Butterfly Valves Components Manufacturer

Custom Butterfly Valves: China Valve Foundry

Mga Nilalaman ipakita ang

1. Panimula

Custom Butterfly valves are essential components in modern fluid control systems, known for their compact design, fast operation, at maraming nalalaman.

Originally conceptualized in the early 20th century, these Mga balbula have evolved significantly to meet the growing demands of industries requiring efficient and cost-effective flow control solutions.

Ngayon, butterfly valves are widely used in diverse sectors such as paggamot ng tubig, langis at gas, HVAC, pagproseso ng kemikal, marine, at pagkain at inumin mga industriya.

Their popularity stems from their ability to handle a broad range of fluids—including gases, liquids, and slurries—with minimal pressure drop and rapid shutoff capabilities.

2. What Is a Butterfly Valve?

A balbula ng paruparo is a type of quarter-turn rotary valve used to regulate, isolate, or control the flow of fluids, mga gas, or slurries in piping systems.

Its name is derived from the disc’s operation, which resembles a butterfly’s wings as it rotates within the valve body.

Butterfly valves are widely recognized for their compact na disenyo, quick actuation, mababang gastos, at broad size range, making them suitable for both low- and high-pressure applications across a variety of industries.

Mga Valve ng Butterfly
Mga Valve ng Butterfly

Core Components and Their Functions

Valve Body

The valve body is the outer casing that houses all internal components and interfaces with the pipeline through wafer, lug, flanged, or butt-welded ends.

Valve sizes typically range from DN50 (2 pulgada) to over DN3000 (120 pulgada) for large-scale industrial applications.

Butterfly Disc

The disc is the rotating element that regulates flow. Shaped like a circular or elliptical plate, it is mounted either centrally or slightly offset on the shaft.

When rotated 0° (parallel sa daloy), the disc allows full flow through the valve. When turned 90° (patayo), it fully blocks the flow, achieving shutoff.

Valve Stem (Shaft)

The stem connects the actuator to the disc, transmitting the torque necessary for rotation.

In large or high-pressure valves, the stem may include upper and lower bearings or bushings to reduce operating torque and extend service life.

Upuan (Seal)

The seat is a ring-shaped sealing surface located inside the valve body. It interacts with the disc edge to provide a tight seal when closed. The seat plays a critical role in leak-tightness and longevity.

Actuator

A mechanism (manu-manong, niyumatik, mga elektriko, or hydraulic) that drives the disc’s rotation. Manual actuators use handwheels or levers; automated versions integrate with control systems for remote operation.

3. Working Principle of Butterfly Valves

Butterfly valves function based on a quarter-turn rotational motion that controls the position of a disc relative to the flow path.

The simplicity of this design allows for mabilis na operasyon, reliable shutoff, and efficient flow modulation, making them widely used in both on-off and throttling applications.

Basic Operating Principle

At the heart of a butterfly valve’s operation is the disc, which rotates around a central or offset shaft:

  • Open Position (0°): When the disc is aligned parallel to the flow direction, the valve offers minimal flow resistance.
    This allows the medium to pass through almost unimpeded, resulting in a low-pressure drop across the valve.
  • Closed Position (90°): When the disc is rotated perpendicular to the flow, it presses tightly against the seat, forming a seal that stops the flow.
    Depending on the valve type (nababanat, mataas na pagganap, or triple offset), this seal may be either soft or metal-to-metal.
  • Throttling (10°–80°): Intermediate positions allow partial opening of the valve, where the disc restricts the flow similar to an orifice plate.
    The valve can be used to control flow rate, although accuracy varies based on disc design and valve type.

Flow Modulation Characteristics

The relationship between disc angle and flow rate is non-linear, particularly for standard resilient-seated butterfly valves.

At lower disc angles, small movements cause significant changes in flow, which can make precise modulation challenging.

Gayunpaman, high-performance and triple offset butterfly valves offer improved control characteristics and are better suited for regulated flow applications.

Sealing Mechanisms

Butterfly valves achieve shutoff through direct contact between the disc edge and the valve seat. Ang type of seal determines both the performance and application suitability:

  • Resilient-Seated: Utilizes a soft elastomeric seat (hal., EPDM, NBR) for bubble-tight sealing.
    Ideal for low- to medium-pressure systems but may degrade in corrosive or high-temperature environments.
  • Mataas na Pagganap (Double Offset): The disc is offset from the seat centerline, reducing friction during operation and improving sealing under pressure. Suitable for moderate pressure and temperature applications.
  • Triple Offset: Adds a third geometric offset to eliminate friction entirely during operation, allowing metal-to-metal sealing suitable for high-pressure, mataas na temperatura, and critical service conditions.

