻa:

  • Nā Kuʻuna kālā: 6063 ʻoi aku ka nui o ke kumukūʻai-kūpono a me ka nui, Ke hana nei i kahi koho kālā-aloha no nā papahana he nui.
  • Pono nā pono kūikawā: 6061 ʻoi aku paha ke kumukūʻai akā he mea pono no nā noi kiʻekiʻe, e hōʻoia ana i ke kumukūʻai kiʻekiʻe.

Loiloi i ka nommability a me ka mancinability:

  • ʻO nāʻano paʻakikī a me nā profiles: 6063 e maʻalahi keʻano o keʻano a me ke kumu, ʻO ka hoʻolālā kūpono no nā hoʻolālā komoʻana a me nā profile.
  • Maki: 6061 he kūpono kūpono no nā noi noi e koi ana i ka mana kūpono a me ka ikaika kiʻekiʻe, e like me ka aerospace a me nā mea hana AutoMottive.

E noʻonoʻo i ka hoʻohanaʻana a me nā hiʻohiʻona hui:

  • Nā koi e pono ai: 6061 ʻoi aku ka maikaʻi akā pono ke koi pono i ka hoʻokele wela, me ke komoʻana a me ka hana wela wela.
  • Nā mea paʻaʻoleʻole: 6063 He kūpono no nā noi kahi i liloʻole ai i ka manaʻo nui, a iʻole kahi e hui pū ai, e like me ka hoʻomaʻemaʻeʻana, makemakeʻia.

Loiloi i ka hana wela:

  • Nā waiwai nui: ʻO nā alloysʻelua he wela-mālamaʻia, aka, 6061 Loaʻa nā pōmaikaʻi hou mai ke kaʻina, ʻaeʻia no ka hoʻomaikaʻi nuiʻana i ka ikaika a me ka nui.
  • Nā kaʻina hana maʻalahi: 6063 hiki ke hoʻohanaʻia me kaʻole o ka mālama wela no nā noi he nui, Hoʻololi i ka hana hana a me ka hōʻemiʻana i nā uku.

E nānā no kaʻoihana a iʻole nā ​​kūlana hoʻoponopono:

  • Kamana: E hōʻoia i ka mea i kohoʻia ai ka mea i kohoʻia e pili ana i kaʻoihanaʻoihana a me nā kūlana hoʻoponopono no kāu noi, e like me ka astm a iʻole nā ​​kūlana o ISO.

Kūkākūkā me kahi loea a iʻole mea kūʻai aku:

  • 'Ōlelo aʻo: E kūkākūkā me nā mea loea a iʻole nā ​​mea lawelawe e loaʻa ai i nā'ōlelo aʻoaʻo e pili ana i ka pono o kāu papahana. Hiki iā lākou ke hāʻawi i nā meaʻike waiwai a me nā'ōlelo noʻonoʻo.
  • Kākoʻo kākoʻo: Hiki i nā mea kūʻai aku ke hāʻawi aku i ke kākoʻo loea a me ke alakaʻi ma ke koho a me ke kaʻina hana, Ke hōʻoia neiʻoe e hana i ke koho kūpono no kāu papahana.

9. Hopena

I ka hōʻuluʻuluʻana, 6061 a 6063 ʻO Aluminim heʻano maʻamau a hoʻohana pinepineʻia nā alloys, kēlā me kēia me kāna mau hana pono'ī a me nā noi.

6061 ua makemakeʻia no nā noi kiʻekiʻe a me nā noi a me nā noiʻana ma muli o kona ikaika kiʻekiʻe a me ka nui,

oiai 6063 he kūpono no nā noi a me nā noi haʻahaʻa haʻahaʻa, Mahalo i kāna hana maikaʻi loa a me ka hoʻopauʻana.

Hoʻomaopopo i kā lākou mauʻokoʻa koʻikoʻi eʻae iāʻoe e hana i ke koho kūpono no kāu mau koi kūpono.

I ka wa kanalua, He mea maikaʻi loa ia kūkākūkā me kēia No ka hōʻoiaʻana i ke kohoʻana i nā mea kūpono.

FaqS

Q: ʻO ka alloy alloy no ka hoʻohanaʻana i waho?

A: Elua 6061 a 6063 Hāʻawi i ke kū'ēʻana o ka maikaʻi, aka, 6061 ʻoi aku ka nui o nā pale, nui loa ma nā wahi moana.
No nā noi o waho, 6061 ʻo ka pinepine ka meaʻoi aku ka maikaʻi ma muli o kona mau manawaʻoi loa a me ka ikaika.

Q: Hiki 6061 a 6063 e hoʻohanaʻia?

A: Aʻo lākou e kaʻana like i kekahi mau mea like, 6061 a 6063 he mau mea likeʻole a kūpono paha no nā noi likeʻole.
Hiki iā lākou ke alakaʻi i ka hana suboptimal, No lailaʻoi aku ka maikaʻi e koho i ka alloy e kūpono i kāu mau pono.

Q: Aia kekahi mau hopohopo palekana me ka hoʻohanaʻana i kēia mau alloys?

A: Elua 6061 a 6063 E palekana i ka hoʻohanaʻana i nā noi. Akā naʻe,, hana kūpono a me ka hoʻoiliʻana,
e like me ka hoʻohanaʻana i nā lako palekana palekana kūpono a me nā papa kuhikuhi palekana palekana, he mea pono e hōʻoia i ka palekana.
KAHUIA, E hahai i nā hana maikaʻi loa no ka hoʻohanaʻana a me ka machining e pale aku i nā pōʻino.