Speed of Operation

Thanks to the 90° rotational motion, butterfly valves can be operated rapidly:

  • Manual valves typically require one quick turn of the lever or several turns of a gearbox.
  • Automated valves (mga elektriko, niyumatik, o haydroliko actuators) can open or close in 1 sa 5 mga segundo, depending on valve size and actuator type.

This speed makes butterfly valves ideal for emergency shutdown systems (ESD), frequent cycling operations, or processes requiring rapid flow isolation.

4. Types of Butterfly Valves

Butterfly valves come in a wide variety of configurations tailored to specific installation requirements, performance criteria, and actuation preferences.

They are commonly classified based on body design, Pagganap ng pagbubuklod, at actuation method.

Based on Body Design

This classification refers to how the valve connects to the piping system and how it is supported structurally.

Wafer Type Butterfly Valve

Ang wafer-style butterfly valve is the most common and cost-effective design.

It is designed to be sandwiched between two pipeline flanges using long bolts that pass through the valve body and both flanges.

Wafer Type Butterfly Valves Components
Wafer Type Butterfly Valves Components

The wafer valve provides a tight seal against bi-directional pressure, preventing backflow.

Gayunpaman, it does not support downstream piping, so it is not suitable for applications requiring dead-end service.

Lug Type Butterfly Valve

The lug design features protruding lugs with threaded inserts around the valve body, allowing the valve to be bolted to each flange separately.

Lug Type Butterfly Valves
Lug Type Butterfly Valves

This configuration enables one side of the piping system to be disconnected without affecting the other, making it useful for systems that require periodic maintenance or isolation of a single side.

Lug-type valves are suitable for dead-end service when installed with the appropriate pressure rating.

Double Flanged Butterfly Valve

The double-flanged design includes flanges on both ends of the valve body, which are bolted directly to the pipeline flanges.

This construction provides enhanced mechanical strength and support for heavy piping systems.

Double Flanged Butterfly Valves
Double Flanged Butterfly Valves

It is particularly suited to large-diameter pipelines, buried installations, and applications involving frequent opening and closing.

Butt-Welded End Butterfly Valve

Sa ganitong uri, the valve is permanently welded to the pipeline, eliminating flanged joints and reducing potential leak points.

Butt-Welded End Butterfly Valves
Butt-Welded End Butterfly Valves

This design is ideal for high-pressure, mataas na temperatura, or hazardous environments where joint integrity and long-term sealing are critical.

Typical applications include oil and gas, pamamahagi ng halamang singaw, and process plants handling toxic or flammable fluids.

Based on Sealing and Performance

Butterfly valves also vary based on the sealing mechanism and their suitability for different pressure and temperature conditions.

Resilient-Seated Butterfly Valve

These valves use a soft elastomeric seat (such as EPDM, NBR, o Viton) to provide bubble-tight shutoff.

The disc compresses against the seat to form a seal, which is effective for clean water, hangin, and non-aggressive fluids.

Resilient Seated Butterfly Valves
Resilient Seated Butterfly Valves

Resilient-seated valves are widely used in water treatment, HVAC, and low-pressure industrial applications.

They typically operate within a pressure rating of PN10–PN16 and temperatures up to 200°C.

High-Performance Butterfly Valve (Double Offset)

High-performance butterfly valves incorporate a disc that is offset from the centerline of both the pipe and the shaft.

This double-offset design reduces friction between the disc and seat during operation, extending the valve’s lifespan and allowing it to handle higher pressures and temperatures—up to Class 300 and around 400°C.

High-Performance Butterfly Valve
High-Performance Butterfly Valve

These valves are suited for applications in power generation, petrochemical systems, and steam service.

Triple Offset Butterfly Valve

The triple offset design includes a third geometric offset that results in a conical seating surface, eliminating rubbing between the disc and seat.

These valves typically use metal-to-metal seating, allowing them to achieve zero-leakage shutoff (Class VI) under high-pressure and high-temperature conditions—up to Class 600 and 600°C.

Triple Offset Butterfly Valves
Triple Offset Butterfly Valves

Triple offset valves are ideal for critical applications such as steam, cryogenic service, hydrocarbon processing, and corrosive chemical handling.

Based on the Actuation Method

The actuation method determines how the valve is operated—manually or through automation.

Manual Actuation Butterfly Valve

Manual butterfly valves are operated using a lever (for small diameters) or a gear operator (for larger sizes). Ang mga ito ay cost effective, simple to install, and easy to maintain.

These valves are appropriate for systems where flow changes are infrequent and remote operation is unnecessary.

Electric Actuation Butterfly Valve

Electric actuators use a motor to open and close the valve disc, providing precise control over valve positioning.

These actuators can be integrated into automated systems such as SCADA or PLCs, enabling remote operation and diagnostics.

Electric actuation is commonly used in building automation, water distribution networks, and industrial process control.

Pneumatic Actuation Butterfly Valve

Pneumatic actuators operate the valve using compressed air. They are known for rapid response times and reliable cycling.

Pneumatic butterfly valves are commonly found in chemical plants, food processing facilities, and clean-in-place (CIP) mga sistema, where frequent actuation and quick shutoff are required.

Hydraulic Actuation Butterfly Valve

Hydraulic actuators use pressurized hydraulic fluid to generate torque, making them suitable for large-diameter valves or systems with high operating pressure.

They offer excellent force transmission and are used in demanding industries such as offshore drilling, mga planta ng kuryente, and heavy manufacturing.

5. Materials and Coatings of Butterfly Valves

The choice of materials and coatings in butterfly valve construction is critical to ensuring durability, chemical compatibility, pressure integrity, at paglaban sa kaagnasan.

Depending on the application—whether it’s potable water, mga kemikal na nakakasira ng katawan, steam, or slurry—various combinations of body, disc, seat, and coating materials are selected to meet operational and environmental demands.

Stainless Steel Butterfly Valve Components
Stainless Steel Butterfly Valve Components

Valve Body and Disc Materials

The valve body and disc are structural components that must withstand internal pressure, mekanikal na stress, at pagkakalantad ng kemikal. Kabilang sa mga karaniwang materyales ang:

  • Cast Iron (CI)
    Cost-effective and widely used in low-pressure water and HVAC systems. Not suitable for corrosive or high-temperature applications.
  • Ductile Iron (DI)
    Stronger and more impact-resistant than cast iron. Often used in water distribution, paggamot ng wastewater, and fire protection systems.
  • Carbon Steel
    Suitable for high-pressure systems and industrial environments. Requires protective coatings to prevent corrosion.
  • Hindi kinakalawang na asero (SS304/SS316)
    Napakahusay na paglaban sa kaagnasan; commonly used in chemical processing, mga kapaligiran sa dagat, and food-grade applications. SS316 offers superior resistance to chlorides and acids compared to SS304.
  • Bronze or Nickel-Aluminum Bronze (NAB)
    Commonly used in seawater applications due to their exceptional resistance to saltwater corrosion and biofouling.
  • Duplex and Super Duplex Stainless Steel
    Provide high mechanical strength and excellent resistance to pitting, bitak na kaagnasan, at pag-crack ng kaagnasan ng stress. Ideal for aggressive chemical or offshore environments.
  • PVC, CPVC, and Other Plastics
    Magaan at lumalaban sa kaagnasan; ideal for chemical dosing, low-pressure water, and non-metallic piping systems.

Upuan (Seal) Mga Materyal

  • EPDM (Ethylene Propylene Diene Monomer)
    Suitable for water, hangin, and mild chemicals. Not compatible with oils or hydrocarbons. Saklaw ng temperatura: –40°C to +120°C.
  • NBR (Nitrile Rubber)
    Resistant to oils, mga gasolina, and some chemicals. Used in industrial, petroleum, and hydraulic applications. Saklaw ng temperatura: –10°C to +100°C.
  • Viton (FKM)
    Excellent chemical and heat resistance. Suitable for aggressive fluids, mga solvent, at mga kapaligiran na may mataas na temperatura. Saklaw ng temperatura: –20°C to +200°C.
  • PTFE (Polytetrafluoroethylene)
    Inert to nearly all chemicals. Ideal for corrosive and high-purity applications. Offers non-stick surface with minimal friction. Saklaw ng temperatura: –50°C to +250°C.
  • Metal-to-Metal (Stellite, SS, Inconel)
    Used in triple-offset butterfly valves for high-temperature, mataas na presyon, and zero-leakage applications. Resistant to erosion, magsuot ng, and thermal cycling.

Shaft and Bearing Materials

  • Hindi kinakalawang na asero
    Commonly used for corrosion resistance and strength.
  • 17-4 PH Hindi kinakalawang na Asero
    Offers high strength and hardness with good corrosion resistance.
  • Bronze or Teflon-Coated Bearings
    Reduce friction, enhance wear resistance, and improve actuation smoothness.

Coating and Lining Options

Protective coatings and internal linings enhance corrosion resistance, improve flow, and prolong service life:

  • Fusion-Bonded Epoxy (FBE)
    Provides excellent corrosion protection for potable water and wastewater applications. Applied electrostatically and cured to form a durable coating.
  • Nylon Coating
    Used for enhanced chemical resistance and smoother surface finish, reducing friction and buildup.
  • Rubber Lining
    Natural or synthetic rubber lining offers abrasion resistance and chemical protection, especially in slurry handling and acidic services.
  • PTFE Lining
    Offers superior chemical inertness, used in highly corrosive environments and hygienic applications such as food and pharmaceuticals.
  • Glass Flake or Ceramic Epoxy Coatings
    Used in harsh environments to resist erosion, mataas na presyon, and chemical attack.

6. Key Technical Specifications of Butterfly Valves

Pressure Ratings

Butterfly valves are manufactured to handle specific pressure ranges, defined by international standards:

  • PN Ratings (metric)
    • PN10: Maximum pressure 10 bar (~145 psi)
    • PN16: Maximum pressure 16 bar (~232 psi)
    • PN25, PN40 also available for high-performance valves
  • ANSI/ASME Class Ratings (imperyal)
    • Klase 150 (hanggang sa 285 psi at 38°C)
    • Klase 300 and above for high-pressure applications

Saklaw ng Temperatura

The operating temperature of a butterfly valve depends largely on the body, disc, and seat materials:

Uri ng Materyal Tipikal na Saklaw ng Temperatura
EPDM Seat –40°C to +120°C
NBR Seat –10°C to +100°C
PTFE Seat –50°C to +250°C
Viton Seat –20°C to +200°C
Metal Seated Up to 600°C
PVC/Plastic Bodies –10°C to +60°C

Size Range (Nominal Diameter)

Butterfly valves are available in a wide range of nominal diameters:

  • Common Range:
    DN50 (2 pulgada) to DN1200 (48 pulgada)
  • Extended Range:
    Up to DN3000 (120 pulgada) for large industrial and infrastructure projects (hal., mga halaman ng paggamot ng tubig, dam outlets)

Flow Coefficient (Cv/Kv)

Flow coefficient represents the valve’s ability to allow fluid passage:

  • CV (Imperial): Flow rate (gallons/min) of water at 60°F with 1 psi pressure drop
  • Kv (Metriko): Flow rate (m³/hr) ha 1 bar pressure drop

Custom butterfly valves typically offer high Cv values due to their full-bore design when fully open. Cv depends on disc shape, valve size, and degree of opening. Halimbawa na lang:

  • DN100 (4″) balbula ng paruparo: Cv ≈ 120–150
  • DN300 (12″) balbula ng paruparo: Cv ≈ 1500–2000

Leakage Classes

Defined by international standards such as ANSI/FCI 70-2 at EN 12266, leakage classes indicate the valve’s sealing performance:

Klase Paglalarawan Karaniwang Paggamit
Class I Dust tight (not tested) Basic industrial systems
Class IV Metal-to-metal seat, minimal leakage Process control
Class VI Bubble-tight shutoff (soft seat) Tubig, hangin, gas services

Resilient-seated butterfly valves typically meet Class VI, while metal-seated or triple-offset valves may achieve Class IV or tighter with specialized machining.

Torque Requirements

Operating torque depends on valve size, presyon, media type, and seat friction:

  • Small valves (DN50–DN150): ~20–80 Nm
  • Large valves (DN600–DN1200): >1000 Nm

7. Mga kalamangan ng Butterfly Valves

  • Compact and Lightweight: Ideal for space-constrained installations.
  • Fast Operation: Quarter-turn design enables rapid open/close cycles.
  • Epektibo sa Gastos: Especially in large-diameter applications compared to gate or ball valves.
  • Low Pressure Drop: Streamlined flow when fully open minimizes energy losses.
  • Multi-function: Suitable for both on-off and throttling services.
  • Simple Design: Fewer moving parts result in lower maintenance needs and enhanced reliability.

8. Limitations and Challenges

  • Not Suitable for High-Pressure Throttling: Disc position may cause cavitation and vibration.
  • Seal Degradation: Especially in resilient-seated designs exposed to abrasive or high-cycle operations.
  • Flow Obstruction: The disc remains in the flow path even when fully open.
  • Limited Temperature Range: Elastomeric seats restrict use in high-temperature applications.
  • Potential for Leakage: Especially in low-cost or improperly selected valves under high stress.

9. Mga Application ng Butterfly Valves

Double Offset Butterfly Valve Components
Double Offset Butterfly Valve Components
  • Tubig & Wastewater Treatment: Efficient for isolation and control of clean and dirty water.
  • Langis & Gas: Used for fuel handling, refinery, and offshore systems.
  • Mga Sistema ng HVAC: Regulating hot or chilled water and air distribution.
  • Chemical and Petrochemical: Resistant materials handle aggressive fluids and vapors.
  • Marine & Malayo sa pampang: Compact size is beneficial for tight engine rooms.
  • Pagkain & Beverage: Hygienic valves with PTFE or stainless internals are standard.
  • Pagbuo ng Kapangyarihan: Cooling water and auxiliary service lines.
  • Pulp & Papel: Handles slurry and fiber-laden flows with robust disc and seat designs.

10. Butterfly Valve vs. Other Valve Types

Tampok Butterfly balbula Balbula ng Gate Globe Valve Balbula ng Bola
Operasyon Quarter-turn (90° rotation) Multi-turn (multiple turns to open/close) Multi-turn (linear motion) Quarter-turn
Kontrol ng Daloy On/off and moderate throttling Primarily on/off, poor throttling Excellent throttling and flow regulation Excellent shutoff, limited throttling
Pressure Drop Low when fully open Very low when fully open Higher due to tortuous flow path Minimal, full bore flow
Sukat & Timbang Compact, magaan ang timbang, suitable for large sizes Bulkier and heavier Bulkier, typically smaller sizes Compact for small sizes; bulky for large sizes
Sealing Capability Soft/metal seats, moderate tightness Good shutoff Excellent shutoff Bubble-tight, very tight shutoff
Actuation Speed
Mabilis na (quarter-turn) Mabagal (multiple turns) Mabagal (multiple turns) Mabilis na (quarter-turn)
Pagpapanatili Easy, fewer parts More prone to jamming, mas kumplikado Katamtaman, frequent maintenance needed Requires disassembly for internal servicing
Gastos Matipid sa kabuhayan, especially in large diameters Mas Mataas, especially for large sizes Katamtaman hanggang sa mataas Mas Mataas, especially at large sizes
Mga Karaniwang Aplikasyon HVAC, paggamot ng tubig, low/medium pressure systems Water distribution, langis & gas pipelines Steam control, precise flow applications High-pressure isolation, pagproseso ng kemikal
Mga Limitasyon Not ideal for high-pressure throttling Slow operation, not suited for throttling Higher pressure loss, bulkier Bulky and expensive for large diameters

11. Pamantayan sa Pagpili

Choosing the right butterfly valve involves a thorough evaluation of multiple factors to ensure optimal performance, panghabang buhay, and cost-effectiveness within a specific application.

Key criteria include:

Fluid Characteristics

  • Type of Fluid: Clean liquids, Mga Slurries, mga kemikal na nakakasira ng katawan, or gases—each requires specific seat materials and body construction to withstand erosion, kaagnasan, at gasgas na.
  • Viscosity: Higher viscosity fluids may require valves with enhanced sealing and actuator torque.
  • Presence of Solids: Fluids containing suspended solids or particulates demand robust seats and body designs to prevent wear and leakage.

Operating Pressure and Temperature

  • Rating ng Presyon: Match valve pressure class (hal., PN10, PN16, Klase 150) to pipeline operating pressure to avoid premature failure.
  • Saklaw ng Temperatura: Consider seat and body material limits—rubber seats for low temperatures and PTFE or metal seats for high-temperature service up to 600°C.

Required Shutoff Tightness

  • Leakage Class: For critical isolation, triple-offset butterfly valves offer near zero leakage (Class VI).
    For less demanding applications, resilient seated valves provide economical sealing with acceptable leakage.

Valve Actuation

  • Manual vs Automated: Determine whether manual lever, kagamitan, niyumatik, mga elektriko, or hydraulic actuators best suit the operation frequency, safety requirements, and integration into control systems.
  • Speed of Operation: Applications requiring rapid open/close cycles may favor quarter-turn actuators.

Installation Constraints

  • Space Availability: Custom Butterfly valves have a compact design, making them suitable for limited space installations compared to bulkier valve types.
  • Connection Type: Consider compatibility with piping—wafer, lug, or flanged designs based on installation and maintenance needs.

Gastos vs. Performance Balance

  • Weigh upfront costs, maintenance requirements, and expected lifespan. Sometimes investing in high-performance valves reduces total cost of ownership through reliability and fewer replacements.

12. Future Trends in Butterfly Valve Technology

  • Smart Integration: IoT-enabled actuators with sensors for real-time monitoring (presyon, temperatura, posisyon), enabling predictive maintenance.
  • Mga Advanced na Materyal: Carbon fiber bodies (30% lighter than steel) for offshore use; ceramic seats for extreme abrasion.
  • Extreme Environments: Cryogenic models (-196°C) for LNG; high-temperature designs (800°C) for hydrogen plants.
  • Sustainability: Low-leakage designs (Class VI+) to reduce emissions; recyclable materials for valve bodies.

13. Pangwakas na Salita

Custom butterfly valves are essential components in modern fluid control systems, known for their compact design, fast operation, at maraming nalalaman.

Originally conceptualized in the early 20th century, these Mga balbula have evolved significantly to meet the growing demands of industries requiring efficient and cost-effective flow control solutions.

Ngayon, butterfly valves are widely used in diverse sectors such as paggamot ng tubig, langis at gas, HVAC, pagproseso ng kemikal, marine, at pagkain at inumin mga industriya.

Their popularity stems from their ability to handle a broad range of fluids—including gases, liquids, and slurries—with minimal pressure drop and rapid shutoff capabilities.

Custom butterfly valves are a cornerstone of modern fluid handling systems due to their efficiency, mababang gastos, at kakayahang umangkop.

Whether used in municipal pipelines, industrial processing, or precision-controlled environments, selecting the right butterfly valve—matched to pressure, fluid, and operational needs—is essential for long-term performance and reliability.

DEZE: High-Precision Valve Casting Solutions for Demanding Applications

DEZE is a specialized provider of precision valve casting services, delivering high-performance components for industries that require reliability, pressure integrity, at katumpakan ng sukat.

From raw castings to fully machined valve bodies and assemblies, DEZE offers end-to-end solutions engineered to meet stringent global standards.

Our Valve Casting Expertise Includes:

Pamumuhunan sa Paghahagis for Valve Bodies & I-trim

Utilizing lost wax casting technology to produce complex internal geometries and tight-tolerance valve components with exceptional surface finishes.

buhangin paghahagis & Paghahagis ng Shell Mold

Ideal for medium to large valve bodies, mga flanges, and bonnets—offering a cost-effective solution for rugged industrial applications, pati na ang langis & gas and power generation.

Precision Machining for Valve Fit & Seal Integrity

CNC machining of seats, mga thread, and sealing faces ensures every cast part meets dimensional and sealing performance requirements.

Material Range for Critical Applications

From stainless steels (CF8/CF8M/CF3/CF3M), tanso, ductile na bakal, to duplex and high-alloy materials, DEZE supplies valve castings built to perform in corrosive, mataas na presyon, o mataas na temperatura na kapaligiran.

Whether you require custom-engineered steam traps, balbula ng paruparo, plug valves, Mga balbula ng globo, mga balbula ng gate, or high-volume production of industrial valve castings, DEZE is your trusted partner for precision, tibay ng katawan, and quality assurance.

Mga FAQ

What is the difference between a wafer and lug-style butterfly valve?

Wafer valves clamp between flanges (no bolt holes), while lug valves have threaded lugs for bolted installation, allowing one-sided removal. Lug valves suit higher pressure (≤25 bar) than wafer (≤16 bar).

How long do butterfly valves last?

Service life ranges from 10–15 years for resilient-seated valves in clean service to 5–8 years for metal-seated valves in abrasive environments. Proper maintenance extends life by 30–50%.

Are butterfly valves suitable for slurry or abrasive fluids?

Metal-seated triple-offset valves are suitable; resilient seats erode quickly. Use hardened disc materials (hal., duplex stainless steel) for extended wear.

 